Monel 400 Socket Weld Forged Fittings

Monel 400 Socket Weld Forged Fittings

Monel 400 Socket Weld 90 Deg. Elbow, Monel 400 Socket Weld Tee, UNS N04400 Socket Weld Cross, DIN NR. 2.4360 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the known suppliers of Monel Alloy 400 Socket Weld Forged Fittings, which has been used in a variety of applications. Monel 400 Socket Weld Elbow Forged Fittings is a solid-solution binary alloy and is resistant to both steam and seawater. Monel 400 Socket Weld Tee Forged Fittings has good mechanical properties from sub-zero temperatures up to 549 Degree C. Monel 400 Socket Weld Cap Forged Fittingsis particularly resistant to hydrochloric and hydrofluoric acids when they are de-aerated. Monel 400 Socket Weld Coupling Forged Fittings is a low corrosion rate in rapidly flowing brackish or seawater combined with excellent resistance to stress-corrosion cracking in most fresh waters.

Monel 400 Socket Weld Cross Forged Fittings is widely used in many fields, especially marine and chemical processing. Monel 400 Socket Weld Lateral Tee Forged Fittingshas high strength and can be hardened only by cold working. The Curie Temperature of Monel 400 Socket Weld Union Forged Fittings lies in the ambient temperature range. Forging of Monel 400 Socket Weld Plug Forged Fittingsis to be done by controlled procedures. Forging of Monel UNS N04400 Socket Weld Forged Fittingsmay be carried out between 2150 Degree F (1175 Degree C) and 1200 Degree F (650 Degree C). The corrosion resistance of Nickel Alloy 400 Socket Weld Forged Fittings is particular strong in rapid flowing brackish water or seawater.

Monel 400 Socket Weld Cap, Monel 400 Socket Weld Bend, Monel 400 Socket Weld Cross, Monel 400 Socket Weld Bushing, UNS N04400 Socket Weld Coupling, ASTM B564 Monel 400 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Monel 400 Socket Weld Forged Fittings Specifications

Grade Monel 400 | UNS N04400
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee.
Type Socket Weld Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Monel 400 2.4360 N04400 NW 4400 NA 13 МНЖМц 28-2,5-1,5 NU-30M NiCu30Fe

Monel 400 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cu Mo Ni Fe
Monel 400 0.30 max 2 max 0.50 max – 0.024 max 28 – 34 – 63.00 min 2.50 max

Monel 400 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.8 g/cm3 1350 °C (2550 °F) Psi – 80000 , MPa – 550 Psi – 35000 , MPa – 240 40 %

Other Types of Monel 400 Socket Weld Threaded Forged Fittings

  • Monel 400 Socket Weld Forged Elbow Supplier in UAE
  • Monel 400 Socket Weld Equal Tee Manufacturer in India
  • Monel 400 Socket Weld Cross
  • Monel 400 Socket Weld Union
  • UNS N04400 Socket Weld Plug
  • UNS N04400 Socket Weld Hex Plug
  • DIN NR. 2.4360 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4360 Socket Weld Bushing
  • Monel 400 Socket Weld Lateral Tee
  • Monel 400 Socket Weld Cross
  • Monel 400 Socket Weld Coupling Exporter in Russia
  • Monel 400 Socket Weld Tees
  • UNS N04400 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N04400 Socket Weld 90 deg Elbow
  • DIN NR. 2.4360 Socket Weld Cap in Qatar
  • DIN NR. 2.4360 Socket Weld Bend Flanges
  • Monel 400 Socket Weld Union
  • Monel 400 Socket Weld Bushing
  • NU-30M Socket Weld Lateral Tee
  • NiCu30Fe Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Monel 400 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Monel 400 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today