Monel K500 Pipe Fittings

Monel K500 Pipe Fittings

ASME SB366 Alloy K500 Long Stub, ASTM B366 K500 Monel Alloy 90 Degree Elbow, Monel K500 Pipe Fittings, Alloy K500 Equal Tee, Monel K500 45 Degree Elbow, Monel DIN 2.4375 Cross Manufacturer in Mumbai,India.

Nickel Super Alloys is of the well-known traders of Monel Alloy K500 Butt Weld Pipe Fittings, which is exceptionally good dimensional stability. Monel K500 Elbow Pipe Fittings is resistant to corrosion and acids, and some alloys can with stand a fire in pure oxygen. Monel K500 Tee Pipe Fittings is age hardenable and good for sea water applications. Monel K500 Reducer Pipe Fittings has approximately three times the yield strength and double the tensile strength. Monel K500 Cross Pipe Fittings is a nickel-copper alloy with age hardening properties imparted by alloying additions of aluminum and titanium. Monel K500 Bend Pipe Fittings is used by heating under controlled conditions so that submicroscopic particles are precipitated throughout the matrix.

Low corrosion rates in sea water make Monel K500 Stub End Pipe Fittings suitable for marine service although pitting may occur in stagnant waters but the rate of pitting slows after initial attack. Monel K500 End Cap Pipe Fittings has many different industrial applications, some of which include pump shafts and impellers. Monel K500 Dish Cap Pipe Fittings should be quenched after forging from a temperature of 1450 Degree F (790 Degree C) minimum. Monel K500 Lateral Tee Pipe Fittings is possible, however, to develop a magnetic layer on the surface of the material during processing. By a thermal processing, Monel K500 Concentric ReducerPipe Fittingsis used to effect precipitation, typically called age hardening or aging.

Alloy K500 Short Radius Elbow, Monel 3D Pipe Bend, Monel UNS N05500 Seamless Pipe Fittings, K500 Monel Alloy End Cap, ANSI B16.9 Monel K500 Welded Buttweld Fittings, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Monel K500 Pipe Fittings Specifications

Grade Monel K500 / UNS N05500
Standard ASTM B366, ASME SB366
Dimensions ASME B16.28, ASME/ANSI B16.9, MSS-SP-43
Monel K500 Seamless Fittings 1/2" NB - 10" NB
Monel K500 Welded Fittings 1/2" NB - 48" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Wall Thickness from 2 to 40 mm
Type Seamless / Welded / Fabricated
Standard Monel K500
Werkstoff Nr. 2.4375
UNS N05500
JIS NW 5500
AFNOR -
BS -
GOST -
EN -

Monel K500 Pipe Fittings Chemical Composition

Monel K500 Ni C Al Mn Si Fe Cu S Ti Cr
63.0 min 0.25 max 2.3 – 3.15 1.5 max 0.5 max 05 – 2 27.0 – 33.0 0.010 max 0.35 – 0.85 –

Monel K500 Pipe Fittings Mechanical Properties

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
8.44 g/cm3 1350 °C (2460 °F) Psi – 1,15,000 , MPa – 790 Psi – 1,60,000 , MPa – 1100 20 %

Other Types of Monel K500 Pipe Fittings

  • Monel K500 Buttweld Tee Supplier in UAE
  • UNS N05500 Cross Manufacturer in India
  • DIN 2.4375 Butwteld Tee
  • DIN 2.4375 45 deg.Elbow
  • Monel K500 Buttweld Pipe Fittings
  • Monel K500 Short Radius Elbow
  • UNS N05500 Ecentric Reducer Distributors
  • Monel K500 Buttweld Pipe Fitting
  • ASME SB366 Stub End
  • K500 Monel Concentric Reducer
  • Monel K500 Long Radius Elbow Exporter in Russia
  • Monel K500 U Bend
  • Monel K500 Stub End Supplier in Poland
  • K500 Monel Short Radius Elbow
  • Monel K500 Equal Tee in Qatar
  • UNS N05500 End Cap
  • ASME SB366 Concentric Reducer
  • Monel K500 Seamless Fitting
  • Monel K500 180 Deg Elbow
  • Monel K500 Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Monel K500 Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Monel K500 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today