Stainless Steel 904L Pipes & Tubes

Stainless Steel 904L Pipes & Tubes

SS DIN 1.4539 Rectangular Welded Pipes, TP 904L SS ERW Pipes, ASTM B677 TP 904L SS Seamless Pipes & Tubes, Stainless Steel TP 904L Black Round Tubes, 904L SS Polished Pipes & Tubes Manufacturer in Mumbai,India.

Nickel Super Alloys is one of known manufacturing and stockist firm of Stainless Steel 904L Pipes and Tubes, which is known for its excellent corrosion properties. Stainless Steel 904L Seamless Pipes combines molybdenum and copper with iron for tremendously increased resistance to reducing acids like sulfuric acid. The molybdenum addition in Stainless Steel 904L Welded Tubes gives it superior resistance to localized attack (pitting and crevice corrosion) by chlorides. Stainless Steel 904L EFW Pipes is designed for moderate to high corrosion resistance. Stainless Steel 904L ERW Tubes is widely used in applications where the corrosion properties of other steels are not adequate. Stainless Steel 904L Round Pipes is a non-stabilized austenitic stainless steel with low carbon content.

Stainless Steel 904L Square Tubes is designed for corrosion and pitting resistance in a wide range of process environments. Stainless Steel 904L Rectangular Pipes is used in chemical plant, petrochemical plants, and oil refinery. Stainless Steel 904L Electropolish Tubes offers better corrosion resistance than chrome nickel stainless steels. Further, Stainless Steel 904L Hexagonal Pipes has highly alloyed chemistry with 25 percent nickel and 4.5 percent molybdenum. 904L Stainless Steel Tubes is intended for use under severe corrosion conditions within the process industry. Stainless Steel Din 1.4539 Pipes is used in pharmaceutical and medical environments. Theaddition of copper to Stainless Steel UNS N08904 Tubes gives it greatly improved resistance to strong reducing acids, particularly sulfuric acid.

Stainless Steel 904L Welded Tubes, ASTM B674 SS 904L Round Pipes & Tubes, SS UNS N08904 Square Pipes & Tubes, ASTM B673 SS TP904L Pipes & Tubes, 904L Stainless Steel EFW Tubing Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

SS 904L Pipe Stock Size Range and Specifications

Grade Stainless Steel 904L / SS TP 904L
Size 1/2" NB TO 24"
Standard ASTM A / ASME SA213 / A249 / A269 / A312 / A358 CL. I to V ASTM A789 / A790
Steel ERW 904L Pipes 1/2" NB - 24" NB
Steel EFW 904L Pipes 6" NB - 100" NB
Form Round, Square, Rectangular, Hydraulic Etc
Schedule SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS
Length Single Random, Double Random & Cut Length. (Custom Sizes Available as per customers requirement)
Type Seamless / ERW / Welded / Fabricated / EFW
End Plain End, Beveled End, Treaded
Grade 904L
UNS No N08904
Old British BS : 904S13
En : -
Euronorm No: 1.4539
Name :X1NiCrMoCuN25-20-5
Swedish SS 2562
Japanese JIS -

904L Stainless Steel Pipes Chemical Composition

Grade C Mn Si P S Cr Mo Ni N
904L min. – – – – – 19.0 4.00 23.00 0.10
max. 0.20 2.00 1.00 0.045 0.035 23.0 5.00 28.00 0.25

Stainless Steel 904L Pipe Mechanical Properties

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
904L 490 220 35 70-90 typical –

Other Types of Stainless Steel 904L Pipes & Stainless Steel Tubes

  • SS 904L Seamless Pipes Supplier in UAE
  • Stainless Steel 904L Pipes Manufacturer in India
  • SS 904L Welded Pipes
  • ASTM A312 TP 904L Fabricated Pipes
  • Stainless Steel 904L Tubes
  • SS 904L Round Tubes
  • Stainless Steel 904L Square Pipe
  • 904L Electropolish ERW Pipes
  • UNS N08904 Hexagonal Pipe
  • 904L Stainless Stel Hallow Pipe
  • UNS N08904 Welded Tubes Exporter in Russia
  • Steel 904L Bush Hex Pipe
  • Stainless Steel 904L Round Pipe Supplier in Poland
  • SS 904L ERW Pipes
  • Stainless Steel 904L EFW Pipes in Qatar
  • Stainless Steel 904L Steel Pipes
  • Werkstoff Nr. 1.4539 Tubing
  • DIN 1.4539 Tubes
  • SUS 904L Pipes
  • SUS 904L Rectangular Pipe

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 904L Pipes​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports ​Stainless Steel 904L Pipes to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today