Incoloy 825 Threaded Forged Fittings

Incoloy 825 Threaded Forged Fittings

Incoloy 825 Forged Threaded 90 Deg. Elbow, Incoloy 825 Threaded Tee, ASTM B564 Incoloy 825 Threaded Cross, UNS N08825 Threaded Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the leading supplier and distributor of Inconel Alloy 825 Threaded Forged Fittings, which has a very stable austenite structure. Inconel 825 Threaded Elbow Forged Fittings has excellent resistance to localized attacks such as pitting and crevice corrosion. Inconel 825 Threaded Tee Forged Fittings has good resistance in neutral chloride media. Inconel 825 Threaded Cross Forged Fittings has good mechanical properties from moderate to high temperatures. Inconel 825 Threaded Cap Forged Fittings is stabilized annealed at the mill to resist inter-granular corrosion as-welded. The nickel content in Inconel 825 Threaded Coupling Forged Fittings is sufficient for resistance to chloride-ion stress-corrosion cracking. Inconel 825 Threaded Bend Forged Fittings has resistance to aggressive forms of corrosion, particularly in aqueous environments.

Inconel 825 Threaded Union Forged Fittings has improved resistance to aqueous corrosion. Inconel 825 Threaded Plug Forged Fittings has nickel in conjunction with the molybdenum and copper. Inconel 825 Threaded Bushing Forged Fittings has resistant to inter-granular attack after exposure to temperatures in a range that would sensitize unstabilized stainless steels. Inconel 825 Threaded Hexagonal Plus Forged Fittings has excellent resistance to both reducing and oxidizing acids like sulfuric and phosphoric. Inconel 825 Threaded Lateral Tee Forged Fittings has resistant to chloride-ion SCC and, pitting & crevice corrosion. Combined with molybdenum and copper, Inconel 825 Threaded Hex Plus Forged Fittings provides substantially improved corrosion resistance in reducing environments when compared to conventional austenitic stainless steels.

ASME SB564 Incoloy 825 Threaded Cap, Incoloy 825 Threaded Bend, DIN 2.4858 Threaded Weld Cross, Incoloy 825 Threaded Bushing, Incoloy 825 Threaded Coupling, Incoloy 825 Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Incoloy 825 Threaded Forged Fittings Specifications

Grade Incoloy 825 | UNS N08825
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB
Class 2000 LBS, 3000 LBS, 8250 LBS, 9000 LBS
Form Threaded weld 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Socket weld Forged Fittings

Standard Incoloy 825
UNS N08825
GOST ЭП703
AFNOR NFE30C20DUM
BS NA 16
JIS NCF 825
EN NiCr21Mo
WERKSTOFF NR. 2.4858
OR XH38BT

Incoloy 825 Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cu Ni Fe
Incoloy 825 0.05 max 1.00 max 0.5 max – 0.030 max 19.50 – 23.50 1.50 – 3.00 38.00 – 46.00 22.00 min

Incoloy 825 Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.14 g/cm3 1400 °C (2550 °F) Psi – 80,000 , MPa – 550 Psi – 32,000 , MPa – 220 30 %

Other Types of Incoloy 825 Threaded Forged Fittings

  • Incoloy 825 Forged Elbow Supplier in UAE
  • Incoloy 825 Equal Tee Manufacturer in India
  • Incoloy 825 Threaded Cross
  • Incoloy 825 Threaded Union
  • UNS N08825 Hexagonal Plug
  • UNS N08825 Threaded Hex Plug
  • DIN 2.4858 45 Deg Threaded Elbow Distributors
  • DIN 2.4858 Threaded Bushing
  • Incoloy 825 Threaded Lateral Tee
  • Incoloy 825 Alloy Threaded Cross
  • Incoloy 825 Threaded Coupling Exporter in Russia
  • Incoloy 825 Threaded Tees
  • Incoloy 825 45 deg Elbow Supplier in Poland
  • Incoloy 825 Threaded 90 deg Elbow
  • NiCr21Mo Threaded Cap in Qatar
  • NFE30C20DUM-20 Threaded Bend Flanges
  • Incoloy 825 Threaded Union
  • NiCr21Mo Threaded Bushing
  • NFE30C20DUM Lateral Tee
  • GOST ЭП703 Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Incoloy 825 Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Incoloy 825 Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo