Duplex Steel UNS S31803 / S32205 Threaded Forged Fittings

Duplex Steel UNS S31803 / S32205 Threaded Forged Fittings

Duplex Steel UNS S31803 / S32205 Forged Threaded 90 Deg. Elbow, UNS S32205 Threaded Tee, UNS S31803 Threaded Cross, DIN 1.4462 Threaded Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the prominent suppliers of Duplex Steel S31803 / S32205 Threaded Forged Fittings, which is the most widely used grade in the duplex family of stainless steels.Duplex Steel S31803 Threaded Elbow Forged Fittingsis suitable for severe corrosion conditions, particularly where there is frequent contact with high levels of chlorides, carbon dioxide and hydrogen sulfide. Duplex Steel S31803 Threaded Tee Forged Fittings is applied in the industrial fields like seawater desalination plant, chemical plant, seawater pump, and so on. Duplex Steel S31803 Threaded Cross Forged Fittingssuffers from precipitation neither of brittle micro constituents, nor below -50 Degree C because of its ductile-to-brittle-transition. Duplex Steel S31803 Threaded Cap Forged Fittingsdisplay properties characteristic of both austenitic and ferritic stainless steels.

Duplex Steel S31803 Threaded Coupling Forged Fittings demonstrates erosion, crevice, pitting, and general corrosion in severe environments. Duplex Steel S31803 Threaded Bend Forged Fittings is often used in brewing tanks, process plant, and desalination plant. Duplex Steel S31803 Threaded Union Forged Fittings have roughly twice the yield strengthof their counterpart austenitic grades.The austenitic-ferritic chemical composition of Duplex Steel S31803 Threaded Bushing Forged Fittingsresults in excellent mechanical properties. Duplex Steel S31803 Threaded Plug Forged Fittingsis generally supplied in the annealed condition giving yield strengths. Pitting Resistance Equivalent ensures that the resistance to pitting corrosion is as high as possible for Duplex Steel S31803 Threaded Lateral Tee Forged Fittings.

Duplex Steel UNS S31803 Threaded Cap, Duplex 2205 Threaded Bend, UNS S32205 Threaded Weld Cross, UNS S31803 Threaded Bushing, DIN 1.4462 Threaded Coupling, UNS S32205 Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Duplex Steel UNS S31803 / S32205 Threaded Forged Fittings Specifications

Grade Duplex UNS S31803 / S32205
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Duplex S31803 / S32205 1.4462 S31803 / S32205 - - - - -

UNS S31803 / S32205 Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni N Fe
S31803 0.030 max 2.00 max 1.00 max 0.030 max 0.020 max 22.0 – 23.0 3.0 – 3.5 4.50 – 6.50 0.14 – 0.20 63.72 min
S32205 0.030 max 2.00 max 1.00 max 0.030 max 0.020 max 21.0 – 23.0 2.50 – 3.50 4.50 – 6.50 0.8 – 0.20 63.54 min

UNS S31803 / S32205 Threaded Forged Fittings Mechanical Properties

Grades Density (g/cm 3) Density (lb/in 3) Melting Point (°C) Melting Point (°F)
S31803 / S32205 7.805 0.285 1420 – 1465 2588 – 2669

Other Types of UNS S31803 / S32205 Threaded Forged Fittings

  • Duplex Steel UNS S31803 Forged Elbow Supplier in UAE
  • Duplex Steel UNS S32205 Equal Tee Manufacturer in India
  • UNS S31803 Threaded Cross
  • UNS S32205 Threaded Union
  • UNS S31803 Hexagonal Plug
  • DIN 1.4462 Threaded Hex Plug
  • DIN 1.4462 45 Deg Threaded Elbow Distributors
  • A182 Duplex Steel F57 Threaded Bushing
  • UNS S31803 Threaded Lateral Tee
  • UNS S32205 Alloy Threaded Cross
  • Duplex Steel UNS S31803 Threaded Coupling Exporter in Russia
  • Duplex Steel UNS S32205 Threaded Tees
  • UNS S32205 45 deg Elbow Supplier in Poland
  • UNS S31803 Threaded 90 deg Elbow
  • DIN 1.4462 Threaded Cap in Qatar
  • DIN 1.4462 Threaded Bend Flanges
  • Duplex UNS S31803 Threaded Union
  • Duplex UNS S32205 Threaded Bushing
  • Duplex 2205 Lateral Tee
  • Duplex 2205 Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Duplex Steel UNS S31803 / S32205 Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Duplex Steel UNS S31803 / S32205 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today