Stainless Steel 347 / 347H Pipes & Tubes

Stainless Steel 347 / 347H Pipes & Tubes

DIN 1.4550 SS 347 Pipes, Stainless Steel UNS S34700 Welded Pipe & Tubes, DIN 1.4961 SS 347H Pipes, ASTM A312 TP 347 SS Seamless Pipes & Tubes, 347 SS Electropolished Pipes & Tubes Manufacturer in Mumbai,India.

Nickel Super Alloys is one of the prominent supplying and distributing firm of Stainless Steel 347 / 347H Pipes and Tubes, which is stabilized with columbium. Stainless Steel 347 Seamless Pipes uses columbium as a stabilizing element to maximize its principal feature: resistance to inter-granular corrosion. Stainless Steel 347H Welded Tubes is a non-heat treatable, austenitic and electric furnace processed grade of alloy. Stainless Steel 347 EFW Pipes is common in the petroleum refining industries. Stainless Steel 347H ERW Tubes have high corrosion resistance than other steels owing to the presence of large amounts of chromium. Stainless Steel 347 Round Pipesis a high carbon austenitic chromium stainless steel. In addition, Stainless Steel 347H Square Tubes has slightly improved corrosion resistance in strongly oxidizing environments.

Stainless Steel 347 Rectangular Pipes has general corrosion resistance and somewhat better resistance in strong oxidizing conditions. Stainless Steel 347H Electropolish Tubes offers an excellent resistance to inter-granular corrosion. Stainless Steel 347 Hexagonal Pipes allows for the elimination of carbide precipitation, and, consequently, inter-granular corrosion. Stainless Steel 347H Hallow Tubes is used for construction parts which should be resistant to scaling up to about 1050 Degree C. Stainless Steel UNS S34700 Pipes is an austenitic steel alloy with added Niobium/Columbium which acts as a stabilizer. Stainless Steel UNS S34709 Tubes is stabilized against chromium carbide formation by the addition of columbium and tantalum.

347H SS Hexagonal Pipes & Tubes, UNS S34709 Welded Pipe & Tubes, SS 347 Welded Pipes, 347 SS Hollow Pipe, ASTM A312 TP 347H SS Seamless Pipes & Tubes, SS 347H Pipe & Tubes, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

SS 347 / 347H Pipe Stock Size Range and Specifications

Grade Stainless Steel 347 / SS TP 347 / DIN 1.4550 Pipes / UNS S34700 Pipes
Size 1/8″NB TO 30″NB IN
Standard ASTM / ASME SA213 / A249 / A269 / A312 / A358 CL. I to V ASTM A789 / A790
Steel EFW 347 Pipes 1/2" NB - 24" NB
Form Round, Square, Rectangular, Hydraulic Etc
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Length Single Random, Double Random & Cut Length. (Custom Sizes Available as per customers requirement)
Type Seamless / ERW / Welded / Fabricated / EFW
End Plain End, Beveled End, Treaded
Standard SS 347
Werkstoff Nr. 1.4550
UNS S34700
JIS -
AFNOR -
BS -
GOST -
EN -

347 / 347H Stainless Steel Pipes Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
347 min. – – – – – 17.0 2.00 9.0 –
max. 0.08 2.0 1.00 0.045 0.030 20.0 3.00 13.0 –

Stainless Steel 347 / 347H Pipe Mechanical Properties

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
347 515 205 40 95 201

Other Types of Stainless Steel 347 / 347H Pipes & Stainless Steel Tubes

  • SS 347 Seamless Pipes Supplier in UAE
  • Stainless Steel 347H Pipes Manufacturer in India
  • SS 347 Welded Pipes
  • ASTM A312 TP 347H Fabricated Pipes
  • Stainless Steel 347 Tubes
  • SS 347H Round Tubes
  • Stainless Steel 347 Square Pipe
  • 347H Electropolish ERW Pipes
  • UNS S34700 / S34709 Hexagonal Pipe
  • 347 Stainless Stel Hallow Pipe
  • UNS S34700 / S34709 Welded Tubes Exporter in Russia
  • Steel 347H Bush Hex Pipe
  • Stainless Steel 347 Round Pipe Supplier in Poland
  • SS 347H ERW Pipes
  • Stainless Steel 347 EFW Pipes in Qatar
  • Stainless Steel 347H Steel Pipes
  • Werkstoff Nr. 1.4961 / 1.4550 Tubing
  • DIN 1.4961 / 1.4550 Tubes
  • SUS 347 Pipes
  • SUS 347H Rectangular Pipe

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 347 / 347H Pipes​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports ​Stainless Steel 347 / 347H Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today