Inconel 600 / 601 Threaded Forged Fittings

Inconel 600 / 601 Threaded Forged Fittings

Inconel 601 Forged Threaded 90 Deg. Elbow, Inconel 600 Threaded Tee, ASTM B564 Inconel 601 Threaded Cross, UNS N06600 / N06601 Threaded Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the prominent manufacturers, suppliers and exporters of Inconel Alloy 600 / 601 Threaded Forged Fittings, which retains strength over a wide temperature range. Controlled chemical composition limits in Inconel 600 Threaded Elbow Forged Fittings are applied in the nuclear industry to eliminate the risk of SCC by high purity water containing chloride ions. With high nickel content, Inconel 601 Threaded Tee Forged Fittings is virtually immune to chloride-induced SCC. Inconel 600 Threaded Cross Forged Fittingsh as good corrosion resistance of the dry chlorine and chlorine hydride. Inconel 601 Threaded Cap Forged Fittings is used for nuclear engineering and sparking electrodes. The high nickel content of Inconel 600 Threaded Coupling Forged Fittings provides good resistance to reducing environments.

Inconel 601 Threaded Bend Forged Fittings is used in a variety of corrosion resisting applications. Inconel 600 Threaded Union Forged Fittings features superior strength and can be easily formed. Inconel 601 Threaded Bushing Forged Fittings is also used for aerospace and heat treating industries to name a few. The high nickel content in Inconel 600 Threaded Plug Forged Fittings enables it to retain considerable resistance under reducing conditions. Inconel 601 Threaded Hexagonal Plus Forged Fittings makes virtually immune to chloride-ion SCC. Inconel 600 Threaded Lateral Tee Forged Fittings has good resistance in carburizing and chloride containing environments. Inconel UNS N06600 Threaded Forged Fittings displays good heat resistance and freedom from aging or stress corrosion throughout the annealed to heavily cold worked condition range.

ASME SB564 Inconel 600 Threaded Cap, Inconel 601 Threaded Bend, DIN 2.4816 / 2.4851 Threaded Weld Cross, Inconel 600 Threaded Bushing, Inconel 601 Threaded Coupling, Inconel 600 Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 600 / 601 Threaded Forged Fittings Specifications

Grade Inconel Alloy 600 | UNS N06600
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

Standard Inconel 600
UNS N06600
GOST МНЖМц 28-2,5-1,5
BS NA 13
JIS NCF 600
AFNOR NC15FE11M
WERKSTOFF NR. 2.4816
EN NiCr15Fe
OR ЭИ868

Inconel 600 / 601 Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cu Ni Fe
Inconel 600 0.15 max 1 max 0.5 max – 0.015 max 14 – 17 0.50 max 72 min 6.0-10.0
Inconel 601 0.10 max 1.00 max 0.50 max – 0.015 max 21.00-25.00 1.00 max 58-63 Balance

Inconel 600 / 601 Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.1 g/cm3 1411 °C (2571 °F) Psi – 80000 , MPa – 550 Psi – 30000 , MPa – 205 30 %

Other Types of Inconel 600 / 601 Threaded Forged Fittings

  • Inconel 600 Forged Elbow Supplier in UAE
  • Inconel 601 Equal Tee Manufacturer in India
  • Inconel 600 Threaded Cross
  • Inconel 601 Threaded Union
  • UNS N06600 Hexagonal Plug
  • UNS N06601 Threaded Hex Plug
  • DIN 2.4816 45 Deg Threaded Elbow Distributors
  • DIN 2.4851 Threaded Bushing
  • Inconel 600 Threaded Lateral Tee
  • Inconel 601 Alloy Threaded Cross
  • Inconel 600 Threaded Coupling Exporter in Russia
  • Inconel 601 Threaded Tees
  • Inconel 600 45 deg Elbow Supplier in Poland
  • Inconel 601 Threaded 90 deg Elbow
  • NiCr15Fe Threaded Cap in Qatar
  • NiCr23Fe Threaded Bend Flanges
  • Inconel 600 Threaded Union
  • Inconel 601 Threaded Bushing
  • NC15FE11M Lateral Tee
  • NC23FeA Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 600 / 601 Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 600 / 601 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today