Stainless Steel 304 / 304L Threaded Forged Fittings

Stainless Steel 304 / 304L Threaded Forged Fittings

Stainless Steel 304 / 304L Socket Weld 90 Deg. Elbow, UNS S30400 / S30403 Socket Weld Tee, DIN NR. 1.4301 / 1.4306 Socket Weld Cross, SS 304 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of leading supplier and distributor of Stainless Steel 304 / 304L Socket Weld Forged Fittings, which has better corrosion resistance. Stainless Steel 304 Socket Weld Elbow Forged Fittings is used in a variety of household and industrial applications. Essentially non-magnetic, Stainless Steel 304 Socket Weld Tee Forged Fittings becomes slightly magnetic when cold worked. Stainless Steel 304L Socket Weld Cross Forged Fittings is used in heavy gauge components for improved weldability. Stainless Steel 304 Socket Weld Cap Forged Fittings has good forming and welding properties as well as strong corrosion resistance and strength. Stainless Steel 304L Socket Weld Coupling Forged Fittings has excellent corrosion that takes place next to grain boundaries.

Stainless Steel 304 Socket Weld Union Forged Fittings is often used to avoid possible sensitization corrosion in welded components. Stainless Steel 304L Socket Weld Plug Forged Fittings have excellent weld-ability characteristics with or without the addition of filler metals. Stainless Steel 304 Socket Weld Lateral Tee Forged Fittings is used in high-temperature applications. The chromium content in Stainless Steel UNS S30400 Socket Weld Forged Fittings promotes the considerable resistance to the effects of corrosion and oxidation. Stainless Steel UNS S30403 Socket Weld Forged Fittings increases the strength (particularly at temperatures above about 500 Degree C). Stainless Steel 304L Socket Weld Bushing Forged Fittings has a higher corrosion resistance than regular steel. SS 304 Socket Weld Forged Fittings has excellent forming and welding properties.

Stainless Steel 304 Socket Weld Cap, Stainless Steel 304L Socket Weld Bend, SS 304 Socket Weld Cross, UNS S30400 / S30403 Socket Weld Bushing, DIN NR. 1.4301 / 1.4306 Socket Weld Coupling, Stainless Steel 304 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 304 / 304L Socket Weld Forged Fittings Specifications

Grade SS 304 | Stainless Steel 304 | UNS S30400
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee.
Type Socket Weld Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 304 1.4301 S30400 SUS 304 304S31 08Х18Н10 Z7CN18‐09 X5CrNi18-10
SS 304L 1.4306\1.4307 S30403 SUS 304L 304S11 03Х18Н11 Z7CN18‐09 X2CrNi18-9 / X2CrNi19-11

Stainless Steel 304 / 304L Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
SS 304 0.08 max 2 max 0.75 max 0.045 max 0.030 max 18 – 20 – 8 – 11 –
SS 304L 0.35 max 2 max 1.00max 0.045 max 0.030 max 18 – 20 – 8 – 13 –

Stainless Steel 304 / 304L Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.0 g/cm3 1400 °C (2550 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 304 / 304L Socket Weld Threaded Forged Fittings

  • Stainless Steel 304 Socket Weld Forged Elbow Supplier in UAE
  • SS 304L Socket Weld Equal Tee Manufacturer in India
  • SS 304 Socket Weld Cross
  • UNS S30400 / S30403 Socket Weld Union
  • UNS S30400 / S30403 Socket Weld Plug
  • DIN NR. 1.4301 / 1.4306 Socket Weld Hex Plug
  • DIN NR. 1.4301 / 1.4306 45 Deg Socket Weld Elbow Distributors
  • Stainless Steel 304 Socket Weld Bushing
  • Stainless Steel 304L Socket Weld Lateral Tee
  • SUS 304 Socket Weld Cross
  • Stainless Steel 304 Socket Weld Coupling Exporter in Russia
  • Stainless Steel 304L Socket Weld Tees
  • UNS S30400 / S30403 45 deg Socket Weld Elbow Supplier in Poland
  • UNS S30400 / S30403 Socket Weld 90 deg Elbow
  • DIN NR. 1.4301 / 1.4306 Socket Weld Cap in Qatar
  • DIN NR. 1.4301 / 1.4306 Socket Weld Bend Flanges
  • SS 304L Socket Weld Union
  • X2CrNi19-11 Socket Weld Bushing
  • X5CrNi18-10 Socket Weld Lateral Tee
  • X2CrNi18-9 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 304 / 304L Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 304 / 304L Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today