Nickel Alloy 201 Socket Weld Forged Fittings

Nickel Alloy 201 Socket Weld Forged Fittings

Nickel Alloy 201 Socket Weld 90 Deg. Elbow, Nickel Alloy 201 Socket Weld Tee, UNS N02201 Socket Weld Cross, DIN NR. 2.4068 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the finest exporters of Nickel 201 Socket Weld Forged Fittings in India, which is generally used for reactors and vessels. Nickel 201 Socket Weld Elbow Forged Fittings is used for chemical corrosion resistance in caustic solutions. Nickel 201 Socket Weld Tee Forged Fittings is highly resistant to corrosion by neutral and alkaline salt solutions, fluorine and chlorine. Nickel 201 Socket Weld Cap Forged Fittings can also be used under oxidizing conditions when a passive oxide film is formed. Nickel 201 Socket Weld Coupling Forged Fittings is often used in food manufacturing such as handling of cooling brine, fruit juices and fatty acids due to the material’s resistance against acids.

Nickel 201 Socket Weld Cross Forged Fittings is resistant to all dry gases at room temperature and in dry chlorine and hydrogen chloride may be used in temperatures up to 550 Degree C. Nickel 201 Socket Weld Lateral Tee Forged Fittings has a low hardness and good ductility and malleability. Nickel 201 Socket Weld Union Forged Fittings has excellent corrosion resistance to distilled and natural waters. Nickel 201 Socket Weld Plug Forged Fittings is as well used for lead in wires for heating elements, and battery connections/terminals. Heat treatment of Nickel UNS N02201 Socket Weld Forged Fittings is normally performed at the temperature range from 760 Degree C to 1050 Degree C followed by being quenched in water or rapidly cooled by other means.

Nickel Alloy 201 Socket Weld Cap, Nickel Alloy 201 Socket Weld Bend, Nickel 201 Socket Weld Cross, Nickel 201 Socket Weld Bushing, UNS N02201 Socket Weld Coupling, ASTM B564 Nickel 201 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Nickel 201 Socket Weld Forged Fittings Specifications

Grade Nickel Alloy 201 | UNS N02201
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2010 LBS, 3000 LBS, 2010 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Nickel 201
UNS N02201
BS NA 12
AFNOR -
GOST НП-2
WERKSTOFF NR. 2.4068
JIS NW 2201
EN LC-Ni 99

Nickel 201 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cu Mo Ni Fe
Nickel 201 0.02 max 0.35 max 0.35 max – 0.01 max 0.25 max – 99.00 min 0.40 max

Nickel 201 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.9 g/cm3 1446 °C (2635 °F) Psi – 67000 , MPa – 462 Psi – 21500 , MPa – 148 45 %

Other Types of Nickel 201 Socket Weld Threaded Forged Fittings

  • Nickel 201 Socket Weld Forged Elbow Supplier in UAE
  • Nickel 201 Socket Weld Equal Tee Manufacturer in India
  • Nickel 201 Socket Weld Cross
  • Nickel 201 Socket Weld Union
  • UNS N02201 Socket Weld Plug
  • UNS N02201 Socket Weld Hex Plug
  • DIN NR. 2.4068 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4068 Socket Weld Bushing
  • Nickel 201 Socket Weld Lateral Tee
  • Nickel 201 Socket Weld Cross
  • Nickel 201 Socket Weld Tees
  • UNS N02201 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N02201 Socket Weld 90 deg Elbow
  • DIN NR. 2.4068 Socket Weld Cap in Qatar
  • DIN NR. 2.4068 Socket Weld Bend Flanges
  • Nickel 201 Socket Weld Union
  • Nickel 201 Socket Weld Bushing
  • Nickel 201 Socket Weld Lateral Tee
  • Nickel 201 Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Nickel 201 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Nickel 201 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today