Stainless Steel 347 / 347H Pipe Fittings

Stainless Steel 347 / 347H Pipe Fittings

Stainless Steel 347 180 Deg bend, ASTM A403 347H Stainless Steel 90 degree Elbow, SS WP 347 45 degree Elbow, SS 347 Equal Tee, ASTM A403 347 Stainless Steel 90 degree Elbow Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the prominent supplying and distributing firm of Stainless Steel 347 / 347H Butt Weld Pipe Fittings, which is stabilized by the additions of chromium and tantalum. However, tantalum in Stainless Steel 347 Pipe Fittings occurs in nature in conjunction with columbium. Stainless Steel 347H Elbow Pipe Fittings is used to make radiant super-heaters and boiler tubes. Stainless Steel 347 Tee Pipe Fittings is found in applications that demand high temperature resistance. Stainless Steel 347H Cross Pipe Fittings form another group known as precipitation-hardened steels, which are a combination of martensitic and austenitic alloys. Stainless Steel 347 Reducer Pipe Fittings is developed to provide an 18-8 type alloy with improved inter-granular-corrosion resistance.

Stainless Steel 347HBend Pipe Fittings has excellent resistance to inter-granular corrosion after exposure to temperatures in the chromium carbide precipitation range of 427 Degree C – 816 Degree C. Stainless Steel 347 Stub End Pipe Fittings follows exposure to temperatures in the chromium carbide precipitation range from 800 Degree F to 1500 Degree F. Stainless Steel 347HEnd Cap Pipe Fittings is preferable for aqueous and low temperature environments due to its good resistance to inter-granular attack. Stainless Steel UNS S34700Pipe Fittings is extensively inured to the effect of sulfurous gases, especially above 900 Degree C, which is very low. Stainless Steel UNS S34709Pipe Fittings is suitable for service in aqueous and low temperature environments.

ANSI B16.9 Stainless Steel 347 Welded Buttweld Fittings, ASME SA403 SS 347H Long Stub,SS 347H Pipe Elbow, SS 347H Pipe bend, SS 347H Equal Tee, Stainless Steel UNS S34709 Seamless Pipe Fittings, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 347 / 347H Pipe Fittings Specifications

Grade SS 347 | UNS S34700
Standard ASTM A403 / ASME SA403
Dimensions ANSI/ASME B16.9, B16.28, MSS-SP-43.
Thickness 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75
Size 1/2" NB - 48" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Type Seamless / Welded / Fabricated

STANDARD SS 347
UNS S34700
WERKSTOFF NR. 1.4550
AFNOR Z6CNDT17-123<
JIS SUS 347
GOST 08Ch17N13M2T
BS 320S31
EN X6CrNiMoTi17-12-2<

Stainless Steel 347 / 347H Pipe Fittings Chemical Composition

Grade C Ni Mn P S Cr Si Mo N
347 0.08 max 9.00-13.00 2.0 max 0.045 max 0.030 max 17.00 – 20.00 1.0 max – –
347H 0.08 max 9.00-13.00 2.0 max 0.045 max 0.030 max 17.00 – 20.00 1.0 max – –

Stainless Steel 347 / 347H Pipe Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.0 g/cm3 1454°C (2650°F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 347 / 347H Pipe Fittings

  • SS 347/347H Buttweld Tee Supplier in UAE
  • Stainless UNS s31703 Cross Manufacturer in India
  • SS 347/347H Butwteld Tee
  • DIN 1.4550 45deg.Elbow
  • DIN 1.4961 Buttweld Pipe Fittings
  • 347 Steel Short Radius Elbow
  • UNS s31703 Ecentric Reducer Distributors
  • SS 347H Buttweld Pipe Fitting
  • ASME B16.28 Stub End
  • SS 347 Concentric Reducer
  • ASME SA403 SS Long Radius Elbow Exporter in Russia
  • Stainless Steel 347 U Bend
  • WNR. 1.4550 SS 347H Stub End Supplier in Poland
  • 347 Short Radius Elbow
  • WP 347H Steel Equal Tee in Qatar
  • UNS S34709 End Cap
  • ASME SA403 Concentric Reducer
  • SS 347H Seamless Fitting
  • Stainless Steel 347 45 Elbow
  • SS 347H Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 347 / 347H Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 347 / 347H Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today