Stainless Steel 202 Plates & Sheets

Stainless Steel 202 Plates & Sheets

Stainless Steel 202 Plates, SS 202 Sheets, SS 202 Golden Designer Sheet, SS 202 Silver Design Sheet, SS 202 Chequered Sheet & Plate Manufacturer in Mumbai, India.

Nickel Super Alloys is a popular firm that supplies,manufactures, and exports these SS 202 Sheets, Plates and Coils, which is one of the most desired and widely used grades of stainless on the market. Relying on our expertise in this domain, we are into offering Stainless Steel 202 Plates, which contributes to non-corrosive for longer. The manganese helps preserve the austenitic phase in Stainless Steel 202 Coils, as does the nickel. SS202 Plates has excellent resistance to pitting, corrosion and SCC. SS 202 Coils possesses good corrosion resistance, high harness, toughness, and strength. 202 Stainless Steel Sheets is very inexpensive so clients can use it in indoor applications like indoor fabrication, automobile trim and application where atmosphere is not a considerable factor.

202 Stainless Steel Platesis non-magnetic high manganese steel, and is generally an ordinary magnetic steel or low alloy steel. Manganese content in 202 Stainless Steel Coils has a lesser effect on the corrosion and heat resistance but modifies the mechanical and physical properties like weldability, fabricability, and machinability. Stainless Steel UNS S20200 Sheets has high carbon that may cause stress corrosion cracking, especially after welding thicker material. Catering to the requirements of our clients, we are involved in offering Stainless Steel UNS S20200 Plates, which enhances the passivity in more aggressive conditions. The machinability of Stainless Steel UNS S20200 Coils produces long and gummy chips.

Stainless Steel 202 Cold Rolled Plates, ASME SA240 Stainless Steel 202 Coils, 202 SS Chequered Plate, Stainless Steel 202 Plates, SS 202 Sheets, SS UNS S20200 Plates, SS Grade 202 Polished Plates Suppliers in India.

Key Charactristic:

  • Corrosion resistance
  • Resistance to oxidation and sulfidation
  • Cryogenic strength
  • Resistance to abrasion and erosion
  • Surface finish
  • Magnetic properties
  • Ductility
  • Elevated temperature strength
  • Stability of properties in service
  • Suitability for intended fabrication techniques

Stainless Steel 202 Sheets & Plates Specifications

Standard ASTM A240/A480
Steel Grades AISI202 (1.4373)
Width 1000mm, 1250mm, 1500mm, 2000mm, Other sizes on request
Thickness Min: 0.4mm Max: 10.0mm
Finish 1D, 2B, BA, N4, N5, SB, HL, N8,Oil base wet polished, Both sides polished available
Application Medical equipment, Food industry, Construction material, Kitchen utensils, BBQ grill, Building construction, Electric equipment,
Form Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Perforated Sheet, Chequered Plate, Strip, Flats, Blank (Circle), Ring (Flange)
End Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Stainless Steel 202 Sheets & Plates Chemical Composition

Grade
C
Mn
Si
P
S
Cr
Ni
N
SS 202
0.15 max
7.50-10
1.0 max
0.060 max
0.030 max
17–19
4-6
0.25 max

Stainless Steel 202 Sheets & Plates Mechanical Properties

Grade
Tensile Strength (MPa) min
Yield Strength 0.2% Proof (MPa) min
Elongation (% in 50mm) min
202
515
275
40

Other Types of Stainless Steel 202 Sheets & Plates

  • Stainless Steel TP202 Plates Supplier in UAE
  • ASME SA240 SS TP202 Cold Rolled Sheets Manufacturer in India
  • Stainless Steel TP202 Sheets
  • ASTM A240 SS TP202 Hot Rolled Plates
  • Stainless Steel TP202 A240M HR Sheets
  • DIN 1.4373 Plates
  • UNS S20200 Embossed Sheets Distributors
  • ASME SA240 SS 202 Mill Finished Plates
  • AISI 202 Austenitic Stainless Steel Shim Sheets
  • SS 202 Hot Rolled Plates
  • SS 202 Cold Rolled Plates
  • SS 202 Polished Plates Supplier in Poland
  • Stainless Steel 202 Perforated Sheets
  • Stainless Steel 202 Chequered Plate in Qatar
  • Stainless Steel 202 Perforated Sheet
  • SS 202 Silver Designer Sheets
  • SS 202 Golden Designer Sheets
  • UNS S20200 Sheets
  • DIN 1.4373 Plates

Countries We Export to

Nickel Super Alloys manufactures and exports ​Stainless steel 202 Plates & Sheets​ to various countries such as Saudi Arabia, Bangladesh, United States, United Arab Emirates, Canada, Angola, Argentina, Austria, Azerbaijan, Pakistan, Peru, Chile, Kuwait, Mexico, Malaysia, Nigeria, Serbia, Singapore, Taiwan, Chile, Venezuela, Ecuador, Netherlands, Brazil, Vietnam, South Africa, Nigeria, Mexico, Turkey, Hungary, Algeria, Belarus, Belgium, Bhutan, Bolivia, Bulgaria, Croatia, Czech Republic, Estonia, Finland, Greece, Italy, Japan, Libya, Colombia, Ghana, Iran, Denmark, Poland, Australia, Afghanistan, Bahrain, Costa Rica, Egypt, Iraq, Jordan, South Korea, Kazakhstan, Sri Lanka, Lithuania, Norway, Oman, Philippines, Poland, Qatar, Spain, France, United Kingdom, Indonesia, Israel, Iran, Russia, Romania, Thailand, Trinidad & Tobago,Tunisia, Ukraine, Yemen, Hong Kong, Gabon, China, Portugal, Switzerland, New Zealand, Sweden, Slovakia, Kenya, Lebanon, Morocco, Mongolia

Cities We Deliver to

Nickel Super Alloys manufactures and exports Stainless steel 202 Plates & Sheets to multiple cities such as Mumbai, Thane, Navi Mumbai, Pune, Pimpri-Chinchwad, Vadodara, Kolkata, Gurgaon, Ahmedabad, Seoul, Hyderabad, Singapore, Abu Dhabi, Tehran, Calgary, Noida, Riyadh, London, Coimbatore, Jakarta, Istanbul, Bangkok, Kuwait City, Sharjah, Muscat, Edmonton, Busan, Mexico City, Doha, New Delhi, Bengaluru, Chennai, Surat, Bhopal, Ulsan, Faridabad, Houston, Dubai, Jeddah, Aberdeen, Cairo, Geoje-si, Perth, Santiago, Chandigarh, Indore, Kuala Lumpur, Rio de Janeiro, Dammam, Melbourne, Madrid, La Victoria, Bogota, Lahore, Los Angeles, Algiers, Chiyoda, Ankara, Ho Chi Minh City, Toronto, Hong Kong, Howrah, Sydney, Ahvaz, Karachi, Rajkot, Brisbane, Petaling Jaya, Ernakulam, Secunderabad, Gimhae-si, Al Jubail, Port-of-Spain, Thiruvananthapuram, Milan, Atyrau, Lagos, Hanoi, New York, Caracas, Vung Tau, Al Khobar, Manama, Montreal, Granada, Courbevoie, Visakhapatnam, Ludhiana, Moscow, Dallas, Haryana, Colombo

If you have any queries related to our products. Enquire us Today