Hastelloy B2 Pipe Fittings
ASME SB366 Alloy B2 Long Stub, Hastelloy B2 180 Deg bend, Alloy B2 Short Radius Elbow, ANSI B16.9 Hastelloy B2 Welded Buttweld Fittings, Hastelloy B2 90 Degree Elbow, Hastelloy DIN 2.4617 Cross Manufacturer in Mumbai,India.
Nickel Super Alloys is one of the known supplier and exporter of Hastelloy Alloy B2 Butt Weld Pipe Fittings, which is a solid-solution strengthened nickel alloy. Hastelloy B2 Elbow Pipe Fittings has significant resistance to reducing environments like hydrogen chloride gas and sulfuric acid. Hastelloy B2 Tee Pipe Fittingsprovides resistance to pure sulfuric acid and a number of non-oxidizing acids. Therefore, Hastelloy B2 Cross Pipe Fittings has great resistance to stress-corrosion cracking and pitting. Hastelloy B2 Reducer Pipe Fittings has significantly lower silicon,carbon and iron compared to its’ predecessor. Hastelloy B2 Stub End Pipe Fittings resists formation of grain boundary carbides in the weld HAZ. Hastelloy B2 End Cap Pipe Fittings may be used in the as-welded condition.
In many corrosion media only Tantaline shows a dramatically better cost/performance ratio than Hastelloy B2 Dish Cap Pipe Fittings. In addition, Hastelloy B2 Lateral Tee Pipe Fittings must betested under actual service conditions to determine their suitability for a particularpurpose. Hastelloy B2 Concentric Reducer Pipe Fittings has excellent resistance to pitting corrosion, SCC, and knife line and weld heat-affected zone attack. Hastelloy B2 Eccentric Reducer Pipe Fittings contain many elements in a variety of combinations designed to provide unique material properties for specific applications. Hastelloy B2 Equal Tee Pipe Fittingsis a solid solution strengthened, nickel-molybdenum alloy, typically used in extreme reducing conditions. Hastelloy B2 Unequal Tee Pipe Fittings has significant corrosion resistance to reducing environments.
ASTM B366 B2 Hastelloy Alloy 180 Degree Elbow, Hastelloy B2 Pipe Elbow, Hastelloy 3d Pipe Bend, B2 Hastelloy End Cap, B2 Hastelloy Alloy Reducer, Hastelloy UNS N10665 Seamless Pipe Fittings Suppliers in India.
Key Charactristic:
- Corrosion resistance
- Resistance to oxidation and sulfidation
- Cryogenic strength
- Resistance to abrasion and erosion
- Surface finish
- Magnetic properties
- Ductility
- Elevated temperature strength
- Stability of properties in service
- Suitability for intended fabrication techniques
Hastelloy B2 Pipe Fittings Specifications
| Grade | Hastelloy Alloy B2 / UNS N10665 |
| Standard | ASTM B366, ASME SB366 |
| Dimensions | ASME B16.28, ASME/ANSI B16.9, MSS-SP-43 |
| Hastelloy B2 Seamless Fittings | 1/2" NB - 10" NB |
| Hastelloy B2 Welded Fittings | 1/2" NB - 48" NB |
| Form | 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap |
| Schedule | SCH 5 To SCH XXS |
| Wall Thickness | from 2 to 40 mm |
| Type | Seamless / Welded / Fabricated |
| Standard | Hastelloy B2 |
| UNS | N10665 |
| WERKSTOFF NR. | 2.4617 |
Hastelloy B2 Pipe Fittings Chemical Composition
| Hastelloy B2 | Ni | C | Mo | Mn | Si | Fe | P | S | Co | Cr |
| Balance | 0.02 max | 26.0-30.0 | 1.0 max | 0.10 max | 2.0 max | 0.040 max | 0.030 max | 1.0 max | 1.0 max |
Hastelloy B2 Pipe Fittings Mechanical Properties
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
| 9.2 g/cm3 | 1370 °C (2500 °F) | Psi – 51,000, MPa – 350 | Psi -1,10,000, MPa -760 | 40 % |
Other Types of Hastelloy B2 Pipe Fittings
- Hastelloy B2 Buttweld Tee Supplier in UAE
- UNS N10665 Cross Manufacturer in India
- DIN 2.4617 Butwteld Tee
- DIN 2.4617 45 deg.Elbow
- Hastelloy B2 Buttweld Pipe Fittings
- Hastelloy B2 Short Radius Elbow
- UNS N10665 Ecentric Reducer Distributors
- Hastelloy B2 Buttweld Pipe Fitting
- ASME SB366 Stub End
- B2 Hastelloy Concentric Reducer
- Hastelloy B2 Long Radius Elbow Exporter in Russia
- Hastelloy B2 U Bend
- Hastelloy B2 Stub End Supplier in Poland
- B2 Hastelloy Short Radius Elbow
- Hastelloy B2 Equal Tee in Qatar
- UNS N10665 End Cap
- ASME SB366 Concentric Reducer
- Hastelloy B2 Seamless Fitting
- Hastelloy B2 180 Deg Elbow
- Hastelloy B2 Pipe Bends
Countries We Export to
Nickel Super Alloys manufactures and exports Hastelloy B2 Pipe Fittings to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia
Cities We Deliver to
Nickel Super Alloys manufactures and exports Hastelloy B2 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo