Inconel 718 Flanges

Inconel 718 Flanges

ANSI B16.5 Alloy 718 Blind Flanges, Inconel 718 Plate flange, Inconel 718 Slip On Flanges, ASME SB564 Alloy 718 Lap Joint Flange, Inconel 718 Long weld neck, Alloy 718 RTJ Flange Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the leading names in supplying Inconel Alloy 718 Flanges, which features a melting point of 2300 Degree C. Inconel 718 Slip On Raised Flanges has excellent weldability when compared to the nickel-base super alloys hardened by aluminum and titanium. Inconel 718 Blind Raised Flanges has excellent welding characteristics, resistant to post-weld age cracking. Typically sold in the solution annealed temper of Inconel 718 Spectacle Blind Flanges, but can be ordered cold worked, aged, or cold worked & aged. The creation of Inconel 718 Threaded Flanges was a direct offshoot of nearly a decade of research to create a Nickel Chromium Molybdenum Niobium (Ni-Cr-Mo) super-alloy. Inconel 718 Weld Neck Flanges is also usedfor fasteners and instrumentation parts. Inconel 718 Socket Weld Flanges are typically used in high temperature applications.

Inconel 718 Lap Joint Flanges is used for resistance to chlorides, stress corrosion and sulfide stress cracking. The addition of niobium in Inconel 718 Ring Joint Type Flanges acts with the molybdenum to stiffen the alloy’s matrix. The room temperature strength of Inconel 718 Spacer Flanges is substantially increased by precipitation heat treatment. The excellent heat treatment in Inconel 718 Long Weld Neck Flanges should be used to obtain the best combination of tensile properties and stress rupture properties. Aerospace engineers rely on super-alloys like Inconel 718 Nippolet Flanges for the hot sections of turbo-reactors. Inconel UNS N07718 Flanges has corrosion-resistance, high strength, and good fabrication characteristics.

Inconel 718 Nippolet Flanges, Inconel UNS N07718 Pipe Flanges, ASTM B564 Inconel 718 Threaded Flanges, Inconel 718 Spacer, Inconel 718 Pipe Flanges, Alloy 718 Orifice Flange, Inconel 718 Nippo Flanges Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Inconel 718 Flanges Specifications

Grade Inconel Alloy 718 / UNS N07718
Standard ASTM B564, ASME SB564
Dimensions ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44
Size 1/2" - 48" (15NB - 1200NB)
Class / Pressure Rating 150 Class, 300 Class, 718 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc.
Form Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges
Flange Face Type Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ)
Standard Inconel 718
UNS N07718
WERKSTOFF NR. 2.4668

Inconel 718 Flanges Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 718 0.08 max 0.35 max 0.35 max 0.015max 0.30 max – 50.00 – 55.00 17.00 – 21.00

Incoloy 718 Flanges Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 718 8.2 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 482 45 %

Other Types of Incoloy 718 Flanges

  • Inconel 718 Tongue & Groove Flanges Supplier in UAE
  • Inconel 718 Spectacle blind flanges Manufacturer in India
  • Inconel 718 Long Weld Neck Flanges
  • Inconel 718 Flat Face Flanges
  • UNS N07718 High Hub Blind Flanges
  • UNS N07718 Lap Joint Flanges
  • DIN 2.4668 Reducing Flanges Distributors
  • DIN 2.4668 Blind Flanges
  • Inconel 718 Slip On Flanges
  • UNS N07718 Threaded Flanges
  • Inconel 718 Orifice Flanges Exporter in Russia
  • Inconel 718 400# Forged Flanges
  • Inconel 718 F91 600# Plate Flanges Supplier in Poland
  • Inconel 718 900# Spacer Ring Flanges
  • DIN 2.4668 PN6 Nipo Flange in Qatar
  • DIN 2.4668 PN10 Nipolet Flanges
  • Inconel 718 Pipe Flanges
  • UNS N07718 SORF Flanges
  • Inconel 718 WNRF Flanges
  • Inconel 718 Threaded Flanges

Countries We Export to

Nickel Super Alloys manufactures and exports ​Inconel 718 Flanges​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Inconel 718 Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today