Nickel Alloy 200 Socket Weld Forged Fittings

Nickel Alloy 200 Socket Weld Forged Fittings

Nickel Alloy 200 Socket Weld 90 Deg. Elbow, Nickel Alloy 200 Socket Weld Tee, UNS N02200 Socket Weld Cross, DIN NR. 2.4066 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the finest manufacturers of Nickel 200 Socket Weld Forged Fittings in India, which is ferromagnetic. Nickel 200 Socket Weld Elbow Forged Fittings has low hardness, good weldability and good ductility, making the metal easy to fabricate. Nickel 200 Socket Weld Tee Forged Fittings has a number of useful characteristics including good ductility and mechanical properties. The extra-low carbon content of Nickel 200 Socket Weld Cap Forged Fittings gives virtual immunity to inter-granular attack above about 315 Degree C. At higher temperatures, Nickel 200 Socket Weld Coupling Forged Fittings suffers from graphitization which results in severely compromised properties. Nickel 200 Socket Weld Cross Forged Fittingscan also be used under oxidizing conditions when a passive oxide film is formed.

Nickel 200 Socket Weld Lateral Tee Forged Fittings is used in in structural applications where resistance to corrosion is a prime consideration. Nickel 200 Socket Weld Union Forged Fittings also has a high curie temperature and good magnetostrictive properties. Nickel 200 Socket Weld Plug Forged Fittings is highly resistant to various reducing chemicals. In alkaline,acid and neutral salt solutions Nickel 200 Socket Weld Bend Forged Fittings shows good resistance, but in oxidizing salt solutions severe attack will occur. Nickel 200 Socket Weld 45 Degree Elbow Forged Fittings can be shaped through all hot working and cold working practices. Nickel 200 Socket Weld 90 Degree Elbow Forged Fittingshas exceptional resistance to caustic alkalis at various temperatures and concentrations.

Nickel Alloy 200 Socket Weld Cap, Nickel Alloy 200 Socket Weld Bend, Nickel 200 Socket Weld Cross, Nickel 200 Socket Weld Bushing, UNS N02200 Socket Weld Coupling, ASTM B564 Nickel 200 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Nickel 200 Socket Weld Forged Fittings Specifications

Grade Nickel Alloy 200 | UNS N02200
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 2000 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Nickel 200
UNS N02200
GOST НП-2
WERKSTOFF NR. 2.4066
BS NA 11
AFNOR N-100M
EN Ni 99.2
JIS NW 2200

Nickel 200 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cu Mo Ni Fe
Nickel 200 0.15 max 0.35 max 0.35 max – 0.01 max 0.25 max – 99.00 min 0.40 max

Nickel 200 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.9 g/cm3 1446 °C (2635 °F) Psi – 67000 , MPa – 462 Psi – 21500 , MPa – 148 45 %

Other Types of Nickel 200 Socket Weld Threaded Forged Fittings

  • Nickel 200 Socket Weld Forged Elbow Supplier in UAE
  • Nickel 200 Socket Weld Equal Tee Manufacturer in India
  • Nickel 200 Socket Weld Cross
  • Nickel 200 Socket Weld Union
  • UNS N02200 Socket Weld Plug
  • UNS N02200 Socket Weld Hex Plug
  • DIN NR. 2.4066 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4066 Socket Weld Bushing
  • Nickel 200 Socket Weld Lateral Tee
  • Nickel 200 Socket Weld Cross
  • Nickel 200 Socket Weld Tees
  • UNS N02200 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N02200 Socket Weld 90 deg Elbow
  • DIN NR. 2.4066 Socket Weld Cap in Qatar
  • DIN NR. 2.4066 Socket Weld Bend Flanges
  • Nickel 200 Socket Weld Union
  • Nickel 200 Socket Weld Bushing
  • Nickel 200 Socket Weld Lateral Tee
  • Nickel 200 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Nickel 200 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Nickel 200 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today