Hastelloy B3 Pipe & Tubes

Hastelloy B3 Pipe & Tubes

Alloy B3 Pipe & Tubes, B3 Hastelloy Pipes & Tubes, Hastelloy WERKSTOFF NR. 2.4600 Pipe & Tubes, UNS N010675 Welded Pipe & Tubes, ASME SB622 Hastelloy Pipe & Tubes Manufacturer in Mumbai,India.

Nickel Super Alloys is a known manufacturer and supplier of Hastelloy B3 Pipes and Tubes, which contains no significant chromium addition. Hastelloy B3 Seamless Pipes has excellent resistance to pitting, corrosion, and SCC. Hastelloy B3 Welded Tubes exhibits extremely high resistance to pure hydrochloric, sulfuric and hydro-bromic acids. Hastelloy B3 EFW Pipes has greatly improved structural stability compared with previous B-type alloys. Hastelloy B3 ERW Tubes gives excellent resistance to hydrochloric acid at all concentrations and temperatures from ambient to high. Hastelloy B3 Round Pipes is an additional member of the nickel-molybdenum family of alloys with excellent resistance to hydrochloric acid at all concentrations and temperatures. Hastelloy B3 Square Tubeshas great resistance to knife-line and heat-affected zone attack.

Hastelloy B3 Rectangular Pipes has a special chemistry designed to achieve a level of thermal stability greatly superior to that of its predecessors. Hastelloy B3 Electropolish Tubes belongs to the family of nickel-molybdenum alloys and has an average composition of nickel and molybdenum. Hastelloy B3 Hexagonal Pipes has poor corrosion resistance to oxidizing environments. Hastelloy B3 Hallow Tubes is resistant to HCl which led to an attack at all temperatures. The improved thermal stability of Hastelloy Bush Hex Pipes minimizes the problems associated with fabrication of B-2 alloy components. Hastelloy B3 Heat Exchanger Tubes has significantly better thermal stability, fabricability and SCC resistance.Hastelloy UNS N10675 Pipes is available in different sizes and shapes at best possible rates.

B3 Alloy Seamless Pipes & Tubes, B3 Hastelloy Hollow Pipe & Tubes, ASTM B619 Hastelloy B3 Seamless Pipes & Tubes, B3 Hastelloy Seamless Pipes & Tubes, Hastelloy B3 Hexagonal Pipe & Tubes, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Hastelloy B3 Pipe & Tubes Specifications

Grade Hastelloy B3
Standard ASTMA B622, ASTM B619 / ASME SB-622, ASME SB-619
Range 15 NB UP TO 600 NB
Hastelloy B3 Seamless Pipes 1/4" NB To 6" NB
Hastelloy B3 Welded / ERW Pipes 1" NB To 16" NB
Form Round, Square, Rectangular, Hydraulic Etc
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Length Single Random, Double Random & Cut Length.
Type Seamless / ERW / Welded / Fabricated / EFW
End Plain End, Beveled End, Treaded
Standard Hastelloy B3
UNS N10675
WERKSTOFF NR. 2.4600

Hastelloy B3 Pipe & Tubes Chemical Composition

Hastelloy B3 Ni C Mo Mn Si Fe Cu Ti Co Cr
65.0 min 0.01 max 28.5 3.0 max 0.10 max 1.5 0.20 max 0.2 max 3.0 max 1.5

Hastelloy B3 Pipe & Tubes Mechanical Properties

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
– – – – –

Other Types of Hastelloy B3 Pipe & Tubes

  • Austenitic B3 Hastelloy Pipes Supplier in UAE
  • Hastelloy B3 Seamless Pipes Manufacturer in India
  • ASTM B622 Hastelloy Capillary Tube
  • B3 Hastelloy Seamless Tubing
  • ASTM B619 Hastelloy Welded Pipes
  • SB622 Hastelloy Welded Tubes
  • Hastelloy B3 ERW Pipes Distributors
  • B3 Rectangular Seamless Pipes
  • Hastelloy B3 EFW Tubes
  • UNS N10675 Coiled Seamless Tubing
  • Hastelloy B3 Pipes Exporter in Russia
  • UNS N10675 Hastelloy Pipes
  • Alloy B3 Rectangular Pipe Supplier in Poland
  • Alloy N10675 Seamless Pipes
  • Alloy UNS N10675 Welded Pipes in Qatar
  • Alloy B3 Round Pipe
  • ASTM B619 Alloy B3 Pipe
  • Hastelloy B3 ERW Pipes
  • Alloy B3 EFW Pipe
  • Hastelloy B3 Fabricated Pipes

Countries We Export to

Nickel Super Alloys manufactures and exports ​Hastelloy B3 Pipes & Tubes​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Hastelloy B3 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today