Stainless Steel 347 / 347H Socket Weld Forged Fittings

Stainless Steel 347 / 347H Socket Weld Forged Fittings

Stainless Steel 347 Socket Weld 90 Deg. Elbow, UNS S34700 / S34709 Socket Weld Tee, DIN NR. 1.4550 / 1.4961 Socket Weld Cross, SS 347H Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the prominent supplying and distributing firm of Stainless Steel 347 / 347H Socket Weld Forged Fittings, which have a stronger affinity for carbon than chromium. Stainless Steel 347 Socket Weld Elbow Forged Fittings has the resulting columbium carbide that is more stable and insoluble than the titanium carbide. Stainless Steel 347H Socket Weld Tee Forged Fittings are also used for heavy-duty exhaust systems and manifolds. Stainless Steel 347 Socket Weld Cross Forged Fittings is used for heavy welded equipment when annealing is not possible. Stainless Steel 347H Socket Weld Cap Forged Fittings can be welded using most of the resistance and fusion methods.

Stainless Steel 347 Socket Weld Coupling Forged Fittings is used in strongly oxidizing environments as a result of the addition of columbium (niobium) and tantalum. Stainless Steel 347H Socket Weld Union Forged Fittings also possesses good low temperature toughness. Stainless Steel 347Socket Weld Plug Forged Fittingsis often used in High temperature gaskets and Rocket engine parts. Stainless Steel UNS S34700 Socket Weld Forged Fittings may also be used for exposures where sensitization and inter-granular corrosion are of concern. Stainless Steel UNS S34709 Socket Weld Forged Fittings has high temperature oxidation resistance, which is useful to 1500 Degree F. The use of a higher alloyed filler metal like Stainless Steel 347H Socket Weld Lateral Tee Forged Fittings can be necessary due to the cast structure of the weld metal.

Stainless Steel 347 Socket Weld Cap, Stainless Steel 347H Socket Weld Bend, SS 347 Socket Weld Cross, UNS S34700 / S34709 Socket Weld Bushing, DIN NR. 1.4550 / 1.4961 Socket Weld Coupling, Stainless Steel 347H Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 347 / 347H Socket Weld Forged Fittings Specifications

Grade SS 347 | Stainless Steel 347 | UNS S34700
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee.
Type Socket Weld Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 347 1.4550 S34700 SUS 347 – 08Ch18N12B – X6CrNiNb18-10

Stainless Steel 347 / 347H Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cb Ni Fe
SS 347 0.08 max 2 max 1.0 max 0.045 max 0.030 max 17 – 20 10xC – 1.10 9 – 13 62.74 min

Stainless Steel 347 / 347H Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.0 g/cm3 1454 °C (2650 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 347 / 347H Socket Weld Threaded Forged Fittings

  • Stainless Steel 347 Socket Weld Forged Elbow Supplier in UAE
  • SS 347H Socket Weld Equal Tee Manufacturer in India
  • SS 347 Socket Weld Cross
  • UNS S34700 / S34709 Socket Weld Union
  • UNS S34700 / S34709 Socket Weld Plug
  • DIN NR. 1.4550 / 1.4961 Socket Weld Hex Plug
  • DIN NR. 1.4550 / 1.4961 45 Deg Socket Weld Elbow Distributors
  • Stainless Steel 347 Socket Weld Bushing
  • Stainless Steel 347H Socket Weld Lateral Tee
  • SUS 347 Socket Weld Cross
  • Stainless Steel 347 Socket Weld Coupling Exporter in Russia
  • Stainless Steel 347H Socket Weld Tees
  • UNS S34700 / S34709 45 deg Socket Weld Elbow Supplier in Poland
  • UNS S34700 / S34709 Socket Weld 90 deg Elbow
  • DIN NR. 1.4550 / 1.4961 Socket Weld Cap in Qatar
  • DIN NR. 1.4550 / 1.4961 Socket Weld Bend Flanges
  • SS 347H Socket Weld Union
  • X6CrNiNb18-10 Socket Weld Bushing
  • 08Ch18N12B Socket Weld Lateral Tee
  • SUS 347H Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 347 / 347H Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 347 / 347H Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today