Hastelloy X Threaded Forged Fittings

Hastelloy X Threaded Forged Fittings

Hastelloy X Forged Threaded 90 Deg. Elbow, Hastelloy X Threaded Tee, UNS N06002 Threaded Cross, DIN 2.4665 Threaded Forged Cap Manufacturer in Mumbai, India.

Nickel Super Alloys is a known supplier and manufacturer of Hastelloy Alloy X Threaded Forged Fittings, which is non-magnetic. Hastelloy X Threaded Elbow Forged Fittings has great high temperature and stress rupture characteristics above 790 Degree C or 1450 Degree F. Hastelloy X Threaded Tee Forged Fittings has highly resistant to stress corrosion cracking in petrochemical applications. Hastelloy X Threaded Reducer Forged Fittings has good resistance to stress-corrosion cracking and carburization. Hastelloy X Threaded Cross Forged Fittings transition ducts, spray bars,combustor cans, and flame holders. Hastelloy X Threaded Coupling Forged Fittingshas excellent forming and welding characteristics. Hastelloy X Threaded Cap Forged Fittings is well suited for forming and welding.

Furnace rolls made of Hastelloy X Threaded Bend Forged Fittings were still in good condition after operating for 8,700 hours at 2150 Degree F. Hastelloy X Threaded Union Forged Fittings can be forgedand, because of its goodductility, can be cold worked. Hastelloy X Threaded Bushing Forged Fittings is primarily noted for heat and oxidation resistance. Hastelloy X Threaded Plug Forged Fittings also has good resistance to chloride stress-corrosion cracking. Hastelloy X Threaded Hexagonal Plus Forged Fittingscan be welded by gas-tungsten- arc, metal arc, and gas-metal-arc. Hastelloy X Threaded Lateral tee Forged Fittings is corrosion resistant, oxidation resistant and heat resistant. Hastelloy UNS N06002 Threaded Forged Fittings is popular and effective nickel-chromium-iron-molybdenum alloy, which offer users a wide range of principal features.

Hastelloy X Threaded Cap, Alloy X Threaded Bend, UNS N06002 Threaded Weld Cross, Hastelloy X Threaded Bushing, DIN 2.4665 Threaded Coupling, Hastelloy X Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Hastelloy X Threaded Forged Fittings Specifications

Grade Hastelloy X | UNS N06002
Standard ASTM B564 & ASME SB564
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, X0 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

Standard Hastelloy X
UNS N06002
WERKSTOFF NR. -

Hastelloy X Threaded Forged Fittings Chemical Composition

Grade Ni Mo Cr Fe Mn C Co Si P S
X Balance 8.0 -10.0 20.50 – 23.00 17.00 – 20.00 1.00 max 0.05 – 0.15 0.50 – 2.50 1.00 max 0.04 max 0.03 max

Hastelloy X Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.22 g/cm³ 1355°C 655 MPa 240 MPa 35%

Other Types of Hastelloy X Threaded Forged Fittings

  • Hastelloy X Forged Elbow Supplier in UAE
  • Hastelloy X Equal Tee Manufacturer in India
  • Hastelloy X Threaded Cross
  • UNS N06002 Threaded Union
  • UNS N06002 Hexagonal Plug
  • DIN 2.4665 Threaded Hex Plug
  • DIN 2.4665 45 Deg Threaded Elbow Distributors
  • Hastelloy X Threaded Bushing
  • Hastelloy X Threaded Lateral Tee
  • Alloy X Alloy Threaded Cross
  • Hastelloy X Threaded Coupling Exporter in Russia
  • Alloy X Threaded Tees
  • UNS N06002 45 deg Elbow Supplier in Poland
  • UNS N06002 Threaded 90 deg Elbow
  • DIN 2.4665 Threaded Cap in Qatar
  • DIN 2.4665 Threaded Bend Flanges
  • Hastelloy X Threaded Union
  • Alloy X Threaded Bushing
  • Hastelloy X Lateral Tee
  • Hastelloy X Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Hastelloy X Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Hastelloy X Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today