API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe

API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe

API 5l x42 PSL1 Welded Pipes, API 5l x42 PSL2 Pipes, API 5L X42 PSL 2 Seamless Pipes, API 5l x42 PSL1 Seamless Pipes, API 5l x42 PSL2 LSAW Pipes Manufacturer in Mumbai,India.

Nickel Super Alloys is a well-known firm that manufactures and suppliers API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe, which are easily available at industry leading rates.API 5L X42 PSL 1 Seamless Pipesis manufactured by our authentic expert as per the current technological advancement in strict adherence to the set industry norms and is quality tested.Meeting the needs of customers as an exporter,trader, and supplier, we are betrothed in presenting API 5L X42 PSL 2Welded Pipes, which is processed utilizing premium quality steel & other material needed coupled with sophisticated technology. Offered range of API 5L X42 PSL 1 EFW Pipesis widely demanded amongst the clients for its creative patterns and different designs.

We manufacture API 5L X42 PSL 2 ERW Pipesby using excellent quality of raw material.Our API 5L X42 PSL 1 Round Pipesare manufactured from optimum quality components and following world class standards.Apart from this, API 5L X42 PSL 2Square Pipesis used in chemical industry, petroleum, oil,electric power, gas, and construction fields.We offer collection of supreme quality API 5L X42 PSL 1 Rectangular Pipeswith our expertise and experience in the field of manufacturing.Optimum grade ofAPI 5L X42 PSL 2Electropolish Pipesare utilized for the production process, which uphold consistency in the quality of the joint.

API 5L X42 PSL 1 Seamless Steel Pipes, API 5L X42 PSL 2 SAW Pipes, API 5l PSL 2 welded Pipe, API 5L X42 PSL 2 Welded Pipes, API 5L X42 PSL1 ERW Pipes, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe Specifications

Grade API 5L X42 PSL 1 (American Petroleum Institute)
API 5L X42 PSL1 ERW Pipe Size 1/2" NB - 24" NB
API 5L X42 PSL1 SAW/LSAW Pipe Size 16" NB - 100" NB
API 5L X42 PSL1 Seamless Pipe Size 1/2" NB - 60" NB
Form Round, Square, Rectangular, Hydraulic Etc
Type Seamless / ERW / Welded / Fabricated / EFW
Length Single Random, Double Random & Cut Length.
Length Min 3 Meters, Max18 Meters, or according to customer's requirement.

API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe Chemical Composition

Mass fraction, based upon heat and product analysis a
SEAMLESS PIPE
C Mn P V Nb Ti
maxb maxb max. max. max. max. max.
0.28 1.20 0.030 0.030 c,d c,d d
WELDED PIPE
0.26 1.20 0.030 0.030 c,d c,d d

API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe Mechanical Properties

Y.S T.S ELONGATION
Mpa(psi) Mpa(psi)
min min min
245(35 500) 415(60 200) 28%

Other Types of API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe

  • PSL1 API 5L X42 PSL1 Line Piping Supplier in UAE
  • API 5L X42 PSL 2 Welded Pipes Manufacturer in India
  • API 5L PSL1 X42 EFW Pipes
  • Carbon Steel API 5L X42 PSL2 ERW Pipes
  • API 5L X42 PSL 1 Seamless Pipes
  • API 5L X42 PSL 2 Pipes
  • API 5L X42 PSL2 Seamless Pipes Distributors
  • API 5L X42 PSL 1 Welded Pipes
  • API 5L X42 PSL 2 Welded Pipes
  • API 5L X42 PSL 1 Seamless Steel Pipes
  • API 5L X42 PSL 2 Seamless Pipes Exporter in Russia
  • Carbon Steel API 5L PSL1 Seamless Pipes
  • API 5L X42 PSL 2 Line Pipe Supplier in Poland
  • API 5L Grade X42 PSL1 Seamless Tubes
  • Carbon Steel X42 PSL2 Welded Pipes in Qatar
  • API 5L Grade X42 PSL1 Pipes
  • Carbon Steel API 5L PSL 2 Pipes
  • API 5L Grade X42 PSL 1 Welded Pipes
  • API 5L X42 PSL 2 LSAW Pipe
  • PSL1 API 5L X42 PSL1 Seamless Line Pipe

Countries We Export to

Nickel Super Alloys manufactures and exports ​API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports API 5L X42 PSL 1 / API 5L X42 PSL 2 Pipe to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today