Inconel 625 Threaded Forged Fittings

Inconel 625 Threaded Forged Fittings

Inconel 625 Forged Threaded 90 Deg. Elbow, Inconel 625 Threaded Tee, ASTM B564 Inconel 625 Threaded Cross, UNS N06625 Threaded Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the finest supplier and exporter of Inconel Alloy 625 Threaded Forged Fittings, which is a nickel-chromium alloy used for its high strength. Inconel 625 Threaded Elbow Forged Fittings is incredibly resistant to oxidation at high temperatures—up to 2,100 Degree F (1,148 Degree C)—as well as carburizing and nitriding. Inconel 625 Threaded Tee Forged Fittings resists a wide range of severely corrosive environments. Inconel 625 Threaded Cross Forged Fittings has excellent corrosion resistance in a wide range of corrosive media. In the soft-annealed condition, Inconel 625 Threaded Cap Forged Fittings is used for wet corrosion applications. Inconel 625 Threaded Coupling Forged Fittings also demonstrates remarkable protection against corrosion and oxidation.

The outstanding strength and toughness of Inconel 625 Threaded Bend Forged Fittings is due to the addition of niobium. Inconel 625 Threaded Union Forged Fittings has excellent fatigue strength and stress-corrosion cracking resistance to chloride ions. Inconel 625 Threaded Bushing Forged Fittings is alloyed through solid solution strengthening. The strength of Inconel 625 Threaded Plug Forged Fittings is primarily a solid solution effect from molybdenum and columbium. Inconel 625 Threaded Hexagonal Plus Forged Fittingshas excellent mechanical properties at both extremely low and extremely high temperatures. Inconel 625 Threaded Lateral Tee Forged Fittings is developed for high temperature strength. Inconel 625 Threaded Hex Plus Forged Fittings is supplemented by various alloys and metals that support its performance characteristics.

ASME SB564 Inconel 625 Threaded Cap, Inconel 625 Threaded Bend, DIN 2.4856 Threaded Weld Cross, Inconel 625 Threaded Bushing, Inconel 625 Threaded Coupling, Inconel 625 Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 625 Threaded Forged Fittings Specifications

Grade Inconel Alloy 625 | UNS N06625
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6250 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

Standard Inconel 625
UNS N06625
GOST ХН75МБТЮ
BS NA 21
AFNOR NC22DNB4M
JIS NCF 625
EN NiCr22Mo9Nb
WERKSTOFF NR. 2.4856
OR ЭИ602

Inconel 625 Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cu Ni Fe
Inconel 625 0.10 max 0.50 max 0.50 max – 0.015 max 20.0 – 23.0 – 58 min 5.0 max

Inconel 625 Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.4 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 517 42.5 %

Other Types of Inconel 625 Threaded Forged Fittings

  • Inconel 625 Forged Elbow Supplier in UAE
  • Inconel 625 Equal Tee Manufacturer in India
  • Inconel 625 Threaded Cross
  • Inconel 625 Threaded Union
  • UNS N06625 Hexagonal Plug
  • UNS N06625 Threaded Hex Plug
  • DIN 2.4856 45 Deg Threaded Elbow Distributors
  • DIN 2.4856 Threaded Bushing
  • Inconel 625 Threaded Lateral Tee
  • Inconel 625 Alloy Threaded Cross
  • Inconel 625 Threaded Coupling Exporter in Russia
  • Inconel 625 Threaded Tees
  • Inconel 625 45 deg Elbow Supplier in Poland
  • Inconel 625 Threaded 90 deg Elbow
  • NiCr22Mo9Nb Threaded Cap in Qatar
  • NC22DNB4M Threaded Bend Flanges
  • ХН75МБТЮ Threaded Union
  • Inconel 625 Threaded Bushing
  • NiCr22Mo9Nb Lateral Tee
  • NC22DNB4M Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 625 Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 625 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today