Incoloy 800 / 800H / 800HT Threaded Forged Fittings

Incoloy 800 / 800H / 800HT Threaded Forged Fittings

Incoloy 800 Forged Threaded 90 Deg. Elbow, Incoloy 800H Threaded Tee, ASTM B564 Incoloy 800HT Threaded Cross, UNS N08800 / N08810 / N08811 Threaded Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of leading distributors and suppliers of Inconel Alloy 800 / 800H / 800HT Threaded Forged Fittings, which has excellent resistance to chloride stress-corrosion cracking.Applications of Inconel 800Threaded Elbow Forged Fittings have extended from petrochemical processing reformer tubing, to bellows and flare tips in refinery service.Inconel 800H Threaded Tee Forged Fittingshas resistant to high temperature corrosion and prolonged exposure. Inconel 800HT Threaded Cross Forged Fittings sis extremely functional as it maintains a stable structure, even when exposed to high temperature.Inconel 800 Threaded Cap Forged Fittingshas excellent carburization in high temperature atmospheres. The restricted chemical compositions, combined with the high temperature anneal, assure these Inconel 800H Threaded Coupling Forged Fittingshave greater creep and rupture strength.

Inconel 800HT Threaded Bend Forged Fittings is commonly welded for applications under 1450 Degree F. Resistance in Inconel 800 Threaded Union Forged Fittings is needed from carburization, oxidation, and other types of high-temperature corrosion. Inconel 800H Threaded Plug Forged Fittings was intended for high temperature structural applications. Inconel 800HT Threaded Bushing Forged Fittings have set the industry standard in high-temperature applications requiring optimum creep andrupture properties. Inconel 800 Threaded Hexagonal Plus Forged Fittings doesn't form the embrittling sigma phase after long time exposure at 1200 Degree F. Inconel 800H Threaded Lateral Tee Forged Fittings is capable of remaining stable and maintaining its austenitic structure even after long time exposures to high temperatures.

ASME SB564 Incoloy 800 Threaded Cap, Incoloy 800H Threaded Bend, DIN 1.4876 / 1.4958 / 1.4876 Threaded Weld Cross, Incoloy 800HT Threaded Bushing, Incoloy 800 Threaded Coupling, Incoloy 800H Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Incoloy 800 / 800H / 800HT Threaded Forged Fittings Specifications

Grade Incoloy Alloy 800 / 800H / 800HT | UNS N08800 / N08810 / N08811
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 8000 LBS, 9000 LBS
Form Threaded weld 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Incoloy 800 Incoloy 800H Incoloy 800HT
UNS N08800 N08810 N08811
EN X10NiCrAlTi32-20 X5NiCrAlTi31-20 X8NiCrAlTi32-21
AFNOR Z8NC32-21 Z8NC33-21 -
JIS NCF 800 NCF 800H NCF 800HT
BS NA 15 NA 15(H) NA 15(HT)
WERKSTOFF NR. 1.4876 1.4958 / 1.4876 1.4859 / 1.4876
GOST ЭИ670 ЭИ670 ЭИ670
OR XH32T XH32T XH32T

Incoloy 800 / 800H / 800HT Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cu Ni Fe
Incoloy 800 0.10 max 1.50 max 1.00 max – 0.015 max 19.00 – 23.00 0.75 max 30.0 – 35.0 39.50 min
Incoloy 800H 0.05 – 0.10 1.50 max 1.00 max – 0.015 max 19.00 – 23.00 0.75 max 30.0 – 35.0 39.50 min
Incoloy 800HT 0.06 – 0.10 1.50 max 1.00 max – 0.015 max 19.00 – 23.00 0.75 max 30.0 – 35.0 39.50 min

Incoloy 800 / 800H / 800HT Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %

Other Types of Incoloy 800 / 800H / 800HT Threaded Forged Fittings

  • Incoloy 800 Forged Elbow Supplier in UAE
  • Incoloy 800H Equal Tee Manufacturer in India
  • Incoloy 800HT Threaded Cross
  • Incoloy 800 Threaded Union
  • UNS N08800 / N08810 Hexagonal Plug
  • UNS N08811 Threaded Hex Plug
  • DIN 1.4958 / 1.4876 45 Deg Threaded Elbow Distributors
  • DIN 1.4859 / 1.4876 Threaded Bushing
  • Incoloy 800 Threaded Lateral Tee
  • Incoloy 800HT Alloy Threaded Cross
  • Incoloy 800H Threaded Coupling Exporter in Russia
  • Incoloy 800 Threaded Tees
  • Incoloy 800HT 45 deg Elbow Supplier in Poland
  • Incoloy 800 Threaded 90 deg Elbow
  • X10NiCrAlTi32-20 Threaded Cap in Qatar
  • X5NiCrAlTi31-20 Threaded Bend Flanges
  • X8NiCrAlTi32-21 Threaded Union
  • Z8NC32-21 Threaded Bushing
  • Z8NC32-21 Lateral Tee
  • X10NiCrAlTi32-20 Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Incoloy 800 / 800H / 800HT Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Incoloy 800 / 800H / 800HT Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today