Stainless Steel 410 Pipes & Tubes

Stainless Steel 410 Pipes & Tubes

ASTM A249 TP 410 SS Seamless Pipes, 410 Stainless Steel EFW Tubing, SS UNS S41000 Square Pipes, ASTM A312 TP410 SS Round Pipes, ASTM A213 SS TP410 Pipes, Manufacturer in Mumbai,India.

Nickel Super Alloys is a popular firm that manufactures and exports Stainless Steel 410 Pipes and Tubes, which are hardenable and straight-chromium stainless steels. Moreover, Stainless Steel 410 Seamless Pipes is a basic martensitic grade which contains 11.5 percent chromium. Stainless Steel 410 Welded Tubes is the general purpose 12 percent of chromium martensitic stainless steel. Meanwhile, Stainless Steel 410 EFW Pipes provides good corrosion resistance properties. Stainless Steel 410 ERW Tubesattains high mechanical properties after heat treatment. Stainless Steel 410 Round Pipes is the general purpose and most widely used of all the Martensitic grades of stainless steels. Further, Stainless Steel 410 Square Tubes is often used in cutlery, hardware and micrometer parts. Stainless Steel 410 Rectangular Pipes is magnetic in both the annealed and hardened conditions.

Stainless Steel 410 Electropolish Tubes has good strength and fairly good corrosion resistance as generally supplied hardened and tempered. Stainless Steel 410 Hexagonal Pipes has a wide range of properties that can be developed with different heat treatments, with ultimate tensile strengths. Stainless Steel 410 Hallow Tubes combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainless steels. In addition, Stainless Steel UNS S41000 Pipes provides excellent corrosion resistance plus high strength and hardness. Stainless Steel WNR 1.4006 Tubes is just sufficient enough to demonstrate corrosion resistance properties in mildsteam, atmospheres and many mild chemical environments.Heat treated 410 Stainless Steel Pipes has mechanical properties comparable to the engineering alloy steel.

Stainless Steel 410 Black Round Tubes, SS DIN 1.4006 Rectangular Welded Pipes, TP 410 SS ERW Pipes, ASTM A312 SS Seamless Pipes, Stainless Steel 410 Welded Tubes, SS 410 Polished Pipes, Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

SS 410 Pipe Stock Size Range and Specifications

Grade Stainless Steel 410 / SS TP 410
Size 1/2" NB TO 24"
Standard ASTM A / ASME SA213 / A249 / A269 / A312 / A358 CL. I to V ASTM A789 / A790
Steel ERW 410 Pipes 1/2" NB - 24" NB
Steel EFW 410 Pipes 6" NB - 100" NB
Form Round, Square, Rectangular, Hydraulic Etc
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Length Single Random, Double Random & Cut Length. (Custom Sizes Available as per customers requirement)
Type Seamless / ERW / Welded / Fabricated / EFW
End Plain End, Beveled End, Treaded
Grade 410
UNS No S41000
Old British BS : 410S21
En : 56A
Euronorm No: 1.4006
Name : X12Cr13
Swedish SS 2302
Japanese JIS SUS 410

410 Stainless Steel Pipes Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
410 min. – – – – – 11.5 – – –
max. 0.15 1.0 1.00 0.040 0.030 13.5 – 0.75 –

Stainless Steel 410 Pipe Mechanical Properties

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
410 480 275 16 95 201

Other Types of Stainless Steel 410 Pipes & Stainless Steel Tubes

  • SS 410 Seamless Pipes Supplier in UAE
  • Stainless Steel 410 Pipes Manufacturer in India
  • SS 410 Welded Pipes
  • ASTM A312 TP 410 Fabricated Pipes
  • Stainless Steel 410 Tubes
  • SS 410 Round Tubes
  • Stainless Steel 410 Square Pipe
  • 410 Electropolish ERW Pipes
  • UNS S41000 Hexagonal Pipe
  • 410 Stainless Stel Hallow Pipe
  • UNS S41000 Welded Tubes Exporter in Russia
  • Steel 410 Bush Hex Pipe
  • Stainless Steel 410 Round Pipe Supplier in Poland
  • SS 410 ERW Pipes
  • Stainless Steel 410 EFW Pipes in Qatar
  • Stainless Steel 410 Steel Pipes
  • Werkstoff Nr. 1.4006 Tubing
  • DIN 1.4006 Tubes
  • SUS 410 Pipes
  • SUS 410 Rectangular Pipe

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 410 Pipes​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports ​Stainless Steel 410 Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today