Nickel Super Alloys is one of leading Supplier & Manufacturer of Sampling Pot in India, Mumbai. We have range of Sampling Pots is designed to provide safe containment for storage, examination and transportation of both liquids and gases. We have ability to customize Sampling (Pot) Cylinders to suit your exact needs . The range is designed for and used across the world in various industries, including petrochemical refineries and well sites, analytic laboratories, alternative fuel technologies, and manufacturing. These Sampling Cylinder is available in Stainless Steel 304, Stainless Steel 316, Carbon Steel, Monel,Hastelloy,Inconel.

Our Sampling Pots are designed to capture individual samples over a period of time allowing for a combined sample representation of long-term pipeline flow. The systems injection mode is programmable to sample proportion to flow or time. Either mode will supply a highly accurate composite sample of the total measured product flow.

Hastelloy Sampling Cylinders in 1800 psi ,3000 psi and 10000 psi Supplier in India

Datasheet of Sampling Cylinder 1800 PSI

PART No. P NPT - F Pressure Rating PSIG Capacity (Internal Vol.)cm 3±5% L mm D mm
FSC150-4N2 1/4” 1800 150 135 50.8
FSC300-4N2 1/4” 1800 300 225 50.8
FSC400-4N2 1/4” 1800 400 290 50.8
FSC500-4N2 1/4” 1800 500 350 50.8
FSC1000-4N2 1/4” 1800 1000 275 88.9
FSC2250-4N2 1/4” 1800 2250 435 120
FSC3785-4N2 1/4” 1800 3785 680 120
FSC1000-8N2 1/2” 1800 1000 275 88.9
FSC2250-8N2 1/2” 1800 2250 435 102
FSC3785-8N2 1/2” 1800 3785 680 102
FSC1000-12N2 3/4” 1800 1000 275 88.9
FSC2250-12N2 3/4” 1800 2250 435 102
FSC3785-12N2 3/4” 1800 3785 680 102

Datasheet of Sampling Cylinder 5000 PSI

PART No. P NPT - F Pressure Rating PSIG Capacity (Internal Vol.)cm 3±5% L mm D mm
FSC150-4N5 1/4” 5000 150 135 50.8
FSC300-4N5 1/4” 5000 300 225 50.8
FSC400-4N5 1/4” 5000 400 290 50.8
FSC500-4N5 1/4” 5000 500 350 50.8
FSC1000-4N5 1/4” 5000 1000 275 88.9
FSC2250-4N5 1/4” 5000 2250 435 120
FSC3785-4N5 1/4” 5000 3785 680 120
FSC1000-8N5 1/2” 5000 1000 275 88.9
FSC2250-8N5 1/2” 5000 2250 435 102
FSC3785-8N5 1/2” 5000 3785 680 102
FSC1000-12N5 3/4” 5000 1000 275 88.9
FSC2250-12N5 3/4” 5000 2250 435 102
FSC3785-12N5 3/4” 5000 3785 680 102

Datasheet of Sampling Cylinder 10000 PSI

PART No. P NPT - F Pressure Rating PSIG Capacity (Internal Vol.)cm 3±5% L mm D mm
FSC150-4N10 1/4” 10000 150 135 50.8
FSC300-4N10 1/4” 10000 300 225 50.8
FSC400-4N10 1/4” 10000 400 290 50.8
FSC500-4N10 1/4” 10000 500 350 50.8
FSC1000-4N10 1/4” 10000 1000 275 88.9
FSC2250-4N10 1/4” 10000 2250 435 120
FSC3785-4N10 1/4” 10000 3785 680 120
FSC1000-8N10 1/2” 10000 1000 275 88.9
FSC2250-8N10 1/2” 10000 2250 435 102
FSC3785-8N10 1/2” 10000 3785 680 102
FSC1000-12N10 3/4” 10000 1000 275 88.9
FSC2250-12N10 3/4” 10000 2250 435 102
FSC3785-12N10 3/4” 10000 3785 680 102

Material of Construction

Stainless Steel ASME / ASTM SA / A403 SA / A 774 WP-S, WP-W, WP-WX, 304, 304L, 316, 316L, 304/304L, 304H, 316H, 316/316L, 321, 330, 347, 309/S, 310/S, 317/L, 333, 410/S, DIN 1.4301, DIN1.4306, DIN 1.4401, DIN 1.4404
Alloy Steel ASTM SA 182 - E25, E26, E27, E28, E29B, E30B, E39B, E40B, E36B, E36C, E41B, AISI4130, AISI4140, AISI4340, 42CRMO4, 16MNCR5, 20MNCR5, 21CrMoV57, EN353, EN354, F11, F22, F91, F9, P11, P22, P91, P9, P5, P92, EN42J, EN8, EN19
Carbon Steel ASTM A 234 WPB , WPBW, WPHY 42, WPHY 46, WPHY 52, WPH 60, WPHY 65 & WPHY 70
Monel Monel 400, Monel K500, Monel R-405
Nickel Alloy Nickel 200, Nickel 201
Inconel Inconel 600, Inconel 601, Inconel 625, Inconel 718
Incoloy Incoloy 800, Inconel 800H, 800HT
Hastalloy Hastalloy B2, Hastalloy B3, Hastalloy C22, Hastalloy C276, Hastalloy X
Titanium Gr1, Gr2, Gr3, Gr5, Gr7, Gr11
Duplex Steel ASTM / ASME A/SA 182 UNS F44, F45, F51, F53, F55, F60, F61

Countries We Export to

Nickel Super Alloys manufactures and exports ​Sampling Pot​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Sampling Pot to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today