Stainless Steel 347 / 347H Threaded Forged Fittings

Stainless Steel 347 / 347H Threaded Forged Fittings

ANSI B16.11 SS 347 Threaded Street Elbows, Stainless Steel 347H Threaded Cap, Stainless Steel 347 Threaded Tee, ASME SA182M SS 347H Class 6000 Threaded Fittings Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the prominent supplying and distributing firm of Stainless Steel 347 / 347H Threaded Forged Fittings, which has good resistance to inter-granular attack. Stainless Steel 347 Threaded Elbow Forged Fittings can withstand more severely elevated temperatures. Stainless Steel 347HThreaded Tee Forged Fittings is used for high pressure steam pipe, and general refinery piping. Stainless Steel 347 Threaded Cross Forged Fittings has excellent resistance and corrosion protection. However, the hardenability of Stainless Steel 347H Threaded Cap Forged Fittings can be minimized by the use of constant positive feeds and slow speeds. Stainless Steel 347 Threaded Coupling Forged Fittings has a slightly improved corrosion resistance over other alloys.

Stainless Steel 347H Threaded Bend Forged Fittings has good oxidation resistance and creep strength to 1500 Degree F (816 Degree C). Alloyed with columbium-tantalum (referred to as niobium), Stainless Steel 347 Threaded Bushing Forged Fittings allows good mechanical properties at high temperatures. Stainless Steel 347H Threaded Union Forged Fittings offers higher creep and stress rupture properties. Stainless Steel 347 Threaded Plug Forged Fittings offers good resistance to polythionic acid SCC, encountered in oil refineries. Stainless Steel UNS S34700 Threaded Forged Fittings can be used in applications requiring repeated heating in the range of 800 Degree F and 1650 Degree F (427 Degree C -899 Degree C). When choosing the filler metal like Stainless Steel UNS S34709 Threaded Forged Fittings, the corrosion stress has to be regarded, as well.

Stainless Steel 347 Threaded Union, ANSI B16.11 SS 347H Threaded 90 Deg Elbows, Stainless Steel 347 Threaded Bend, SS 347H Hex Plug, Stainless Steel 347 Threaded Coupling, SS 347H Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 347 / 347H Threaded Forged Fittings Specifications

Grade SS 347 | Stainless Steel 347 | UNS S34700
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 347 1.4550 S34700 SUS 347 – 08Ch18N12B – X6CrNiNb18-10

Stainless Steel 347 / 347H Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Cb Ni Fe
SS 347 0.08 max 2 max 1.00 max 0.045 max 0.030 max 17.00 – 20.00 10xC – 1.10 9.00 – 13.00 62.74 min
SS 347H 0.10 max 2 max 1.00 max 0.045 max 0.030 max 17.00 – 19.00 8xC – 1.10 9.00 – 13.00 63.72 min

Stainless Steel 347 / 347H Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.0 g/cm3 1454 °C (2650 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 347 / 347H Threaded Forged Fittings

  • Stainless Steel 347 Forged Elbow Supplier in UAE
  • DIN 1.4550 Equal Tee Manufacturer in India
  • SS 347H Threaded Cross
  • SS 347 Threaded Union
  • UNS S34700 Hexagonal Plug
  • UNS S34709 Threaded Hex Plug
  • DIN S34709 45 Deg Threaded Elbow Distributors
  • DIN 1.4550 Threaded Bushing
  • SS 347 Threaded Lateral Tee
  • 347H Stainless Steel Threaded Cross
  • ASME B16.11 SS 347 Threaded Coupling Exporter in Russia
  • Stainless Steel 347H Threaded Tees
  • SS 347 Threaded 45 deg Elbow Supplier in Poland
  • UNS S34700 Threaded 90 deg Elbow
  • DIN 1.4961 Threaded Cap in Qatar
  • DIN 1.4550 Threaded Bend Flanges
  • SS 347 Threaded Union
  • UNS S34700 Threaded Bushing
  • UNS S34709 Lateral Tee
  • Stainless Steel 347H Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 347 / 347H Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 347 / 347H Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today