Stainless Steel 317 / 317L Threaded Forged Fittings

Stainless Steel 317 / 317L Threaded Forged Fittings

Stainless Steel 317 Socket Weld 90 Deg. Elbow, UNS S31700 / S31703 Socket Weld Tee, DIN NR. 1.4449 / 1.4438 Socket Weld Cross, SS 317L Socket Weld Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the leading manufacturing and supplying firm of Stainless Steel 317 / 317L Socket Weld Forged Fittings, which is often used in pulp and paper applications. Stainless Steel 317 Socket Weld Forged Fittings has somewhat superior corrosion resistance, particularly to pitting, due to its higher molybdenum content. Stainless Steel 317L Socket Weld Elbow Forged Fittings guarantees an increased resistance to chemical attack when compared with chromium-nickel-molybdenum austenitic steels. The high levels of these elements assure Stainless Steel 317 Socket Weld Tee Forged Fittings has superior chloride pitting and general corrosion resistance to the conventional alloys. Stainless Steel 317L Socket Weld Cross Forged Fittings has lower carbon content that leads to resistance to sensitization when welded.

Stainless Steel 317 Socket Weld Cap Forged Fittings is used in nuclear fueled power generation stations. Stainless Steel 317L Socket Weld Coupling Forged Fittings has good corrosion resistance and mechanical properties. Oxyacetylene welding in Stainless Steel 317 Socket Weld Union Forged Fittings should be avoided. Stainless Steel 317L Socket Weld Plug Forged Fittings has high strength, corrosion resistance, and high concentrations of nickel and chromium. Hardenability of Stainless Steel UNS S31700Socket Weld Forged Fittings will be reduced if constant feeds and low speeds are used. Stainless Steel UNS S31703 Socket Weld Forged Fitting provides the excellent fabricability and formability which are typical of the austenitic alloys.

Stainless Steel 317 Socket Weld Cap, Stainless Steel 317L Socket Weld Bend, SS 317 Socket Weld Cross, UNS S31700 / S31703 Socket Weld Bushing, DIN NR. 1.4449 / 1.4438 Socket Weld Coupling, Stainless Steel 317L Socket Weld Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 317 / 317L Socket Weld Forged Fittings Specifications

Grade SS 317 | Stainless Steel 317 | UNS S31700
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Socket Weld Elbow, Socket Weld Tee, Socket Weld Cross, Socket Weld Cap, Socket Weld Coupling, Socket Weld Union , Socket Weld Plug, Socket Weld Lateral Tee.
Type Socket Weld Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 317 1.4449 S31700 SUS 317
SS 317L 1.4438 S31703 SUS 317L  – – –  X2CrNiMo18-15-4

Stainless Steel 317 / 317L Socket Weld Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
SS 317 0.08 max 2 max 1.0max 0.045 max 0.030 max 18 – 20 3.0-4.0 11.0-15.0 57.845 min
SS 317L 0.035 max 2 max 1.0max 0.045 max 0.030 max 18 – 20 3.0-4.0 11.0-15.0 57.89 min

Stainless Steel 317 / 317L Socket Weld Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.9 g/cm3 1400 °C (2550 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 317 / 317L Socket Weld Threaded Forged Fittings

  • Stainless Steel 317 Socket Weld Forged Elbow Supplier in UAE
  • SS 317L Socket Weld Equal Tee Manufacturer in India
  • SS 317 Socket Weld Cross
  • UNS S31700 / S31703 Socket Weld Union
  • UNS S31700 / S31703 Socket Weld Plug
  • DIN NR. 1.4449 / 1.4438 Socket Weld Hex Plug
  • DIN NR. 1.4449 / 1.4438 45 Deg Socket Weld Elbow Distributors
  • Stainless Steel 317 Socket Weld Bushing
  • Stainless Steel 317L Socket Weld Lateral Tee
  • SUS 317 Socket Weld Cross
  • Stainless Steel 317 Socket Weld Coupling Exporter in Russia
  • Stainless Steel 317L Socket Weld Tees
  • UNS S31700 / S31703 45 deg Socket Weld Elbow Supplier in Poland
  • UNS S31700 / S31703 Socket Weld 90 deg Elbow
  • DIN NR. 1.4449 / 1.4438 Socket Weld Cap in Qatar
  • DIN NR. 1.4449 / 1.4438 Socket Weld Bend Flanges
  • SS 317L Socket Weld Union
  • X2CrNiMo18-15-4 Socket Weld Bushing
  • SUS 317 Socket Weld Lateral Tee
  • SUS 317L Socket Weld Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 317 / 317L Socket Weld Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 317 / 317L Socket Weld Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today