Inconel 625 Socket Weld Forged Fittings

Inconel 625 Socket Weld Forged Fittings

Inconel 625 Socket Weld 90 Deg. Elbow, Inconel 625 Socket Weld Tee, UNS N06625 Socket Weld Cross, DIN NR. 2.4856 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the finest supplier and exporter of Inconel Alloy 625 Socket Weld Forged Fittings, which has excellent weldability. Rapid changes in temperature (which are common in heat treat applications) are not as much of an issue for Inconel 625 Socket Weld Elbow Forged Fittings. Some typical applications for Inconel 625 Socket Weld Tee Forged Fittings have included heat shields and furnace hardware. Inconel 625 Socket Weld Cap Forged Fittings has excellent fabricability and outstanding corrosion resistance. Inconel 625 Socket Weld Cross Forged Fittings is especially resistant to pitting and crevice corrosion. Inconel 625 Socket Weld Coupling Forged Fittingsis good for sea water applications.

Inconel 625 Socket Weld Union Forged Fittings is used for pressure vessels in a temperature range from -196 Degree C to 450 Degree C. Inconel 625 Socket Weld Plug Forged Fittings has ability to withstand high stress and a wide range of temperatures, both in and out of water. Inconel 625 Socket Weld Lateral Tee Forged Fittings acts with the molybdenum to stiffen the alloy’s matrix. Nickel Alloy 625 Socket Weld Forged Fittings allows maintaining high strength and toughness at temperatures ranging from cryogenic up to 2000 Degree F (1093 Degree C). Inconel UNS N06625 Socket Weld Forged Fittings has outstanding resistance to crevice corrosion, pitting, and inter-crystalline corrosion. Inconel WNR 2.4856 Socket Weld Forged Fittings has highly alloyed composition also provides a significant level of general corrosion resistance.

Inconel 625 Socket Weld Cap, Inconel 625 Socket Weld Bend, Inconel 625 Socket Weld Cross, Inconel 625 Socket Weld Bushing, UNS N06625 Socket Weld Coupling, ASTM B564 Inconel 625 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 625 Socket Weld Forged Fittings Specifications

Grade Inconel Alloy 625 | UNS N06625
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 6250 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Inconel 625
UNS N06625
GOST ХН75МБТЮ
BS NA 21
AFNOR NC22DNB4M
JIS NCF 625
EN NiCr22Mo9Nb
WERKSTOFF NR. 2.4856
OR ЭИ602

Inconel 625 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cu Ni Fe
Inconel 625 0.10 max 0.50 max 0.5 max – 0.015 max 20.0 – 23.0 – 58 min 5.0 max

Inconel 625 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.4 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 517 42.5 %

Other Types of Inconel 625 Socket Weld Threaded Forged Fittings

  • Inconel 625 Socket Weld Forged Elbow Supplier in UAE
  • Inconel 625 Socket Weld Equal Tee Manufacturer in India
  • Inconel 625 Socket Weld Cross
  • Inconel 625 Socket Weld Union
  • UNS N06625 Socket Weld Plug
  • UNS N06625 Socket Weld Hex Plug
  • DIN NR. 2.4856 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4856 Socket Weld Bushing
  • Inconel 625 Socket Weld Lateral Tee
  • Inconel 625 Socket Weld Cross
  • Inconel 625 Socket Weld Coupling Exporter in Russia
  • Inconel 625 Socket Weld Tees
  • UNS N06625 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N06625 Socket Weld 90 deg Elbow
  • DIN NR. 2.4856 Socket Weld Cap in Qatar
  • DIN NR. 2.4856 Socket Weld Bend Flanges
  • NiCr22Mo9Nb Socket Weld Union
  • NC22DNB4M Socket Weld Bushing
  • ХН75МБТЮ Socket Weld Lateral Tee
  • Inconel 625 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 625 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 625 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today