Stainless Steel 310 / 310S Threaded Forged Fittings

Stainless Steel 310 / 310S Threaded Forged Fittings

Stainless Steel 310 Socket Weld 90 Deg. Elbow, UNS S31000 / S31008 Socket Weld Tee, DIN NR. 1.4841 / 1.4845 Socket Weld Cross, SS 310S Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is a prominent firm in manufacturing an exporting Stainless Steel 310 / 310S Socket Weld Forged Fittings, which has good sulfidation resistance. Stainless Steel 310 Socket Weld Elbow Forged Fittings is recommended that this steel should not be continuously used at 425 Degree C – 860 Degree C (797 Degree F – 1580 Degree F) range due to carbide precipitation. Stainless Steel 310S Socket Weld Tee Forged Fittings has excellent resistancein intermittent service and 1150 Degree C (2102 Degree F) in continuous service. Stainless Steel 310 Socket Weld Cap Forged Fittings is lightly magnetic when cold worked, because heat treatment after welding is normally not usual.

Stainless Steel 310S Socket Weld Coupling Forged Fittings is used in the temperature range where creep strength as a rule is the dimensioning factor and where heat treatment corrosion occurs. Stainless Steel 310 Socket Weld Cross Forged Fittings requires more severely carburizing atmospheres of industrial heat treating furnaces. Stainless Steel 310S Socket Weld Union Forged Fittings is often used at cryogenic temperatures. Stainless Steel 310 Socket Weld Plug Forged Fittings can be utilized in slightly oxidizing, nitriding andcementing applications. Stainless Steel UNS S31000 Socket Weld Forged Fittings is used in coal gasifier internal components, thermowells andlead pots. The higher alloyed Stainless Steel UNS S31008 Socket Weld Forged Fittings generally have excellent strength at elevated temperatures.

Stainless Steel 310 Socket Weld Cap, Stainless Steel 310S Socket Weld Bend, SS 310 Socket Weld Cross, UNS S31000 / S31008 Socket Weld Bushing, DIN NR. 1.4841 / 1.4845 Socket Weld Coupling, Stainless Steel 310 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 310 / 310S Socket Weld Forged Fittings Specifications

Grade SS 310 | SS 310S , UNS S31000 | S31008
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee.
Type Socket Weld Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 310 1.4841 S31000 SUS 310 310S24 20Ch25N20S2 – X15CrNi25-20
SS 310S 1.4845 S31008 SUS 310S 310S16 20Ch23N18 – X8CrNi25-21

Stainless Steel 310 / 310S Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
SS 310 0.015 max 2 max 0.15 max 0.020 max 0.015 max 24 – 26 0.10 19 – 21 –
SS 310S 0.08 max 2 max 1.00 max 0.045 max 0.030 max 24 – 26 0.75 19 – 21 –

Stainless Steel 310 / 310S Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.9 g/cm3 1402 °C (2555 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 40 %

Other Types of Stainless Steel 310 / 310S Socket Weld Threaded Forged Fittings

  • Stainless Steel 310 Socket Weld Forged Elbow Supplier in UAE
  • SS 310S Socket Weld Equal Tee Manufacturer in India
  • SS 310 Socket Weld Cross
  • UNS S31000 / S31008 Socket Weld Union
  • UNS S31000 / S31008 Socket Weld Plug
  • DIN NR. 1.4841 / 1.4845 Socket Weld Hex Plug
  • DIN NR. 1.4841 / 1.4845 45 Deg Socket Weld Elbow Distributors
  • Stainless Steel 310 Socket Weld Bushing
  • Stainless Steel 310S Socket Weld Lateral Tee
  • SUS 310 Socket Weld Cross
  • Stainless Steel 310 Socket Weld Coupling Exporter in Russia
  • Stainless Steel 310S Socket Weld Tees
  • UNS S31000 / S31008 45 deg Socket Weld Elbow Supplier in Poland
  • UNS S31000 / S31008 Socket Weld 90 deg Elbow
  • DIN NR. 1.4841 / 1.4845 Socket Weld Cap in Qatar
  • DIN NR. 1.4841 / 1.4845 Socket Weld Bend Flanges
  • SS 310S Socket Weld Union
  • X15CrNi25-20 Socket Weld Bushing
  • X8CrNi25-21 Socket Weld Lateral Tee
  • 20Ch25N20S2 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 310 / 310S Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310S Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today