Nickel Alloy 200 Pipe Fittings

Nickel Alloy 200 Pipe Fittings

Nickel Alloy 200 Equal Tee, 200 Nickel Alloy End Cap, ASME SB366 Alloy 200 Long Stub, Nickel 10d Pipe Bend, Nickel 200 Pipe Fittings, 200 Nickel Alloy Reducer Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the finest manufacturers of Nickel 200 Butt Weld Pipe Fittings in India, which is commercially pure nickel. Nickel 200 Elbow Pipe Fittings is 99.6 percent pure nickel alloy, and one of the toughest metals. Applications where Nickel 200 Tee Pipe Fittings can be used include synthetic fiber production and processes where sodium hydroxide and fluorine is used. In addition, Nickel 200 Cross Pipe Fittings provides highly ductile mechanical properties across a wide temperature range. Nickel 200 Reducer Pipe Fittings can also be used in oxidizing conditions that cause the formation of a passive oxide film. Nickel 200 Bend Pipe Fittings offers outstanding corrosion resistance to caustic soda and other alkalis.

Nickel 200 Stub End Pipe Fittings has high thermal and electrical conductivities, along with low gas content and low vapor pressure. Nickel 200 End Cap Pipe Fittings is highly resistant to various reducing chemicals and is unexcelled in resistance tocaustic alkalis. Nickel 200 Dish Cap Pipe Fittings has good mechanical properties over a wide range of temperatures and excellent resistance to many corrosives. Nickel 200 Lateral Tee Pipe Fittings has good resistance to corrosion in acids and alkalis and is most useful under reducing conditions. However, the corrosion resistance of Nickel 200 Concentric Reducer Pipe Fittings is better in de-aerated acid. Nickel 200 Eccentric Reducer Pipe Fittingsis one of the world’s toughest metals and imparts a number of advantages to this material.

Nickel 200 45 Degree Elbow, DIN 2.4066 Cross, Nickel Alloy 200 Pipe Bend, ANSI B16.9 Nickel 200 Long & Short Radius Elbow, ASTM B366 200 Nickel Alloy 90 Degree Elbow, Nickel 200 Eccentric & Concentric Reducer Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Nickel 200 Pipe Fittings Specifications

Grade Nickel Alloy 200 / UNS N02200
Standard ASTM B366, ASME SB366
Dimensions ASME B16.28, ASME/ANSI B16.9, MSS-SP-43
Nickel Alloy 200 Seamless Fittings 1/2" NB - 10" NB
Nickel Alloy 200 Welded Fittings 1/2" NB - 48" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Wall Thickness from 2 to 40 mm
Type Seamless / Welded / Fabricated
Standard Nickel 200
UNS N02200
GOST НП-2
WERKSTOFF NR. 2.4066
BS NA 11
AFNOR N-100M
EN Ni 99.2
JIS NW 2200

Nickel 200 Pipe Fittings Chemical Composition

Nickel 200 Ni C Mo Mn Si Fe P S Cu Cr
99.0 min 0.15 max – 0.35 max 0.1 max 0.4 max – 0.01 max 0.25 max –

Nickel 200 Pipe Fittings Mechanical Properties

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
8.9 g/cm3 1446 °C (2635 °F) Psi – 21500 , MPa – 148 Psi – 67000 , MPa – 462 45 %

Other Types of Nickel 200 Pipe Fittings

  • Nickel 200 Buttweld Tee Supplier in UAE
  • UNS N02200 Cross Manufacturer in India
  • DIN 2.4066 Butwteld Tee
  • DIN 2.4066 45 deg.Elbow
  • Nickel 200 Buttweld Pipe Fittings
  • Nickel 200 Short Radius Elbow
  • UNS N02200 Ecentric Reducer Distributors
  • Nickel 200 Buttweld Pipe Fitting
  • ASME SB366 Stub End
  • Nickel 200 Concentric Reducer
  • Nickel 200 Long Radius Elbow Exporter in Russia
  • Nickel 200 U Bend
  • Nickel 200 Stub End Supplier in Poland
  • Nickel 200 Short Radius Elbow
  • Nickel 200 Equal Tee in Qatar
  • UNS N02200 End Cap
  • ASME SB366 Concentric Reducer
  • Nickel 200 Seamless Fitting
  • Nickel 200 180 Deg Elbow
  • Nickel 200 Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Nickel 200 Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Nickel 200 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today