Monel K500 Pipes & Tubes

Monel K500 Pipes & Tubes

Monel K500 ASTM B165 Seamless Pipes, ASTM B 163 Round Pipes, Monel K500 Rectangular Pipes, Monel UNS N05500 ERW Pipes, Alloy K500 Capillary Tubes, Monel Alloy K500 Square Pipes Manufacturer in Mumbai,India.

Nickel Super Alloys is of the well-known traders of Monel Alloy K500 Pipes and Tubes, which is virtually nonmagnetic, even at quite low temperatures. Monel K500 Seamless Pipes is a nickel-copper alloy, precipitation hardenable through additions of aluminum and titanium. The increased properties of Monel K500 Welded Tubesa re obtained by adding aluminum and titanium to the nickel-copper base. By adding Aluminum and Titanium to Monel K500 EFW Pipes, followed by an age hardening process, this enhances the physical properties, giving the material greater strength and hardness. Resistance to hydrogen sulfide makes Monel K500 ERW Tubes useful in sour-gas environments making it extremely popular in the oil patch.

Aluminum and titanium additions, plus controlled heat treat cycles, are responsible for the added strength of Monel K500 Round Pipes. In age-hardened condition, Monel K500 Square Tubesalso has greater tendency toward stress- corrosion cracking in some environments. A useful characteristic of Monel K500 Rectangular Pipes is that it is virtually nonmagnetic, even at quite low temperatures. These Monel K500 Electropolish Tubes are obtained by adding aluminum and titanium to the nickel-copper base. Monel K500 Hexagonal Pipes is precipitation hardenable, due to the additions of Aluminium and Titanium. Monel K500 Hallow Tubesneeds to be turned and worked at slow speeds and low feed rates. Monel K500 Bush Hex Pipes also has low permeability and is nonmagnetic to under -150 Degree F (-101 Degree C).

Monel Alloy K500 EFW Tubing, Monel K500 Welded Tubes, ASTM B 163 Monel K500 Capillary Tube, DIN 2.4375 Hydraulic Tubes, Monel K500 Polished Pipes, ASME SB 165 Monel K500 Black Round Tubes, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Monel K500 Pipe & Tubes Specifications

Grade Monel K500 (UNS No. N05500)
Size 15"NB TO 150"NB IN
Standard ASTM A163, ASME SB163
Range 6.35 mm OD upto 254 mm OD in 0.6 TO 20 mm thickness.
Form Round, Square, Rectangular, Hydraulic Etc
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Length Single Random, Double Random & Cut Length.
Type Seamless / ERW / Welded / Fabricated / EFW
End Plain End, Beveled End, Treaded
Standard Monel K500
Werkstoff Nr. 2.4375
UNS N05500
JIS -
AFNOR -
BS -
GOST -
EN -

Monel K500 Pipe & Tubes Chemical Composition

Monel K500 Ni C Al Mn Si Fe Cu S Ti Cr
63.0 min 0.25 max 2.3 – 3.15 1.5 max 0.5 max 05 – 2 27.0 – 33.0 0.010 max 0.35 – 0.85 –

Monel K500 Pipe & Tubes Mechanical Properties

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
8.44 g/cm3 1350 °C (2460 °F) Psi – 1,15,000 , MPa – 790 Psi – 1,60,000 , MPa – 1100 20 %

Other Types of Monel K500 Pipe & Tubes

  • Monel K500 Seamless Pipes Supplier in UAE
  • Monel K500 Pipes Manufacturer in India
  • Monel K500 Welded Pipes
  • Monel K500 Rectangular Pipe
  • Monel K500 Fabricated Pipes
  • Monel K500 Round Pipe
  • Monel K500 Square Pipe Distributors
  • UNS N05500 Hexagonal Pipe
  • Monel K500 Hallow Pipe
  • DIN 2.4375 Rectangular Seamless Pipes
  • ASME SB 163 Monel K500 ERW Pipes Exporter in Russia
  • ASTM B163 Alloy K500 Welded Pipes
  • JIS NW 5500 Welded Tubing Supplier in Poland
  • Monel Alloy K500 Seamless Tubing
  • ASME SB 165 Monel K500 Welded Tubes in Qatar
  • UNS N05500 Capillary Tubes
  • Monel K500 ERW Tubes
  • UNS N05500 Monel Coiled Seamless Tubing
  • K500 Monel Alloy Round Tubing
  • DIN 2.4375 Rectangular Seamless Pipes

Countries We Export to

Nickel Super Alloys manufactures and exports ​Monel K500 Pipes & Tubes​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Monel K500 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today