Super Duplex Steel UNS S32750 / S32760 Socket Weld Forged Fittings

Super Duplex Steel UNS S32750 / S32760 Socket Weld Forged Fittings

Super Duplex Steel UNS S32750 Socket Weld 90 Deg. Elbow, Duplex Steel UNS S32760 Socket Weld Tee, UNS S32750 Socket Weld Cross, DIN NR. 1.4410 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the notable exporters of Super Duplex Steel S32750 / S32760 Socket Weld Forged Fittings, which is used for service in highly corrosive conditions. Super Duplex S32750 Socket Weld Elbow Forged Fittings are being widely used in offshore oil and gas exploration and production. Super Duplex S32760 Socket Weld Tee Forged Fittingsis also used in sea water desalination and high pressure RO plants. Ambient and sub-zero (down to minus 50 Degree C) notch ductility of Super Duplex S32750 Socket Weld Cap Forged Fittings is good. Low carbon content of Super Duplex S32760 Socket Weld Coupling Forged Fittings greatly lowers the risk of carbide precipitation at the grain boundaries during heat treatment.

Super Duplex S32750 Socket Weld Cross Forged Fittings also provides excellent resistance to inorganic acids, especially those containing chlorides. The balanced duel phase microstructure of Super Duplex S32760 Socket Weld Union Forged Fittings combines high strength with cost effective corrosion resistance particularly in high chloride environments. Super Duplex S32750 Socket Weld Plug Forged Fittingsis resistant to corrosion fatigue, to general corrosion in acids. In dilute sulfuric acid contaminated with chloride ions, Super Duplex S32760 Socket Weld Lateral Tee Forged Fittingshas better corrosion resistance. Usage of Super Duplex 2507 Socket Weld Forged Fittingsshould be limited to applications below 600 Degree F (316 Degree C).

Super Duplex Steel UNS S32750 Socket Weld Cap, Super Duplex Steel UNS S32760 Socket Weld Bend, UNS S32750 Socket Weld Cross, UNS S32760 Socket Weld Bushing, UNS S32750 Socket Weld Coupling, UNS S32760 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Super Duplex Steel UNS S32750 / S32760 Socket Weld Forged Fittings Specifications

Grade Super Duplex S32750 / S32760 | WNR. 1.4410
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Grade S32750 / S32760 / A182 Gr F51 / F52 / F53 / F54 / F55 / F57 / F59 / F60 / F61
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee.
Type Socket Weld Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Super Duplex S32750 / S32760 1.4410 S32750/S32760 – – – – –

Super Duplex Steel UNS S32750 / S32760 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni N Cu
S32750/S32760 0.030max  1.20 max 0.80 max 0.035max 0.020 max 24.0-26.0  3.0-5.0  6.0-8.0 0.24/0.32 0.50

Super Duplex Steel UNS S32750 / S32760 Socket Weld Forged Fittings Mechanical Properties

Grades Density (g/cm 3) Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
S32750 / S32760 7.8 g/cm3 1350 °C (2460 °F) Psi – 80000 , MPa – 550 Psi – 116000 , MPa – 800 15%

Other Types of Super Duplex Steel UNS S32750 / S32760 Socket Weld Threaded Forged Fittings

  • Super Duplex Steel UNS S32750 Socket Weld Forged Elbow Supplier in UAE
  • Super Duplex Steel UNS S32760 Socket Weld Equal Tee Manufacturer in India
  • Duplex 2507 Socket Weld Cross
  • UNS S32750 Socket Weld Union
  • UNS S32760 Socket Weld Plug
  • Super Duplex Steel UNS S32750 Socket Weld Hex Plug
  • DIN NR. 1.4410 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 1.4410 Socket Weld Bushing
  • UNS S32750 Socket Weld Lateral Tee
  • UNS S32760 Socket Weld Cross
  • Super Duplex Steel UNS S32750 Socket Weld Tees
  • Super Duplex Steel UNS S32760 45 deg Socket Weld Elbow Supplier in Poland
  • Duplex 2507 Socket Weld 90 deg Elbow
  • DIN NR. 1.4410 Socket Weld Cap in Qatar
  • DIN NR. 1.4410 Socket Weld Bend Flanges
  • Super Duplex Steel UNS S32750 Socket Weld Union
  • Super Duplex Steel UNS S32760 Socket Weld Bushing
  • UNS S32750 Socket Weld Lateral Tee
  • UNS S32760 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Super Duplex Steel UNS S32750 / S32760 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Super Duplex Steel UNS S32750 / S32760 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today