Inconel 718 Socket Weld Forged Fittings

Inconel 718 Socket Weld Forged Fittings

Inconel 718 Socket Weld 90 Deg. Elbow, Inconel 718 Socket Weld Tee, UNS N07718 Socket Weld Cross, DIN NR. 2.4668 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the finest supplier and exporter of Inconel 718 Socket Weld Forged Fittings, which has excellent weldability. Inconel 718 Forged Socket Weld Elbow has an excellent creep – rupture strength at temperatures up to 700 Degree C (1300 Degree F). Inconel 718 Forged Socket Weld Tee is age hardenable and may be welded in fully aged condition, along with having excellent oxidation resistance up to 1800 degrees F (980 degrees C). We manufacture Inconel 718 Socket Weld Cap and Inconel Socket Weld Cross based on the specifications and requirements of our customers. The rust-free, high durability and hardness offered by our products make it the best selling in the global market.

Inconel 718 Forged Socket Weld Cap can withstand severe mechanical stresses and strains in extreme environments while remaining stable, corrosion and creep resistant. It has been used for jet engine and high – speed airframe parts such as wheels, spacers, buckets, and Inconel 718 Forged Socket Weld Coupling temperature bolts and fasteners. The Inconel 718 Socket Weld Tee and Inconel 718 Socket Weld Elbow are finely finished to ensure flawlessness. They offer high malleability and resistance towards climatic causes of metal degradation. On the other hand, Inconel 718 Socket Weld Reducer is designed to meet the standards of the national and international markets.

Inconel 718 Socket Weld Cap, Inconel 718 Socket Weld Bend, Inconel 718 Socket Weld Cross, Inconel 718 Socket Weld Bushing, UNS N07718 Socket Weld Coupling, ASTM B564 Inconel 718 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 718 Socket Weld Forged Fittings Specifications

Grade Inconel Alloy 718 | UNS N07718
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 7180 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Inconel 718
UNS N07718
WERKSTOFF NR. 2.4668

Inconel 718 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cu Ni Fe
Inconel 718 0.08 max 0.35 max 0.35 max – 0.015 max 17 – 21 0.30 max 50.0-55.0 –

Inconel 718 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.2 g/cm3 1350 °C (2460 °F) Psi –1,35,000 , MPa – 930 Psi – 75,000 , MPa – 482 45 %

Other Types of Inconel 718 Socket Weld Threaded Forged Fittings

  • Inconel 718 Socket Weld Forged Elbow Supplier in UAE
  • Inconel 718 Socket Weld Equal Tee Manufacturer in India
  • Inconel 718 Socket Weld Cross
  • Inconel 718 Socket Weld Union
  • UNS N07718 Socket Weld Plug
  • UNS N07718 Socket Weld Hex Plug
  • DIN NR. 2.4668 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4668 Socket Weld Bushing
  • Inconel 718 Socket Weld Lateral Tee
  • Inconel 718 Socket Weld Cross
  • Inconel 718 Socket Weld Coupling Exporter in Russia
  • Inconel 718 Socket Weld Tees
  • UNS N07718 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N07718 Socket Weld 90 deg Elbow
  • DIN NR. 2.4668 Socket Weld Cap in Qatar
  • DIN NR. 2.4668 Socket Weld Bend Flanges
  • Inconel 718 Socket Weld Union
  • Inconel 718 Socket Weld Bushing
  • Inconel 718 Socket Weld Lateral Tee
  • Inconel 718 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 718 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 718 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today