Inconel 718 Pipe Fittings

Inconel 718 Pipe Fittings

UNS N07718 Inconel 90 Deg & 45 Deg Elbow, Inconel 718 Short Radius Elbow, Alloy 718 Fitting Cross, Inconel 718 Short & Long Stub End, Inconel Alloy 718 Pipe Bend Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the leading names in supplying Inconel Alloy 718 Pipe Fittings, which has excellent weldability. Inconel 718 Elbow Pipe Fittings is used for down-hole shafting and well head parts. Inconel 718 Tee Pipe Fittings maintains high strength and good ductility up to 1300 Degree F (704 Degree C). The age-hardenable Inconel 718 Cross Pipe Fittings can be readily fabricated, even into complex parts. When heated, Inconel 718 Reducer Pipe Fittings forms a thick and stableprotecting the surface from further attack. Inconel 718 Bend Pipe Fittings displays exceptionally high tensile, yield, and creep-rupture properties at high temperatures. Inconel 718 Stub End Pipe Fittings is well suited for applications requiring high strength in temperature ranges from cryogenic up to 1400 Degree F.

Inconel 718 End Cap Pipe Fittings has excellent weldability when compared to the nickel-base super-alloys hardened by aluminum and titanium. Inconel 718 Dish Cap Pipe Fittings has high temperature dynamic applications. It combines corrosion resistance and high strength with outstanding weldability including resistance to post-weld cracking. Beside commercial applications for Inconel 718 Lateral Tee Pipe Fittings, mission-critical defense operations increasingly rely on the peak performance the engines offer. Inconel 718 Concentric Pipe Fittings is strengthened alloy with excellent mechanical properties at elevated temperatures, as well as cryogenic temperatures. Inconel 718 Eccentric Reducer Pipe Fittings is a high strength nickel base super-alloy used for cryogenic temperatures up to long term service at 1200 Degree F.

ASME B16.28 Alloy 718 Short Radius Elbow, UNS N07718 End Cap & Dish Cap, Inconel 718 Eccentric Reducer, Alloy 718 Concentric Reducer, Inconel Alloy 718 Equal Tee & Unequal Tee Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 718 Pipe Fittings Specifications

Grade Inconel Alloy 718 / UNS N07718
Standard ASTM B366, ASME SB366
Dimensions ASME B16.28, ASME/ANSI B16.9, MSS-SP-43
Inconel 718 Seamless Fittings 1/2" NB - 10" NB
Inconel 718 Welded Fittings 1/2" NB - 48" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Wall Thickness from 2 to 40 mm
Type Seamless / Welded / Fabricated
Standard Inconel 718
UNS N07718
WERKSTOFF NR. 2.4668

Inconel 718 Pipe Fittings Chemical Composition

Grade C Mn Si Fe S Cr Al Ni
718 min. – – – bal – 17.0 0.2 50.0
max. 0.08 0.35 0.35 bal 0.01 21.0 0.8 55.0

Inconel 718 Pipe Fittings Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
718 8.14 g/cm3 1400 °C (2550 °F) Psi – 80,000 , MPa – 550 Psi – 32,000 , MPa – 220 30 %

Other Types of Inconel 718 Pipe Fittings

  • Inconel 718 Buttweld Tee Supplier in UAE
  • UNS N07718 Cross Manufacturer in India
  • DIN 2.4668 Butwteld Tee
  • DIN 2.4668 45 deg.Elbow
  • Inconel 718 Buttweld Pipe Fittings
  • Inconel 718 Short Radius Elbow
  • UNS N07718 Ecentric Reducer Distributors
  • Inconel 718 Buttweld Pipe Fitting
  • ASME SB366 Stub End
  • 718 Inconel Concentric Reducer
  • Inconel 718 Long Radius Elbow Exporter in Russia
  • Inconel 718 U Bend
  • Inconel 718 Stub End Supplier in Poland
  • 718 Inconel Short Radius Elbow
  • Inconel 718 Equal Tee in Qatar
  • UNS N07718 End Cap
  • ASME SB366 Concentric Reducer
  • Inconel 718 Seamless Fitting
  • Inconel 718 180 Deg Elbow
  • Inconel 718 Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 718 Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 718 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today