Inconel 625 Flanges

Inconel 625 Flanges

Inconel 625 Nippolet Flanges, Inconel UNS N06625 Pipe Flanges, Inconel 625 Slip On Flanges, Alloy 625 Flanges, Inconel 625 Long Weld Neck, Inconel 625 Spectacle Blind Flanges Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the finest supplier and exporter of Inconel Alloy 625 Flanges, which has excellent weldability and is frequently used to weld. Inconel 625 Slip On Raised Flanges maintains a great degree of its tensile strength in extreme temperatures compared to plain steel alloys. Strength of Inconel 625 Blind Raised Flanges is derived from the solid solution strengthening effect of molybdenum and niobium on its nickel-chromium matrix. Inconel 625 Spectacle Blind Flangesis used for pollution-control equipment, and nuclear reactors. Inconel 625 Threaded Flangesis often used for Marine Industries and Aerospace Industries. The strength of Inconel 625 Weld Neck Flanges can be enhanced by heat treatment.

Inconel 625 Socket Weld Flanges was developed with the purpose of creating a material that could be used for steam-line piping. Inconel 625 Lap Joint Flanges is also used in chemical plant hardware, and special seawater applications. Inconel 625 Ring Joint Type Flanges displays high tensile strength, brazeability and fabricability. Inconel 625 Spacer Flanges has outstanding resistance to chloride pitting and crevice corrosion cracking. Inconel 625 Long Weld Neck Flangeshas high resistance to oxidation at elevated temperatures up to 1050 Degree C. At 1800 Degree F, scaling resistance of Inconel 625 Nippolet Flanges becomes a significant factor in service. Inconel UNS N06625 Flanges is frequently used for Heat shields, Combustion and chimney liners, Tubing, etc. Matching filler metals like Inconel WNR 2.4856 Flanges are also used to join dissimilar metals.

Inconel 625 Pipe Flanges, ASME SB564 Alloy 625 Lap Joint Flange, Inconel DIN 2.4856 Socket Weld Flanges, Alloy 625 Orifice Flange, ANSI B16.5 Alloy 625 Blind Flanges, ASTM B564 Inconel 625 Threaded Flanges Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 625 Flanges Specifications

Grade Inconel Alloy 625 / UNS N06625
Standard ASTM B564, ASME SB564
Dimensions ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44
Size 1/2" - 48" (15NB - 1200NB)
Class / Pressure Rating 150 Class, 300 Class, 625 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc.
Form Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges
Flange Face Type Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ)
Standard Inconel 625
UNS N06625
GOST ХН75МБТЮ
BS NA 21
AFNOR NC22DNB4M
JIS NCF 625
EN NiCr22Mo9Nb
WERKSTOFF NR. 2.4856
OR ЭИ602

Inconel 625 Flanges Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 625 0.10 max 0.50 max 0.50 max 0.015max – 5.0 max 58.0 min 20.0 – 23.0

Inconel 625 Flanges Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 625 8.4 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 517 42.5 %

Other Types of Inconel 625 Flanges

  • Inconel 625 Tongue & Groove Flanges Supplier in UAE
  • Inconel 625 Spectacle blind flanges Manufacturer in India
  • Inconel 625 Long Weld Neck Flanges
  • Inconel 625 Flat Face Flanges
  • UNS N06625 High Hub Blind Flanges
  • UNS N06625 Lap Joint Flanges
  • DIN 2.4856 Reducing Flanges Distributors
  • DIN 2.4856 Blind Flanges
  • UNS N06625 Slip On Flanges
  • UNS N06625 Threaded Flanges
  • Inconel 625 Orifice Flanges Exporter in Russia
  • Inconel 625 400# Forged Flanges
  • Inconel 625 F91 600# Plate Flanges Supplier in Poland
  • Inconel 625 900# Spacer Ring Flanges
  • DIN 2.4856 PN6 Nipo Flange in Qatar
  • DIN 2.4856 PN10 Nipolet Flanges
  • UNS N06625 Pipe Flanges
  • UNS N06625 SORF Flanges
  • Inconel 625 WNRF Flanges
  • Inconel 625 Threaded Flanges

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 625 Flanges​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 625 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today