Stainless Steel 410 Pipe Fittings

Stainless Steel 410 Pipe Fittings

Stainless Steel 410 Stubend, SS 410 Pipe End Cap, SS 410 10d bend, DIN 1.4006 Pipe Fittings, UNS S41000 Eccentric Reducer Pipe Fittings, SS 410 Seamless Buttweld Fittings Manufacturer in Mumbai,India.

Nickel Super Alloys is a popular firm that manufactures and exports Stainless Steel 410 Butt Weld Pipe Fittings, which is often supplied in the hardened condition. Stainless Steel 410 Elbow Pipe Fittings offers both exceptional wear and corrosion resistance.Stainless Steel 410 Tee Pipe Fittings can be heat treated to obtain a wide range of mechanical properties. The corrosion resistance of Stainless Steel 410 Cross Pipe Fittings can be further enhanced by a series of processes. Stainless Steel 410 Reducer Pipe Fittings combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium alloys. Stainless Steel 410 Bend Pipe Fittings is magnetic in both the annealed and hardened conditions.

Stainless Steel 410 Stub End Pipe Fittings has good impact corrosion ,strength, and scaling resistance up to 1200 Degree F (649 Degree C). In its annealed condition, Stainless Steel 410 End Cap Pipe Fittings may be formed, drawn, or shaped. Stainless Steel 410 Dish Cap Pipe Fittings provides good corrosion resistance plus high strength and hardness. 410 Stainless Steel Pipe Fittings has a wide range of properties that can be developed with different heat treatments. High carbon content in Stainless Steel UNS S41000 Pipe Fittings results in the formation of chromium carbide compounds. Oil quenching thisStainless Steel DIN 1.4006 Pipe Fittings from temperatures in the range of 1800 Degree F to 1950 Degree F producesthe highest strength and/or wear resistance as well ascorrosion resistance.

Stainless Steel 410 Cross, SS 410 Welded Buttweld Fittings, 410 Stainless Steel Equal & Unequal Tee, SS 410 Short Radius Elbow, 410 Stainless Steel Short stub end, 410 SS 5D Elbows, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 410 Pipe Fittings Specifications

Grade SS 410 | UNS S41000
Standard ASTM A403 / ASME SA403
Dimensions ANSI/ASME B16.9, B16.28, MSS-SP-43.
Thickness 5s, 10s, 40s, 80s, 10, 20, 40, STD, 60, 80, XS, 100, 120, 140, 160, XXS available with NACE MR 01-75
Size 1/2" NB - 48" NB
Form 90 Elbow, 45 Elbow, Long Radius Elbow, Short Radius Elbow, Concentric Reducer, Eccentric Reducer, Equal Tee, Unequal Tee, Lateral Tee, Cross, Bends 1.5d, 3d, 5d, 10d, U bend, 180 Deg Bend, Short Stub End, Long stub end, End Cap, Dish Cap
Schedule SCH 5 To SCH XXS
Type Seamless / Welded / Fabricated

Grade UNS No Old British Euronorm Swedish SS Japanese JIS
BS En No Name
410 S41000 410S21 56A 1.4006 X12Cr13 2302 SUS 410

Stainless Steel 410 Pipe Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
410 min. – – – – – 11.5 – – –
max. 0.15 1.0 1.00 0.040 0.030 13.5 – 0.75 –

Stainless Steel 410 Pipe Fittings Mechanical Properties

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
410 480 275 16 95 201

Other Types of Stainless Steel 410 Pipe Fittings

  • SS 410 Buttweld Tee Supplier in UAE
  • Stainless UNS S41000 Cross Manufacturer in India
  • SS 410 Butwteld Tee
  • DIN 1.4006 45deg.Elbow
  • DIN 1.4006 Buttweld Pipe Fittings
  • 410 Steel Short Radius Elbow
  • UNS S41000 Ecentric Reducer Distributors
  • SS 410 Buttweld Pipe Fitting
  • ASME B16.28 Stub End
  • SS 410 Concentric Reducer
  • ASME SA403 SS Long Radius Elbow Exporter in Russia
  • Stainless Steel 410 U Bend
  • WNR. 1.4006 SS 347H Stub End Supplier in Poland
  • 410 Short Radius Elbow
  • WP 410 Steel Equal Tee in Qatar
  • UNS S41000 End Cap
  • ASME SA403 Concentric Reducer
  • SS S41000 Seamless Fitting
  • Stainless Steel 410 45 Elbow
  • SS 410 Pipe Bends

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 410 Pipe Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 410 Pipe Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today