Hastelloy X Socket Weld Forged Fittings

Hastelloy X Socket Weld Forged Fittings

Hastelloy X Socket Weld 90 Deg. Elbow, Hastelloy X Socket Weld Tee, UNS N10665 Socket Weld Cross, DIN NR. 2.4617 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is a known supplier and manufacturer of Hastelloy Alloy X Socket Weld Forged Fittings, which may be forged or otherwise hot-worked. Hastelloy X Socket Weld Elbow Forged Fittings is used for fans, roller hearths and support members in industrial furnaces. Hastelloy X Socket Weld Tee Forged Fittings has high degree of oxidation resistance up to 2200 Degree F. Hastelloy X Socket Weld Cap Forged Fittings is suitable for use in applications at temperature limits about 1200 Degree C or 2200 Degree F. Hastelloy X Socket Weld Coupling Forged Fittings is often used for Gas turbine engines and Industrial furnaces. Hastelloy X Socket Weld Cross Forged Fittingsis suitable for petrochemical processing equipment and all types of forming and welding.

Hastelloy X Socket Weld Union Forged Fittings is also used in industrial furnace applications, and in the chemical process industry. Hastelloy X Socket Weld Plug Forged Fittings has high strength up to 1500 Degree F (816 Degree C). Hastelloy X Socket Weld Lateral Tee Forged Fittings has good resistance to oxidizing, reducing and neutral atmospheres encountered in furnace and jet engine operations up to 1204 Degree C. Hastelloy UNS N06002 Socket Weld Forged Fittings is a nickel base alloy that possesses exceptional strength and oxidation resistance up to 2200 Degree F. Hastelloy WNR 2.4665 Socket Weld Forged Fittings can be welded by bothmanual and automatic methodsincluding gastungsten arc (TIG), shielded metal arc(covered electrodes), and gasmetal arc (MIG).

Hastelloy X Socket Weld Cap, Hastelloy X Socket Weld Bend, Hastelloy X Socket Weld Cross, Hastelloy X Socket Weld Bushing, UNS N10665 Socket Weld Coupling, ASTM B564 Hastelloy X Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Hastelloy X Socket Weld Forged Fittings Specifications

Grade Hastelloy X | UNS N06002
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, X0 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Hastelloy X
UNS N06002
WERKSTOFF NR. -

Hastelloy X Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Co Mo Ni Fe Cr
Hastelloy X 0.05 – 0.15 1.00 max 1.00 max 0.04 max 0.03 max 0.50 – 2.50 8.00-10.00 Balance 17.00 – 20.00 20.50-23.00

Hastelloy X Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.22 g/cm³ 1355°C 655 MPa 240 MPa 35 %

Other Types of Hastelloy X Socket Weld Threaded Forged Fittings

  • Hastelloy X Socket Weld Forged Elbow Supplier in UAE
  • Hastelloy X Socket Weld Equal Tee Manufacturer in India
  • Hastelloy X Socket Weld Cross
  • Hastelloy X Socket Weld Union
  • UNS N10665 Socket Weld Plug
  • UNS N10665 Socket Weld Hex Plug
  • DIN NR. 2.4617 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4617 Socket Weld Bushing
  • Hastelloy X Socket Weld Lateral Tee
  • Hastelloy X Socket Weld Cross
  • Hastelloy X Socket Weld Tees
  • UNS N10665 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N10665 Socket Weld 90 deg Elbow
  • DIN NR. 2.4617 Socket Weld Cap in Qatar
  • DIN NR. 2.4617 Socket Weld Bend Flanges
  • Hastelloy X Socket Weld Union
  • Hastelloy X Socket Weld Bushing
  • Hastelloy X Socket Weld Lateral Tee
  • Hastelloy X Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Hastelloy X Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Hastelloy X Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today