Stainless Steel 347 / 347H Flanges

Stainless Steel 347 / 347H Flanges

ASTM A182 SS F347 Threaded Flanges, SS UNS S34709 Pipe Flanges, Stainless Steel F347H Industrial Flanges, ASME SA182 SS 347 Lap Joint Flange, ANSI B16.5 SS 347H Orifice Flange, Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the prominent supplying and distributing firm of Stainless Steel 347 / 347H Pipe Flanges, which is easily welded. Stainless Steel 347 Slip On Raised Flanges can with stand many organic and sufficiently diluted mineral acids depending on the temperature of the solution. Stainless Steel 347H Blind Raised Flanges is mainly used where corrosion resistance and sustained operations at temperatures between 800 Degree F and 1600 Degree F. Stainless Steel 347 Spectacle Blind Flanges has higher carbon that allows for better high temperature creep properties. Upsetting, Forging, and other hot work processes for Stainless Steel 347H Threaded Flanges can be performed at 1149 Degree C to 1232 Degree C (2100 Degree F to 2250 Degree F).

Stainless Steel 347 Socket Weld Flanges should be considered for applications requiring intermittent heating between 800 Degree F (427 Degree C) and 1650 Degree F (899 Degree C). Stainless Steel 347H Weld Neck Flanges has higher strength at temperatures above 1000 Degree F (537 Degree C). Stainless Steel 347 Lap Joint Flanges is often used in Exhaust manifolds and Chemical production equipment. Stainless Steel 347H Ring Joint Type Flanges is the higher carbon composition form and demonstrates improved high temperature and creep properties. Stainless Steel UNS S34700 Flanges maintains good corrosion resistance in applications where the temperature is between 800 Degree F and 1500 Degree F. Stainless Steel UNS S34709 Flanges is also used in rocket engine parts and aircraft collector rings.

Stainless Steel 347 Nippolet Flanges, SS DIN 1.4961 Socket Weld Flanges, Stainless Steel 347H Pipe Flanges, Stainless Steel 347 RTJ Flange, SS UNS S34700 Pipe Flanges, SS 347H Screwed Flanges, SS 347 Slip On Flanges Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 347 / 347H Specifications

Grade Stainless Steel 347 | SS 347 | UNS S34700
Standard ASTM A182, ASME SA182
Dimensions ANSI / ASME B16.5, B16.47 Series A & B, B.16.48, BS4504, BS10, DIN, EN-1092, MSS SP44
Size 1/2" - 48" (15NB - 1200NB)
Class / Pressure Rating 150 Class, 300 Class, 718 Class, 900 Class, 1500 Class, 2500 Class, PN6, PN10, PN16, PN25, PN40, PN64, etc.
Form Slip on Flanges (SORF), Threaded Flanges, Weld neck Flanges (WNRF), Blind Flanges, Socket weld Flanges, Lap Joint Flanges, Ring Type Joint Flanges, Spectacle Blind Flanges, Spacer Ring Flanges, Long weld Neck Flanges, Nipo Flange, Nipolet Flanges, Plate Flanges, Flat Flange, Orifice Flanges, Forged Flanges
Flange Face Type Flat Face (FF), Raised Face (RF), Ring Type Joint(RTJ)

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 347 1.4550 S34700 SUS 347 – 08Ch18N12B – X6CrNiNb18-10

Stainless Steel 347 / 347H Flanges Chemical Composition

Grade C Mn Si P S Cr Cb Ni Fe
SS 347 0.08 max 2.0 max 1.0 max 0.045 max 0.030 max 17.00 – 20.00 10xC – 1.10 9.00 – 13.00 62.74 min
SS 347H 0.04 – 0.10 2.0 max 1.0 max 0.045 max 0.030 max 17.00 – 20.00 8xC – 1.10 9.00 – 13.00 63.72 min

Stainless Steel 347 / 347H Flanges Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.0 g/cm3 1454 °C (2650 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 347 / 347H Flanges

  • DIN 1.4550 / 1.4961 Tongue & Groove Flanges Supplier in UAE
  • SS 347 Spectacle blind flanges Manufacturer in India
  • SUS 347H Long Weld Neck Flanges
  • DIN 1.4550 / 1.4961 Flat Face Flanges
  • UNS S34700 High Hub Blind Flanges
  • DIN 1.4550 Lap Joint Flanges
  • DIN 1.4961 Reducing Flanges Distributors
  • UNS S34700 Blind Flanges
  • ASME SA182 UNS S34709 Slip On Flanges
  • Stainless Steel 347 Threaded Flanges
  • ASME SA182 SS 347 Orifice Flanges Exporter in Russia
  • SS 347H Forged Flanges
  • UNS S34700 SS 347 Plate Flanges Supplier in Poland
  • SS 347H Spacer Ring Flanges
  • SS 347 Nipo Flange in Qatar
  • UNS S34700 / S34709 Nipolet Flanges
  • 347 Stainless Steel Pipe Flanges
  • SS 347H SORF Flanges
  • ASTM A182 SS 347 WNRF Flanges
  • UNS S34700 / S34709 Threaded Flanges

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 347 / 347H Flanges​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 347 / 347H Flanges to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today