Stainless Steel 310 / 310S Threaded Forged Fittings

Stainless Steel 310 / 310S Threaded Forged Fittings

ANSI B16.11 SS 310 Threaded Street Elbows, Stainless Steel 31S Threaded Cap, Stainless Steel 310 Threaded Tee, ASME SA182M SS 310S Class 6000 Threaded Fittings Manufacturer in Mumbai, India.

Nickel Super Alloys is a prominent firm in manufacturing an exporting Stainless Steel 310 / 310S Threaded Forged Fittings, which are essentially nonmagnetic as annealed. Stainless Steel 310 Threaded Elbow Forged Fittings is widely used in environments where sulfur dioxide gas is present at high temperatures. Stainless Steel 310S Threaded Tee Forged Fittings has good resistance to oxidation at temperatures of up to 1040 Degree C (1904 Degree F). Inter-pass temperature for Stainless Steel 310Threaded Cross Forged Fittings should not exceed 150 Degree C. Stainless Steel 310S Threaded Cap Forged Fittings is resistant to spalling and performs better in thermal cycling applications.

A common feature of high temperature Stainless Steel 310 Threaded Coupling Forged Fittings is that they are designed primarily for use at temperatures exceeding ~550 Degree C. Stainless Steel 310S Threaded Bend Forged Fittings is widely used in moderately carburizing atmospheres such as those encountered in petrochemical environments. Stainless Steel 310 Threaded Union Forged Fittings has the retention of a larger fraction of room temperature strength than the common austenitic alloys. Stainless Steel 310S Threaded Plug Forged Fittings has more severe carburizing atmospheres of thermal process equipment. Stainless Steel UNS S31008 Threaded Forged Fittings is used in tube hangers for petroleum refining and steam boilers. Due to its high chromium and nickel content, Stainless Steel UNS S31000 Threaded Forged Fittings is superior in most environments.

Stainless Steel 310 Threaded Union, ANSI B16.11 SS 310S Threaded 90 Deg Elbows, Stainless Steel 310 Threaded Bend, SS 310 Hex Plug, Stainless Steel 310S Threaded Coupling, SS 310 Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 310 / 310S Threaded Forged Fittings Specifications

Grade SS 310 / 310S | UNS S31000 / S31008
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

Standard SS 310 SS 310S
UNS S31000 S31008
WERKSTOFF NR. 1.4841 1.4845
AFNOR - -
JIS SUS 310 SUS 310S
GOST 20Ch25N20S2 20Ch23N18
BS 310S24 310S16
EN X15CrNi25-20 X8CrNi25-21

Stainless Steel 310 / 310S Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni Fe
SS 310 0.015 max 2 max 0.15 max 0.020 max 0.015 max 24 – 26 0.10 max 19 – 21 54.7 min
SS 310s 0.08 max 2 max 1.00 max 0.045 max 0.030 max 24 – 26 0.75 max 19 – 21 53.095 min

Stainless Steel 310 / 310S Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.9 g/cm3 1402 °C (2555 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 40 %

Other Types of Stainless Steel 310 / 310S Threaded Forged Fittings

  • Stainless Steel 310 Forged Elbow Supplier in UAE
  • DIN 1.4841 / 1.4845 Equal Tee Manufacturer in India
  • SS 310S Threaded Cross
  • SS 310 Threaded Union
  • UNS S31000 Hexagonal Plug
  • UNS S31008 Threaded Hex Plug
  • DIN 1.4841 45 Deg Threaded Elbow Distributors
  • DIN 1.4845 Threaded Bushing
  • SS 310S Threaded Lateral Tee
  • 310 Stainless Steel Threaded Cross
  • ASME B16.11 SS 310 Threaded Coupling Exporter in Russia
  • Stainless Steel 310S Threaded Tees
  • SS 310 Threaded 45 deg Elbow Supplier in Poland
  • UNS S31000 Threaded 90 deg Elbow
  • DIN 1.4841 Threaded Cap in Qatar
  • DIN 1.4845 Threaded Bend Flanges
  • SS 310S Threaded Union
  • UNS S31000 Threaded Bushing
  • UNS S31008 Lateral Tee
  • Stainless Steel 310 Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 310 / 310S Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 310 / 310S Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today