Stainless Steel 316 / 316L / 316Ti Flanges

Stainless Steel 316 / 316L / 316Ti Flanges

Stainless Steel 316L Nippolet Flanges, Stainless Steel 316L RTJ Flange, Stainless Steel 316Ti Nippolet Flanges, ASTM A182 SS F316Ti Threaded Flanges, SS 316L Weld Neck Flange Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the leading distributor and supplier of Stainless Steel 316 / 316L / 316Ti Pipe Flanges, which is generally regarded as the most common austenitic stainless steel. Typical applications of Stainless Steel 316 Slip On Raised Flanges are Chemical Processing and Springs. The formation of grain boundary chromium of Stainless Steel 316L Blind Raised Flanges elevates at temperatures in the range of approximately 900 Degree F to 1500 Degree F (425 to 815 Degree C). Stainless Steel 316 Ti Spectacle Flanges can improve the aqueous corrosion resistance of welds made in higher carbon grades. A preheating is not necessary for Stainless Steel 316 Spectacle Flanges, because it has outstanding welding characteristics.

The molybdenum allows Stainless Steel 316L Threaded Flanges to be more resistance to corrosion overall, with specific resistance against chlorine pitting. Stainless Steel 316 Weld Neck Flanges is immune to grain boundary carbide precipitation(sensitization). Titanium addition in Stainless Steel 316Ti Socket Weld Flanges can be used atelevated sensitization temperatures. Stainless Steel 316 Lap Joint Flanges is used especially for more saline or chloride-exposed environments. Stainless Steel 316L Ring Joint Type Flanges are stronger at elevated temperatures. Low maintenance and familiar luster make it an ideal Stainless Steel 316Ti Spacer Flanges for many applications where both the strength of steel and corrosion resistance is required. Stainless Steel 316 Nippolet Flanges is often used for pharmaceutical and petroleum industries.

Stainless Steel UNS S31635 Pipe Flanges, Stainless Steel 316 Pipe Flanges, SS 316Ti Blind Flanges, SS DIN 1.4571 Socket Weld Flanges, ANSI B16.5 SS F316 Ring Type Joint Flanges, SS 316 Lap Joint Flange Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 316 / 316L / 316Ti Specifications

Grade Stainless Steel 316/316L | SS 316/316L | UNS S31600/S31603
Standard ASTM A182, ASME SA182
Dimensions ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44
Size 1/2" - 48" (15NB - 1200NB)
Class / Pressure Rating 150 Class, 300 Class, 718 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc.
Form Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges
Flange Face Type Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ)

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 316 1.4401 / 1.4436 S31600 SUS 316 316S31 / 316S33 – Z7CND17‐11‐02 X5CrNiMo17-12-2 / X3CrNiMo17-13-3
SS 316L 1.4404 / 1.4435 S31603 SUS 316L 316S11 / 316S13 03Ch17N14M3 / 03Ch17N14M2 Z3CND17‐11‐02 / Z3CND18‐14‐03 X2CrNiMo17-12-2 / X2CrNiMo18-14-3

Stainless Steel 316 / 316L / 316Ti Flanges Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
SS 316 0.08 max 2 max 1.0 max 0.045 max 0.030 max 16.00 – 18.00 2.00 – 3.00 11.00 – 14.00 67.845 min
SS 316L 0.035 max 2 max 1.00 max 0.045 max 0.030 max 16.00 – 18.00 2.00 – 3.00 10.00 – 14.00 68.89 min

Stainless Steel 316 / 316L / 316Ti Flanges Mechanical Properties

Grade Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
SS 316 8.0 g/cm3 1400 °C (2550 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %
SS 316L 8.0 g/cm3 1399 °C (2550 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 316 / 316L / 316Ti Flanges

  • DIN 1.4401 / 1.4436 Tongue & Groove Flanges Supplier in UAE
  • SS 316 Spectacle blind flanges Manufacturer in India
  • SUS 316L Long Weld Neck Flanges
  • DIN 1.4404 / 1.4435 Flat Face Flanges
  • UNS S31600 High Hub Blind Flanges
  • DIN 1.4571 Lap Joint Flanges
  • DIN 1.4401 / 1.4436 Reducing Flanges Distributors
  • UNS S31603 Blind Flanges
  • ASME SA182 UNS S31635 Slip On Flanges
  • Stainless Steel 316L Threaded Flanges
  • ASME SA182 SS 316Ti Orifice Flanges Exporter in Russia
  • SS 316 Forged Flanges
  • UNS S31600 SS 316 Plate Flanges Supplier in Poland
  • SS 316L Spacer Ring Flanges
  • SS 316Ti Nipo Flange in Qatar
  • UNS S31603 / S31635 Nipolet Flanges
  • 316 Stainless Steel Pipe Flanges
  • SS 316L SORF Flanges
  • ASTM A182 SS 316L WNRF Flanges
  • UNS S31600 / S31603 Threaded Flanges

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 316 / 316L / 316Ti Flanges​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 316 / 316L / 316Ti Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo