Stainless Steel 317 / 317L Threaded Forged Fittings

Stainless Steel 317 / 317L Threaded Forged Fittings

ANSI B16.11 SS 317 Threaded Street Elbows, Stainless Steel 317L Threaded Cap, Stainless Steel 317 Threaded Tee, ASME SA182M SS 317L Class 6000 Threaded Fittings Manufacturer in Mumbai, India.

Nickel Super Alloys is one of the leading manufacturing and supplying firm of SS 317 / 317L Threaded Forged Fittings, which is recommended to use chip breakers. Stainless Steel 317 Threaded Elbow Forged Fittings has as its main characteristic the great addition of molybdenum to its chemical composition. Stainless Steel 317L Threaded Tee Forged Fittings has increased resistance to chemical attack from acids. Stainless Steel 317Threaded Cross Forged Fittings is used in pulp and paper manufacturing and condensers in fossil. Stainless Steel 317L Threaded Cap Forged Fittings are frequently used for flue gas desulfurization service. Stainless Steel 317 Threaded Coupling Forged Fittings is a corrosion resistant austenitic chromium-nickel-molybdenum stainless steel.

Welding in Stainless Steel 317L Threaded Bend Forged Fittings can be performed using most of the conventional fusion and resistance methods. However, some processes in Stainless Steel 317 Threaded Union Forged Fittings involve extreme operating conditions that demand even higher performance characteristics. In addition, Stainless Steel 317LThreaded Plug Forged Fittings has excellent corrosion resistance and strength properties. Stainless Steel 317 Threaded Bushing Forged Fittings has higher creep, stress to rupture, and tensile strength at elevated temperatures. Stainless Steel 317L Threaded Hex Plus Forged Fittings has improved corrosion resistance. Stainless Steel UNS S31700 Threaded Forged Fittings may become slightly magnetic as a result of welding. The high molybdenum content gives Stainless Steel UNS S31703 Threaded Forged Fittings with superior pitting resistance.

Stainless Steel 317 Threaded Union, ANSI B16.11 SS 317L Threaded 90 Deg Elbows, Stainless Steel 317 Threaded Bend, SS 317L Hex Plug, Stainless Steel 317L Threaded Coupling, SS 317 Threaded Union Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 317 / 317L Threaded Forged Fittings Specifications

Grade SS 317 | Stainless Steel 317 | UNS S31700
Standard ASTM A182 & ASME SA182
Dimensions ASME 16.11, MSS SP-79, 83, 95, 97, BS 3799
Size 1/8” NB to 4” NB (Socketweld & Screwed-Threaded)
Class 2000 LBS, 3000 LBS, 6000 LBS, 9000 LBS
Form Threaded 45 deg Elbow, Threaded 90 deg Elbow, Threaded Tee, Threaded Cross, Threaded Cap, Threaded Bend, Threaded Coupling, Threaded Union , Threaded Bushing, Plug, Hex Plus, Hexagonal Plus, Lateral Tee.
Type Threaded Forged Fittings

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
SS 317 1.4449 S31700 SUS 317 3304S11 – – –

Stainless Steel 317 / 317L Threaded Forged Fittings Chemical Composition

Grade C Mn Si P S Cr Mo Ni Fe
SS 317L 0.035 max 2 max 1.00 max 0.045 max 0.030 max 18.00 – 20.00 3.00 – 4.00 11.00 – 15.00 57.89 min

Stainless Steel 317 / 317L Threaded Forged Fittings Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
7.9 g/cm3 1400 °C (2550 °F) Psi – 75000 , MPa – 515 Psi – 30000 , MPa – 205 35 %

Other Types of Stainless Steel 317 / 317L Threaded Forged Fittings

  • Stainless Steel 317 Forged Elbow Supplier in UAE
  • DIN 1.4438 Equal Tee Manufacturer in India
  • SS 317L Threaded Cross
  • SS 317L Threaded Union
  • UNS S31703 Hexagonal Plug
  • UNS S31703 Threaded Hex Plug
  • DIN 1.4438 45 Deg Threaded Elbow Distributors
  • DIN 1.4438 Threaded Bushing
  • SS 317 Threaded Lateral Tee
  • 317L Stainless Steel Threaded Cross
  • ASME B16.11 SS 317 Threaded Coupling Exporter in Russia
  • Stainless Steel 317L Threaded Tees
  • SS 317L Threaded 45 deg Elbow Supplier in Poland
  • UNS S31703 Threaded 90 deg Elbow
  • DIN 1.4438 Threaded Cap in Qatar
  • DIN 1.4438 Threaded Bend Flanges
  • SS 317L Threaded Union
  • UNS S31703 Threaded Bushing
  • UNS S31703 Lateral Tee
  • Stainless Steel 317 Threaded Cross

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless Steel 317 / 317L Threaded Forged Fittings​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless Steel 317 / 317L Threaded Forged Fittings to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today