Copper Nickel 70/30 Pipe Fittings

Copper Nickel 70/30 Pipe Fittings

70/30 Copper Nickel Long & Short Radius Elbow, Cupro Nickel 10D Pipe Bend, ANSI B16.9 Cu-Ni 70/30 Welded Buttweld Fittings, ASTM B366 Cupro Nickel 70/30 180 Degree Elbow, Cu-Ni 70/30 Pipe Bend Manufacturer in Mumbai,India.

Nickel Super Alloys is a supplier of Copper Nickel 70 / 30 Butt Weld Pipe Fittings, which is used for heat exchangers at cryogenic plants.Cupro Nickel 70 / 30 Elbow Pipe Fittings is being used in severe corrosive conditions in which service lives longer than those of other copper alloys are desired. Cu-Ni 70 / 30 Tee Pipe Fittings are often used in the marine industry due to its high electric resistance ability and corrosion while in sea water. In particular, the corrosion resistance in Copper Nickel 70 / 30 Reducer Pipe Fittings is notably improved in high-velocity waters and polluted seawater. The small iron content gives Cupro Nickel 70 / 30 Cross Pipe Fittings an extraordinary resistance to general corrosion and SCC.

Cu-Ni 70 / 30 Bend Pipe Fittings are utilized in areas where high temperatures and pressures, combined with high velocities and turbulence are serious problems.Copper Nickel 70 / 30 Stub End Pipe Fittingsis used where moderate-to-high sea water corrosion concern is present, for example, in valves, pumps, and high-pressure steam lines. Cupro Nickel 70 / 30 End Cap Pipe Fittings are resistant to SCC and has high strength. Cu-Ni 70 / 30 Dish Cap Pipe Fittings are thermally stable and possess moderate strength even when the temperature is high. Copper Nickel C71500 Pipe Fittings are recognized for its moderate formability, weldability, workability and strength.

70/30 Cupro Nickel End Cap, Cu-Ni 70-30 Equal Tee, Cupro Nickel 10D Pipe Bend, Cu-Ni UNS C71500 Equal Tee & Unequal Tee, 70/30 Short & Long Stub End, 70/30 Cu-Ni Pipe Reducer, 70/30 Cupro Nickel 180 Deg Bend Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Cupro Nickel 70/30 Pipe Fittings Specifications

Grade Copper Nickel 70/30 (C71500) Werkstoff Nr. 2.0882
Standard ASTM B122, B171, B466, B467
Dimensions ASME B16.28, ASME/ANSI B16.9, MSS-SP-43
Size 1/2" to 24" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Wall Thickness from 2 to 40 mm
Type Seamless / Welded / Fabricated

Cupro Nickel 70/30 Pipe Fittings Chemical Composition

Cu-Ni 70/30 Cu Pb Mn Fe Zn Ni
65.0 min 0.05 max 1.0 max 0.4-1.0 1 max 29 – 33

Cupro Nickel 70/30 Pipe Fittings Mechanical Properties

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
0.323 lb/in3 at 68 F 2260 F 20000 psi 50000 psi 30 %

Other Types of Cupro Nickel 70/30 Pipe Fittings

  • Cu-Ni 70-30 Buttweld Tee Supplier in UAE
  • UNS C71500 Cross Manufacturer in India
  • DIN 2.0882 Butwteld Tee
  • DIN 2.0882 45 deg.Elbow
  • Cu-Ni 70-30 Buttweld Pipe Fittings
  • Copper Nickel 70-30 Short Radius Elbow
  • Cupro Nickel 70-30 Ecentric Reducer Distributors
  • UNS C71500 Buttweld Pipe Fitting
  • ASME B16.9 Stub End
  • Cupro Nickel 70-30 Concentric Reducer
  • Cupro Nickel 70-30 Long Radius Elbow Exporter in Russia
  • Copper Nickel 70-30 U Bend
  • Cupro Nickel 70-30 Stub End Supplier in Poland
  • Cu-Ni 70-30 Short Radius Elbow
  • UNS C71500 Equal Tee in Qatar
  • Cu-Ni 70-30 End Cap
  • ASTM B122 Concentric Reducer
  • Cu-Ni 70-30 Seamless Fitting
  • Cu-Ni 70-30 180 Deg Elbow
  • Cu-Ni 70-30 Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Copper Nickel 90-10 Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Copper Nickel 90-10 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today