Incoloy 825 Socket Weld Forged Fittings

Incoloy 825 Socket Weld Forged Fittings

Incoloy 825 Socket Weld 90 Deg. Elbow, Incoloy 825 Socket Weld Tee, UNS N08825 Socket Weld Cross, DIN NR. 2.4858 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the leading supplier and distributor of Inconel Alloy 825Socket Weld Forged Fittings, which helps to avoid stress-corrosion cracking. Inconel 825 Socket Weld Elbow Forged Fittings has excellent resistance to stress corrosion cracking. Inconel 825 Socket Weld Tee Forged Fittings has improved resistance to aqueous corrosion. Inconel 825 Socket Weld Cap Forged Fittings has crevice corrosion, stress- corrosion cracking and intergranular corrosion. If exposed for long times to the sensitive temperature range 1200 Degree F – 1400 Degree F, Inconel 825 Socket Weld Cross Forged Fittings may exhibit severe inter-granular corrosion in certain very aggressive environments.

Inconel 825 Socket Weld Coupling Forged Fittings gives superb resistance to reducing environments such as those containing sulfuric and phosphoric acids. Inconel 825 Socket Weld Union Forged Fittings is alloying with enhancing elements provides added resistance to chemical and environmental corrosion, as well as physical deterioration, such as surface pitting and cracking. Inconel 825 Socket Weld Plug Forged Fittings has excellent resistance to both reducing and oxidizing acids, to SCC. The levels of molybdenum and copper enable Inconel 825 Socket Weld Lateral Tee Forged Fittings to resist reducing agents and acids. The molybdenum in Inconel UNS N08825 Socket Weld Forged Fittings also aids resistanceto pitting and crevice corrosion. The fabrication of Inconel WNR 2.4858 Socket Weld Forged Fittings is typical of nickel-base alloys, with material being readily formable and weldable by a variety of techniques.

Incoloy 825 Socket Weld Cap, Incoloy 825 Socket Weld Bend, Incoloy 825 Socket Weld Cross, Incoloy 825 Socket Weld Bushing, UNS N08825 Socket Weld Coupling, ASTM B564 Incoloy 825 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Incoloy 825 Socket Weld Forged Fittings Specifications

Grade Incoloy 825 | UNS N08825
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 8250 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Incoloy 825
UNS N08825
GOST ЭП703
AFNOR NFE30C20DUM
BS NA 16
JIS NCF 825
EN NiCr21Mo
WERKSTOFF NR. 2.4858
OR XH38BT

Incoloy 825 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si Al S Cr Cu Ni Fe
Incoloy 825 0.05 max 1.0 max 0.5 max 0.02 0.03 max 19.50-23.50 1.50-3.00 30.0-35.0 22 min

Incoloy 825 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.14 g/cm3 1400 °C (2550 °F) Psi – 80,000 , MPa – 550 Psi – 32,000 , MPa – 220 30 %

Other Types of Incoloy 825 Socket Weld Threaded Forged Fittings

  • Incoloy 825 Socket Weld Forged Elbow Supplier in UAE
  • Incoloy 825 Socket Weld Equal Tee Manufacturer in India
  • Incoloy 825 Socket Weld Cross
  • Incoloy 825 Socket Weld Union
  • UNS N08825 Socket Weld Plug
  • UNS N08825 Socket Weld Hex Plug
  • DIN NR. 2.4858 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4858 Socket Weld Bushing
  • Incoloy 825 Socket Weld Lateral Tee
  • Incoloy 825 Socket Weld Cross
  • Incoloy 825 Socket Weld Coupling Exporter in Russia
  • Incoloy 825 Socket Weld Tees
  • UNS N08825 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N08825 Socket Weld 90 deg Elbow
  • DIN NR. 2.4858 Socket Weld Cap in Qatar
  • DIN NR. 2.4858 Socket Weld Bend Flanges
  • NiCr21Mo Socket Weld Union
  • NFE30C20DUM Socket Weld Bushing
  • ЭП703 Socket Weld Lateral Tee
  • Incoloy 825 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Incoloy 825 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Incoloy 825 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today