Incoloy 925 Pipe Fittings

Incoloy 925 Pipe Fittings

Incoloy 925 Pipe Elbow, 925 Incoloy Pipe Cap, ANSI B16.9 Incoloy 925 Short & Long Radius Elbow, Incoloy 925 Pipe Fittings, ASTM B366 925 Incoloy 90 degree Elbow, 925 180 Deg Bend Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the leading names in manufacturing Inconel Alloy 925 Butt Weld Pipe Fittings, which has high strength and excellent corrosion resistance. The nickel, in conjunction with the molybdenum and copper in Inconel 925 Elbow Pipe Fittings, also gives outstanding resistance to reducing chemicals. Inconel 925 Tee Pipe Fittings is a hard and ductile transition metal that is considered corrosion-resistant because of its slow rate of oxidation. The chemical composition in Inconel 925 Cross Pipe Fittings is designed to provide a combination of high strength and excellent corrosion resistance. Inconel 925 Reducer Pipe Fittings is known for a number of different unique properties including protection in oxidizing and reducing atmosphere.

Inconel 925 Bend Pipe Fittings is designed primarily for applications in the production of gas. Inconel 925 Stub End Pipe Fittings has outstanding resistance to general corrosion, crevice corrosion, pitting, and SCC. Inconel 925 End Cap Pipe Fittings is used in packers, and tubulars, along with in sour gas environments. The Titanium and Aluminum are specifically added to give a strengthening of Inconel 925 Lateral Tee Pipe Fittings during ageing throughout the alloy matrix and greatly increases the hardness and strength. Sufficient nickel content in Inconel 925 Concentric Reducer Pipe Fittings provides protection against chloride-ion stress-corrosion cracking. Inconel 925 Eccentric Reducer Pipe Fittings can be strengthened by solid-solution hardening, precipitation hardening and work hardening. Inconel UNS N09925 Pipe Fittings has resistance to chloride ion stress-corrosion cracking.

Alloy 925 Lateral Tee, 925 Incoloy Reducer, Incoloy Alloy 925, UNS N09925 Alloy 925 Unequal & Equal Tee, Alloy 925 Concentric Reducer, Incoloy UNS N09925 Long Stub End, End Cap Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Incoloy 925 Pipe Fittings Specifications

Grade Incoloy Alloy 925 / UNS N09925
Standard ASTM B366, ASME SB366
Dimensions ASME B16.28, ASME/ANSI B16.9, MSS-SP-43
Incoloy 925 Seamless Fittings 1/2" NB - 10" NB
Incoloy 925 Welded Fittings 1/2" NB - 48" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Wall Thickness from 2 to 40 mm
Type Seamless / Welded / Fabricated
Standard Incoloy 925
UNS N09925
WERKSTOFF NR. -

Incoloy 925 Pipe Fittings Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr Al Ti
925 0.03 max 1.00 max 0.05 max 0.03 max 1.50 – 3.00 22.00 min 42.00 – 46.00 19.55 – 22.50 0.01-0.05 max –

Incoloy 925 Pipe Fittings Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
825 8.14 g/cm3 1400 °C (2550 °F) Psi – 80,000 , MPa – 550 Psi – 32,000 , MPa – 220 30 %

Other Types of Incoloy 925 Pipe Fittings

  • Incoloy 925 Buttweld Tee Supplier in UAE
  • UNS N09925 Cross Manufacturer in India
  • Incoloy 925 Butwteld Tee
  • Incoloy 925 45 deg.Elbow
  • Incoloy 925 Buttweld Pipe Fittings
  • Incoloy 925 Short Radius Elbow
  • UNS N09925 Ecentric Reducer Distributors
  • Incoloy 925 Buttweld Pipe Fitting
  • ASME SB366 Stub End
  • 925 Incoloy Concentric Reducer
  • Incoloy 925 Long Radius Elbow Exporter in Russia
  • Incoloy 925 U Bend
  • Incoloy 925 Stub End Supplier in Poland
  • 925 Incoloy Short Radius Elbow
  • Incoloy 925 Equal Tee in Qatar
  • UNS N09925 End Cap
  • ASME SB366 Concentric Reducer
  • Incoloy 925 Seamless Fitting
  • Incoloy 825 180 Deg Elbow
  • Incoloy 925 Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Incoloy 925 Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Incoloy 925 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today