Nickel Alloy 201 Pipe Fittings

Nickel Alloy 201 Pipe Fittings

Nickel Alloy 201 Long & Short Radius Elbow, Nickel Alloy DIN 2.4068 Cross 201 Nickel Alloy Reducer, ASME SB366 Alloy 201 Long Stub End, Nickel 201 190 Degree Elbow Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the finest exporters of Nickel 201 Butt Weld Pipe Fittings in India, which is available in best possible rates to our clients. Nickel Alloy 201 Elbow Pipe Fittings has the lower carbon chemistry, which is preferred for service in temperatures above 600 Degree F (315 Degree C). Nickel Alloy 201 Tee Pipe Fittings has high electrical and thermal conductivity. However, Nickel Alloy 201 Reducer Pipe Fittings does suffer from inter-granular embrittlement by sulfur compounds at temperatures above 315 Degree C. Nickel Alloy 201 Cross Pipe Fittings has good resistance to corrosion in acids and alkalis and is most useful under reducing conditions.

Nickel Alloy 201 Cap Pipe Fittings is highly resistant to various reducing chemicals and is unexcelled in resistance to caustic alkalis.Nickel Alloy 201 Bend Pipe Fittingshas good mechanical properties over a wide range of temperatures and excellent resistance to many corrosives, in particular hydroxides. Nickel Alloy 201 Stub End Pipe Fittings is used in handling and manufacturing sodium hydroxide above 300 Degree C.In particular, Nickel Alloy 201 End Cap Pipe Fittings is used as a material for caustic soda manufacturing equipment by diaphragm electrolysis method. Nickel Alloy 201 Dish Cap Pipe Fittings has good magnetostrictive properties, along with high thermal and electrical conductivity. Nickel Alloy 201 Lateral Tee Pipe Fittingsis a wrought commercially pure Nickel with a maximum carbon level of 0.02 percent.

Nickel 201 Pipe Elbow, Nickel 3D Pipe Bend, Nickel 201 Pipe Fittings, UNS N02201 Seamless Pipe Fittings, Alloy 201 Short Radius Stub End, 201 Nickel Alloy End Cap, ANSI B16.9 Nickel 201 Eccentric & Concentric Reducer Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Nickel 201 Pipe Fittings Specifications

Grade Nickel Alloy 201 / UNS N02201
Standard ASTM B366, ASME SB366
Dimensions ASME B16.28, ASME/ANSI B16.9, MSS-SP-43
Nickel Alloy 201 Seamless Fittings 1/2" NB - 10" NB
Nickel Alloy 201 Welded Fittings 1/2" NB - 48" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Wall Thickness from 2 to 40 mm
Type Seamless / Welded / Fabricated
Standard Nickel 201
UNS N02201
BS NA 12
AFNOR -
GOST НП-2
WERKSTOFF NR. 2.4068
JIS NW 2201
EN LC-Ni 99

Nickel 201 Pipe Fittings Chemical Composition

Nickel 201 Ni C Mo Mn Si Fe P S Cu Cr
Balance 0.15 max – 0.35 max 0.35 max 0.40 max – 0.01 max 0.25 max –

Nickel 201 Pipe Fittings Mechanical Properties

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
8.9 g/cm3 1446 °C (2635 °F) Psi – 21500 , MPa – 148 Psi – 67000 , MPa – 462 45 %

Other Types of Nickel 201 Pipe Fittings

  • Nickel 201 Buttweld Tee Supplier in UAE
  • UNS N02201 Cross Manufacturer in India
  • DIN 2.4602 Butwteld Tee
  • DIN 2.4602 45 deg.Elbow
  • Nickel 201 Buttweld Pipe Fittings
  • Nickel 201 Short Radius Elbow
  • UNS N02201 Ecentric Reducer Distributors
  • Nickel 201 Buttweld Pipe Fitting
  • ASME SB366 Stub End
  • Nickel 201 Concentric Reducer
  • Nickel 201 Long Radius Elbow Exporter in Russia
  • Nickel 201 U Bend
  • Nickel 201 Stub End Supplier in Poland
  • Nickel 201 Short Radius Elbow
  • Nickel 201 Equal Tee in Qatar
  • UNS N02201 End Cap
  • ASME SB366 Concentric Reducer
  • Nickel 201 Seamless Fitting
  • Nickel 201 180 Deg Elbow
  • Nickel 201 Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Nickel 201 Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Nickel 201 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today