Inconel 600 / 601 Socket Weld Forged Fittings

Inconel 600 / 601 Socket Weld Forged Fittings

Inconel 600 Socket Weld 90 Deg. Elbow, Inconel 601 Socket Weld Tee, UNS N06600 / N06601 Socket Weld Cross, DIN NR. 2.4816 / 2.4851 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the prominent suppliers, manufacturers and exporters of Inconel Alloy 600 / 601 Socket Weld Forged Fittings, which has superb corrosion resistance to caustic environments. From its introduction to industry, Inconel 600 Socket Weld Elbow Forged Fittings has developed into a wide spectrum of applications for high temperature strength and corrosion resistance. Inconel 601 Socket Weld Tee Forged Fittings is attractive for high temperature applications where aluminum and steel would succumb to creep as a result of thermally induced crystal vacancies.Inconel 600 Socket Weld Cap Forged Fittings has good mechanical property when below zero, room temperature and high temperature. Inconel 601 Socket Weld Coupling Forged Fittings was designed to resist deformation at high temperatures.

The chromium content in Inconel 600 Socket Weld Cross Forged Fittings provides resistance to weaker oxidizing conditions. The high nickel content of Inconel 601 Socket Weld Union Forged Fittings provides a level of resistance to reducing environments. Inconel 600 Socket Weld Plug Forged Fittings has useful resistance to dry Cl2 and HCl gases at moderately elevated temperatures. Inconel 601Socket Weld Lateral Tee Forged Fittings can also be hardened and strengthened through cold work. Inconel UNS N06600 Socket Weld Forged Fittings can both hot formed and cold form using typical processes. Inconel WNR 2.4816 Socket Weld Forged Fittings is resistant to corrosion by a number of organic and inorganic compounds. Chromium content in Alloy 601SW Tee Forged Fittings confers resistance to sulfur compounds.

Inconel 600 Socket Weld Cap, Inconel 601 Socket Weld Bend, Inconel 600 Socket Weld Cross, Inconel 601 Socket Weld Bushing, UNS N06600 / N06601 Socket Weld Coupling, ASTM B564 Inconel 600 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 600 / 601 Socket Weld Forged Fittings Specifications

Grade Inconel Alloy 600 | UNS N06600
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Inconel 600 2.4816 N06600 NCF 600 NA 13 МНЖМц 28-2,5-1,5 NC15FE11M NiCr15Fe
Inconel 601 2.4851 N06601 NCF 601 NA 49 XH60BT NC23FeA NiCr23Fe

Inconel 600 / 601 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cu Ni Fe
Inconel 600 0.15 max 1 max 0.5 max – 0.015 max 14 – 17 0.50 max 72 min 6.0-10.0
Inconel 601 0.10 max 1 max 0.5 max – 0.015 max 1.0 max 21.0-25.0 58.0-63.0 Balance

Inconel 600 / 601 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.1 g/cm3 1411 °C (2571 °F) Psi – 80,000 , MPa – 550 Psi – 30,000 , MPa – 205 30 %

Other Types of Inconel 600 / 601 Socket Weld Threaded Forged Fittings

  • Inconel 600 Socket Weld Forged Elbow Supplier in UAE
  • Inconel 601 Socket Weld Equal Tee Manufacturer in India
  • Inconel 600 Socket Weld Cross
  • Inconel 601 Socket Weld Union
  • UNS N06600 / N06601 Socket Weld Plug
  • UNS N06600 / N06601 Socket Weld Hex Plug
  • DIN NR. 2.4816 / 2.4851 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4816 / 2.4851 Socket Weld Bushing
  • Inconel 600 Socket Weld Lateral Tee
  • Inconel 601 Socket Weld Cross
  • Inconel 600 Socket Weld Coupling Exporter in Russia
  • Inconel 601 Socket Weld Tees
  • UNS N06600 / N06601 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N06600 / N06601 Socket Weld 90 deg Elbow
  • DIN NR. 2.4816 / 2.4851 Socket Weld Cap in Qatar
  • DIN NR. 2.4816 / 2.4851 Socket Weld Bend Flanges
  • NiCr15Fe Socket Weld Union
  • NiCr23Fe Socket Weld Bushing
  • NC15FE11M Socket Weld Lateral Tee
  • NC23FeA Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 600 / 601 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 600 / 601 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today