Hastelloy C22 Socket Weld Forged Fittings

Hastelloy C22 Socket Weld Forged Fittings

Hastelloy C22 Socket Weld 90 Deg. Elbow, Hastelloy C22 Socket Weld Tee, UNS N06022 Socket Weld Cross, DIN NR. 2.4602 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is a known exporter and supplier of Hastelloy Alloy C22 Socket Weld Forged Fittings, which has the risk of sensitization (inter-granular corrosion attack). The corrosion resistance of Hastelloy C22 Socket Weld Elbow Forged Fittings renders it suitable for many industrial applications. Molybdenum and tungsten in Hastelloy C22 Socket Weld Tee Forged Fittings improve the crevice corrosion and pitting resistance characteristics of the alloy. Hastelloy C22 Socket Weld Cap Forged Fittings possesses prominent resistance performance to different chemical environments, including strong oxidizing matter. With this versatile performance, Hastelloy C22 Socket Weld Cross Forged Fittingscan be used in some troublesome environments or in a variety of production plants.

Hastelloy C22 Socket Weld Coupling Forged Fittings has excellent resistance to oxidizing aqueous media including wet chlorine and mixtures containing nitric acid or oxidizing acids with chlorine ions. The high chromium content in Hastelloy C22 Socket Weld Union Forged Fittings provides much higher resistance to oxidizing media than the family standard. Hastelloy C22 Socket Weld Plug Forged Fittings is the most adaptable nickel alloy in the Hastelloy category. In addition to having exceptional corrosion resistance, Hastelloy C22 Socket Weld Lateral Tee Forged Fittings can also be readily fabricated. Hastelloy UNS N06022 Socket Weld Forged Fittingsis proven to possess excellent weldability and high corrosion resistance as consumable filler wires and electrodes. Hastelloy WNR 2.4602 Socket Weld Forged Fittings has outstanding resistance to pitting and crevice corrosion.

Hastelloy C22 Socket Weld Cap, Hastelloy C22 Socket Weld Bend, Hastelloy C22 Socket Weld Cross, Hastelloy C22 Socket Weld Bushing, UNS N06022 Socket Weld Coupling, ASTM B564 Hastelloy C22 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Hastelloy C22 Socket Weld Forged Fittings Specifications

Grade Hastelloy C22 | UNS N06022
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, C220 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Hastelloy C22
UNS N06022
WERKSTOFF NR. 2.4602
JIS NW 6022
EN NiCr21Mo14W

Hastelloy C22 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Co Mo Ni Fe Cr
Hastelloy C22 0.10 max 0.50 max 0.08 max 0.02 max 0.02 max 2.50 max 12.50 – 14.50 50.015 min* 2.00 – 6.00 20.00 – 22.50

Hastelloy C22 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.69 g/cm3 1399 °C (2550 °F) Psi – 1,00,000 , MPa – 690 Psi – 45000 , MPa – 310 45 %

Other Types of Hastelloy C22 Socket Weld Threaded Forged Fittings

  • Hastelloy C22 Socket Weld Forged Elbow Supplier in UAE
  • Hastelloy C22 Socket Weld Equal Tee Manufacturer in India
  • Hastelloy C22 Socket Weld Cross
  • Hastelloy C22 Socket Weld Union
  • UNS N06022 Socket Weld Plug
  • UNS N06022 Socket Weld Hex Plug
  • DIN NR. 2.4602 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4602 Socket Weld Bushing
  • Hastelloy C22 Socket Weld Lateral Tee
  • Hastelloy C22 Socket Weld Cross
  • Hastelloy C22 Socket Weld Tees
  • UNS N06022 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N06022 Socket Weld 90 deg Elbow
  • DIN NR. 2.4602 Socket Weld Cap in Qatar
  • DIN NR. 2.4602 Socket Weld Bend Flanges
  • Hastelloy C22 Socket Weld Union
  • Hastelloy C22 Socket Weld Bushing
  • NW 6022 Socket Weld Lateral Tee
  • NiCr21Mo14W Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Hastelloy C22 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Hastelloy C22 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo