Hastelloy C22 Flanges

Hastelloy C22 Flanges

Hastelloy UNS N06022 Pipe Flanges, Hastelloy C22 Spectacle Blind Flanges, ANSI B16.5 Alloy C22 Orifice Flange, C22 Alloy Weld Neck Flange, ASTM B564 Hastelloy C22 Threaded Flanges Manufacturer in Mumbai,India.

Nickel Super Alloys is a known exporter and supplier of Hastelloy Alloy C22 Pipe Flanges, whichcan easily be cold-worked because of its ductility. Forging should be started immediately the stock of Hastelloy C22 Slip On Raised Flanges is removed from the reheat furnace and reductions help to retain as much internal heat as possible. Hastelloy C22 Blind Raised Flangesis highly versatile: used in applications ranging from stack liners to heat exchangers. Hastelloy C22 Spectacle Blind Flanges can be applied in many kinds of chemical processing. Carbon content in Hastelloy C22 Threaded Flanges must be maintained below to minimize the formation of intermetallic phases. Hastelloy C22 Socket Weld Flanges has the ability to resist the formation of grain boundary precipitates in the heat affected zone of the weld.

Hastelloy C22 Weld Neck Flanges offers optimum resistance to environments where reducing and oxidizing conditions are encountered in process streams. Hastelloy C22 Lap Joint Flanges is very ductile andexhibits excellent weldability. Hastelloy C22 Ring Joint Type Flanges is ready to ship the most corrosion-resistant metal in its class at a moment's notice. Hastelloy C22 Spacer Flanges has exceptional resistance to a wide variety of chemical process environments, including strong oxidizers. Hastelloy C22 Long Weld Neck Flanges has excellent resistance to oxidizing aqueous media including wet chlorine and mixtures. Hastelloy C22 Nippolet Flanges is an improved alloy for use in a range of aggressive industrial environments.

Hastelloy DIN 2.4602 Socket Weld Flanges, Alloy C22 RTJ Flange, Hastelloy C22 Nippolet Flanges, Hastelloy C22 Nippo Flanges, Alloy C22 Blind Flanges, Hastelloy C22 Pipe Flanges, Hastelloy C22 Slip On Flanges Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Hastelloy C22 Flanges Specifications

Grade Hastelloy Alloy C22 / UNS N06022
Standard ASTM B564, ASME SB564
Dimensions ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44
Size 1/2" - 48" (15NB - 1200NB)
Class / Pressure Rating 150 Class, 300 Class, C22 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc.
Form Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges
Flange Face Type Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ)
Standard Hastelloy C22
UNS N06022
WERKSTOFF NR. 2.4602
JIS NW 6022
EN NiCr21Mo14W

Hastelloy C22 Flanges Chemical Composition

Grade C Mn Si S Co Ni Cr Fe Mo P
C22 0.010 max 0.50 max 0.08 max 0.02 max 2.50 max 50.015 min* 20.00 – 22.50 2.00 – 6.00 12.50 – 14.50 0.02 max

Hastelloy C22 Flanges Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Hastelloy C22 8.69 g/cm3 1399 °C (2550 °F) Psi – 1,00,000 , MPa – 690 Psi – 45000 , MPa – 310 45 %

Other Types of Hastelloy C22 Flanges

  • Hastelloy C22 Tongue & Groove Flanges Supplier in UAE
  • Hastelloy C22 Spectacle blind flanges Manufacturer in India
  • Hastelloy C22 Long Weld Neck Flanges
  • Hastelloy C22 Flat Face Flanges
  • UNS N06022 High Hub Blind Flanges
  • UNS N06022 Lap Joint Flanges
  • DIN 2.4602 Reducing Flanges Distributors
  • DIN 2.4602 Blind Flanges
  • Hastelloy C22 Slip On Flanges
  • UNS N06022 Threaded Flanges
  • Hastelloy C22 Orifice Flanges Exporter in Russia
  • Hastelloy C22 400# Forged Flanges
  • Hastelloy C22 F91 600# Plate Flanges Supplier in Poland
  • Hastelloy C22 900# Spacer Ring Flanges
  • DIN 2.4602 PN6 Nipo Flange in Qatar
  • DIN 2.4602 PN10 Nipolet Flanges
  • Hastelloy C22 Pipe Flanges
  • UNS N06022 SORF Flanges
  • Hastelloy C22 WNRF Flanges
  • Hastelloy C22 Threaded Flanges

Countries We Export to

Nickel Super Alloys manufactures and exports ​Hastelloy C22 Flanges​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Hastelloy C22 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today