Alloy Steel F1 Threaded Forged Fittings

Alloy Steel F1 Threaded Forged Fittings

F1 Chrome Moly Forged Threaded 90 Deg. Elbow, Alloy Steel F1 Threaded Tee, ASME SA182M Alloy Steel F1 Threaded Cross, F1 Chrome Moly Threaded Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is a well-known manufacturer of Alloy Steel F1 Threaded Forged Fittings, which has features like Reliability, Sturdiness, Easy installation, and more. Our organization has gained recognition as an affluent trader and supplier of Alloy Steel F1 Threaded Elbow Forged Fittings, which has seawater pitting and crevice corrosion resistant. With the aim of becoming the prominent name of the industry, we are involved in offering Alloy Steel F1 Threaded Tee Forged Fittings, which are sturdily constructed with the use of modern technology.Alloy Steel F1 Threaded Cross Forged Fittings is rigorously checked on defined parameters to ensure its defect-free nature.

Alloy Steel F1 Threaded Cap Forged Fittings contains higher levels of molybdenum and nickel, which improve corrosion & pitting resistance in more aggressive environments. Our reputation in the market is largely attributable to our precision-designed Alloy Steel F1 Threaded Bend Forged Fittings from our extensive collection of products, which is manufactured using exceptional quality raw-material and the advanced technology by our dexterous professionals. Apart from the latest technology, we also ensure high levels of tensile and ductile strength in Alloy Steel F1 Threaded Coupling Forged Fittings which is highly beneficial. Alloy Steel F1 Threaded Union Forged Fittingsis often used in Refineries, Pipes for potable Water, Irrigation System, and so on. We hereby also assure you of our lowest rates, best quality materials and our prompt & personalized services in Alloy Steel F1 Threaded Plug Forged Fittings.

ASTM A182 Alloy Steel F1 Threaded Cap, ASME 16.11 Alloy Steel Threaded Bend, Alloy Steel F1 Threaded Weld Cross, Alloy Steel F1 Threaded Bushing, F1 Alloy Steel Threaded Coupling, Alloy Steel F1 Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Alloy Steel F1 Threaded Forged Fittings Specifications

Grade Alloy Steel Grade F1
Standard ASTM A182, ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class F10 LBS, 3000 LBS, F10 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

Alloy Steel F1 Threaded Forged Fittings Chemical Composition

Grade C Mn Si S P Cr Mo
Alloy Steel F1 0.15 max 0.3-0.6 0.5 0.03 0.03 4-6 0.44-0.65

Alloy Steel F1 Threaded Forged Fittings Mechanical Properties

Tensile Strength Yield Strength (0.2%Offset) Elongation
275 485 20 %

Other Types of Alloy Steel F1 Threaded Forged Fittings

  • Alloy Steel F1 Forged Elbow Supplier in UAE
  • Gr F1 Alloy Equal Tee Manufacturer in India
  • Alloy Steel F1 Threaded Cross
  • Alloy Steel F1 Threaded Union
  • F1 Chrome Moly Hexagonal Plug
  • F1 Chrome Moly Threaded Hex Plug
  • Alloy Steel F1 45 Deg Threaded Elbow Distributors
  • Alloy Steel F1 Threaded Bushing
  • Grade F1 Alloy Threaded Lateral Tee
  • Grade F1 Alloy F1 Threaded Cross
  • Alloy Steel F1 Threaded Coupling Exporter in Russia
  • Alloy Steel F1 Threaded Tees
  • Gr F1 Alloy Threaded 45 deg Elbow Supplier in Poland
  • Gr F1 Alloy Threaded 90 deg Elbow
  • F1 Chrome Moly Threaded Cap in Qatar
  • F1 Chrome Moly Threaded Bend Flanges
  • Alloy Steel F1 Threaded Union
  • Alloy Steel F1 Threaded Bushing
  • Alloy Steel F1 Lateral Tee
  • Alloy Steel F1 Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Alloy Steel F1 Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Alloy Steel F1 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today