Nickel Alloy 201 Pipe & Tubes

Nickel Alloy 201 Pipe & Tubes

Nickel 201 ERW Pipes, UNS N02201 Welded Tubes, 201 Nickel Pipes & Tubes, 201 Nickel Seamless Pipes & Tubes, ASTM B161 Nickel 201 Seamless Pipes, WERKSTOFF NR. 2.4068 Pipe Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the finest exporters of Nickel 201 Pipes & Tubes in India, which has ferromagnetism and high ductility in a wide temperature range. Nickel 201 Seamless Pipes has a lower carbon content to prevent embrittlement by inter-granular carbon at elevated temperatures. Nickel 201 Welded Tubes has characteristics that are useful in several fields, notably chemical processing and electronics. Nickel 201 EFW Pipes are solid solution strengthened and commercially pure wrought materials. Nickel 201 ERW Tubesis utilized in higher temperature applications (over 600 Degree F). Lower carbon content also reduces hardness, making Nickel 201 Round Pipes particularly suitable for cold-formed items.

Nickel 201 Square Tubes is used primarily for parts requiring excellent corrosion and strong magnetic properties. Nickel 201 Rectangular Pipes offers excellent corrosion resistant against caustic soda and chlorine gas, among others. Nickel 201 Electropolish Tubes has exceptional resistance to caustic alkalis at various temperatures and concentrations. Nickel 201 UNS N02201 Pipes is resistant to acids and alkalis, and dry gases at room temperature. Because of its low carbon content, Nickel DIN 2.4060 Tubes is not subject to embrittlement by intergranularly precipitated carbon or graphite when exposed to temperatures of 315 Degree C to 760 Degree C for prolonged time if carbonaceous materials are not in contact with it. Nickel 201 Hexagonal Pipes combines good mechanical properties with excellent resistance to many corrosive environments.

Nickel DIN NR. 2.4068 Pipes, Nickel 201 EFW Tubes, ASME SB622 Nickel Pipe & Tubes, Nickel 201 Hexagonal Pipe & Tubes, ASME SB622 Welded Nickel Pipes, Nickel 201 Pipes & Tubes, Nickel 201 Bush Hex Pipe & Tubes, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Nickel Alloy 201 Pipe & Tubes Specifications

Grade Nickel 201
Standard ASME SB-161, ASME SB-163, ASME SB-730, ASME SB-751 / BS 3072, BS 3073, BS 3074, BS 3075, BS 3076, NA11 DIN 17740, 17750, 17751, 17752, 17753, 17754
Nickel 201 Seamless Pipes 1/4" NB To 6" NB
Nickel 201 Welded / ERW Pipes 1" NB To 16" NB
Form Round, Square, Rectangular, Hydraulic Etc
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Length Single Random, Double Random & Cut Length.
Type Seamless / ERW / Welded / Fabricated / EFW
End Plain End, Beveled End, Treaded
Standard Nickel 201
UNS N02201
BS NA 12
AFNOR -
GOST НП-2
WERKSTOFF NR. 2.4068
JIS NW 2201
EN LC-Ni 99

Nickel Alloy 201 Pipe & Tubes Chemical Composition

Nickel 201 Ni C Mo Mn Si Fe P S Cu Cr
Balance 0.15 max – 0.35 max 0.35 max 0.40 max – 0.01 max 0.25 max –

Nickel Alloy 201 Pipe & Tubes Mechanical Properties

Density Melting Point Yield Strength (0.2%Offset) Tensile Strength Elongation
8.9 g/cm3 1446 °C (2635 °F) Psi – 21500 , MPa – 148 Psi – 67000 , MPa – 462 45 %

Other Types of Nickel Alloy 201 Pipe & Tubes

  • Alloy N02201 Seamless Pipes Supplier in UAE
  • Nickel 201 Pipes Manufacturer in India
  • Nickel 201 Steel Welded Pipes
  • Alloy 201 Rectangular Pipe
  • Nickel 201 Fabricated Pipes
  • Nickel 201 Round Pipe
  • DIN 2.4068 Round Tubing Distributors
  • UNS N02201 Hydraulic Tubes
  • 201 Nickel Hallow Pipe
  • UNS N02201 Hexagonal Pipe
  • 201 Alloy Seamless Pipes Exporter in Russia
  • Alloy 201 Welded Pipes
  • Nickel 201 Coiled Seamless Tubing Supplier in Poland
  • HIgh Nickel Alloy 201 Capillary Tube
  • Nickel N02201 EFW Pipes in Qatar
  • 201 Nickel ERW Pipes
  • ASTM B161 Alloy 201 Pipes
  • B161 Alloy 201 Pipes
  • Nickel N02201 Rectangular Pipe
  • Nickel 201 Hexagonal Pipe

Countries We Export to

Nickel Super Alloys manufactures and exports ​Nickel Alloy 201 Pipes & Tubes​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Nickel Alloy 201 Pipes & Tubes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today