Duplex Steel UNS S31803 / S32205 Socket Weld Forged Fittings

Duplex Steel UNS S31803 / S32205 Socket Weld Forged Fittings

Duplex Steel UNS S31803 Socket Weld 90 Deg. Elbow, Duplex Steel UNS S32205 Socket Weld Tee, UNS S31803 Socket Weld Cross, DIN NR. 1.4462 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the prominent suppliers of Duplex Steel S31803 / S32205 Socket Weld Forged Fittings, which is used in chemical processing, transport and storage. Duplex Steel S31803 Socket Weld Elbow Forged Fittings may be encountered in the gas, petrochemical and off shore industries. High temperature strength of Duplex Steel S32205 Socket Weld Tee Forged Fittings is similar to Stainless Steel 430 in the range of 1150 Degree C to 950 Degree C. Duplex Steel S31803 Socket Weld Cap Forged Fittings are in most cases, tougher than ferritic stainless steels. Duplex Steel S32205 Socket Weld Coupling Forged Fittingsis often used in pressure vessels, piping, tanks, and heat exchangers.

In addition, Duplex Steel S31803 Socket Weld Cross Forged Fittings offers good resistance to stress corrosion cracking. Duplex Steel S32205 Socket Weld Lateral Tee Forged Fittings has higher strength which is around twice that of Type 304 austenitic stainless steel. High hardness in Duplex Steel S31803 Socket Weld Union Forged Fittings provides better wear resistance in abrasive environments. The advantage ofDuplex Steel S32205 Socket Weld Plug Forged Fittingsis that it combines the favorable qualities of a ferritic alloy (SCC and high strength) with those of an austenitic alloy (corrosion resistance and ease of fabrication). Duplex Steel 2205 Socket Weld Forged Fittings are able to cope with high stress conditions where to use of ordinary austenitic stainless steel will result in mechanical failure.

Duplex Steel UNS S31803 Socket Weld Cap, Duplex Steel UNS S32205 Socket Weld Bend, UNS S31803 Socket Weld Cross, UNS S32205 Socket Weld Bushing, UNS S31803 Socket Weld Coupling, UNS S32205 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Duplex Steel UNS S31803 / S32205 Socket Weld Forged Fittings Specifications

Grade Duplex S31803 / S32205 | WNR. 1.4462
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Grade S31803 / S32205 / A182 Gr F51 / F52 / F53 / F54 / F55 / F57 / F59 / F60 / F61
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee.
Type Socket Weld Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Duplex S31803/S32205 1.4462 S31803/S32205 – – – – –

Duplex Steel UNS S31803 / S32205 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni N Fe
Duplex S31803 0.030max  2.00 max 1.00 max 0.030max 0.020 max 22.0-23.0  3.0-3.5  4.50-6.50 0.14-0.20  63.72 min
Duplex S32205 0.030max  2.00 max 1.00 max 0.030max 0.020 max 21.0-23.0 2.50-3.50  4.50-6.50 0.08-0.20  63.54 min

Duplex Steel UNS S31803 / S32205 Socket Weld Forged Fittings Mechanical Properties

Grades Density (g/cm 3) Density (lb/in 3) Melting Point (°C) Melting Point (°F)
S31803 / S32205 7.805 0.285 1420 – 1465 2588 – 2669

Other Types of Duplex Steel UNS S31803 / S32205 Socket Weld Threaded Forged Fittings

  • Duplex Steel UNS S31803 Socket Weld Forged Elbow Supplier in UAE
  • Duplex Steel UNS S32205 Socket Weld Equal Tee Manufacturer in India
  • Duplex 2205 Socket Weld Cross
  • UNS S31803 Socket Weld Union
  • UNS S32205 Socket Weld Plug
  • Duplex Steel UNS S31803 Socket Weld Hex Plug
  • DIN NR. 1.4462 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 1.4462 Socket Weld Bushing
  • UNS S31803 Socket Weld Lateral Tee
  • UNS S32205 Socket Weld Cross
  • Duplex Steel UNS S31803 Socket Weld Tees
  • Duplex Steel UNS S32205 45 deg Socket Weld Elbow Supplier in Poland
  • Duplex 2205 Socket Weld 90 deg Elbow
  • DIN NR. 1.4462 Socket Weld Cap in Qatar
  • DIN NR. 1.4462 Socket Weld Bend Flanges
  • Duplex Steel UNS S32205 Socket Weld Union
  • Duplex Steel UNS S31803 Socket Weld Bushing
  • UNS S32205 Socket Weld Lateral Tee
  • UNS S310803 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Duplex Steel UNS S31803 / S32205 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Duplex Steel UNS S31803 / S32205 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today