Hastelloy C276 Socket Weld Forged Fittings

Hastelloy C276 Socket Weld Forged Fittings

Hastelloy C276 Socket Weld 90 Deg. Elbow, Hastelloy C276 Socket Weld Tee, UNS N10276 Socket Weld Cross, DIN NR. 2.4819 Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is a known supplier and exporter of Hastelloy Alloy C276 Socket Weld Forged Fittings, which might otherwise oxidize the metal. Low carbon content means Hastelloy C276 Socket Weld Elbow Forged Fittings is resistant to the formation of grain boundary precipitates in the heat-affected zone. Chromium in Hastelloy C276 Socket Weld Tee Forged Fittings conveys resistance to oxidizing media. Hastelloy C276 Socket Weld Cap Forged Fittingsis ductile, easy to weld and form, and possesses exceptional resistance to SCC in chloride-bearing solutions. Hastelloy C276 Socket Weld Coupling Forged Fittings has excellent resistance to pitting, SCC and oxidizing atmospheres up to 1900 Degree F. Industries where Hastelloy C276 Socket Weld Cross Forged Fittings can be utilized are petrochemical and chemical processing.

Hastelloy C276 Socket Weld Union Forged Fittings is used for oil and gas, pharmaceutical, power generation, pulp and paper production and waste water treatment. In chemical processing, Hastelloy C276 Socket Weld Plug Forged Fittings is used for components including heat exchangers and reaction vessels. The formation of embrittling high temperature precipitates in Hastelloy C276 Socket Weld Lateral Tee Forged Fittings will eventually occur. Hastelloy C276 Socket Weld Bushing Forged Fittings can operate in oxidizing atmospheres up to 1900 Degree F (1038 Degree C). Hastelloy C276 Socket Weld Hex Plus Forged Fittings has resisted the formation of grain boundary precipitates in the weld heat-affected zone. Hastelloy UNS N10276 Socket Weld Forged Fittings with stands the corrosive effects of hypochlorite, wet chlorine gas and chlorine dioxide.

Hastelloy C276 Socket Weld Cap, Hastelloy C276 Socket Weld Bend, Hastelloy C276 Socket Weld Cross, Hastelloy C276 Socket Weld Bushing, UNS N10276 Socket Weld Coupling, ASTM B564 Hastelloy C276 Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Hastelloy C276 Socket Weld Forged Fittings Specifications

Grade Hastelloy C276 | UNS N10276
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, C2760 LBS, 9000 LBS
Form Socket weld 45 deg Elbow, Socket weld 90 deg Elbow, Socket weld Tee, Socket weld Cross, Socket weld Cap, Socket weld Bend, Socket weld Coupling, Socket weld Union , Socket weld Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Hastelloy C276
EN NiMo16Cr15W
UNS N10276
OR ЭП760
JIS NW 0276
GOST ХН65МВУ
AFNOR NFE30C20DUM
WERKSTOFF NR. 2.4819
BS -

Hastelloy C276 Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Co Mo Ni Fe Cr
Hastelloy C276 0.10 max 1.00 max 0.08 max 0.04 max 0.03 max 2.50 max 15-17  50.99 min* 4.00 – 7.00 14.50-16.50

Hastelloy C276 Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.89 g/cm3 1370 °C (2500 °F) Psi – 1,15,000 , MPa – 790 Psi – 52000 , MPa – 355 40 %

Other Types of Hastelloy C276 Socket Weld Threaded Forged Fittings

  • Hastelloy C276 Socket Weld Forged Elbow Supplier in UAE
  • Hastelloy C276 Socket Weld Equal Tee Manufacturer in India
  • Hastelloy C276 Socket Weld Cross
  • Hastelloy C276 Socket Weld Union
  • UNS N10276 Socket Weld Plug
  • UNS N10276 Socket Weld Hex Plug
  • DIN NR. 2.4819 45 Deg Socket Weld Elbow Distributors
  • DIN NR. 2.4819 Socket Weld Bushing
  • Hastelloy C276 Socket Weld Lateral Tee
  • Hastelloy C276 Socket Weld Cross
  • Hastelloy C276 Socket Weld Tees
  • UNS N10276 45 deg Socket Weld Elbow Supplier in Poland
  • UNS N10276 Socket Weld 90 deg Elbow
  • DIN NR. 2.4819 Socket Weld Cap in Qatar
  • DIN NR. 2.4819 Socket Weld Bend Flanges
  • Hastelloy C276 Socket Weld Union
  • Hastelloy C276 Socket Weld Bushing
  • ХН65МВУ Socket Weld Lateral Tee
  • NiMo16Cr15W Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Hastelloy C276 Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Hastelloy C276 Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today